Fracture resistance of CAD/CAM occlusal veneers: A systematic review of laboratory studies
Source abstract
Abstract
Objective The purpose of this systematic review was to summarize scientific evidence that evaluates in vitro fracture and fatigue strength of occlusal veneers in different thicknesses, CAD/CAM materials, and under different aging methodologies. Materials and methods An electronic search of 3 English databases (The National Library of Medicine (MEDLINE/PubMed), ScienceDirect, and EBSCOhost) was conducted. Laboratory studies published between September 2009 and October 2019 that evaluated fracture or fatigue strength of CAD/CAM occlusal veneers and used human teeth were selected. The included studies were individually evaluated for the risk of bias following a predetermined criterion. The outcomes assessed included the types of the restorative material, the thickness of the veneers, and aging methods. Results A total of 12 studies fulfilled the inclusion criteria. Most of the included studies (86%) evaluated the fracture strength of occlusal veneers. Two studies evaluated fatigue resistance. There was a significant relationship between the choice of materials and fracture strength. Polymeric materials performed better in fatigue testing in comparison to ceramics. Lithium silicate-based glass ceramics showed more favorable outcomes in a thickness of 0.7-1.0 mm. Fracture resistance values in all the included studies exceeded maximum bite forces in the posterior region. Conclusions The outcomes of this systematic review suggest that occlusal veneers can withstand bite forces in the posterior region, whereas the measurement of thickness should be standardized in order to have a fair comparison. Further research needs to be conducted to evaluate the longevity of this type of restorations clinically.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Temporomandibular Joint Disorders · Dental Research and COVID-19
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Fracture resistance of ceramic and polymer-based occlusal veneer restorations10.1016/j.jmbbm.2017.06.013 ↗
2. Influence of thermomechanical fatigue on the fracture strength of CAD-CAM-fabricated occlusal veneers10.1016/j.prosdent.2018.07.019 ↗
3. Biaxial flexural strength, elastic moduli, and x-ray diffraction characterization of three pressable all-ceramic materials10.1067/mpr.2003.42 ↗
4. Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials10.1016/S0300-5712(03)00025-3 ↗
5. Effect of different computer-aided design/computer-aided manufacturing (CAD/CAM) materials and thicknesses on the fracture resistance of occlusal veneers10.2341/17-131-L ↗
6. Angerame · 2019
7. Edge chipping resistance and flexural strength of polymer infiltrated ceramic network and resin nanoceramic restorative materials10.1016/j.prosdent.2016.02.014 ↗
8. Influence of ceramic thickness and ceramic materials on fracture resistance of posterior partial coverage restorations10.2341/12-459-L ↗
9. Digital dentistry: an overview of recent developments for CAD/CAM generated restorations10.1038/sj.bdj.2008.350 ↗
10. Strength and fracture pattern of monolithic CAD/CAM-generated posterior crowns10.1016/j.dental.2005.02.007 ↗
11. Bonding protocols for improved long-term clinical success
12. Resin-ceramic bonding: a review of the literature10.1067/mpr.2003.50 ↗
13. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
14. In-vitro strength degradation of dental ceramics and novel PICN material by sharp indentation10.1016/j.jmbbm.2013.05.004 ↗
15. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
16. Robotic chewing simulator for dental materials testing on a sensor-equipped implant setup
17. Systematic Reviews: Synthesis of Best Evidence for Clinical Decisions10.7326/0003-4819-126-5-199703010-00006 ↗
18. A critical review of the durability of adhesion to tooth tissue: methods and results10.1177/154405910508400204 ↗
19. Work of adhesion of resin on treated lithia disilicate-based ceramic10.1016/S0109-5641(03)00126-X ↗
20. Clinical performance of a new biomimetic double network material10.2174/1874210620130904003 ↗
21. Does artificial aging affect mechanical properties of CAD/CAM composite materials10.1016/j.jpor.2017.06.001 ↗
22. Fracture resistance and microleakage of endocrowns utilizing three CAD-CAM blocks10.2341/13-143-L ↗
23. The effect of cement type and mixing on the bi-axial fracture strength of cemented aluminous core porcelain discs10.1016/S0109-5641(02)00006-4 ↗
24. Influence of preparation design and ceramic thicknesses on fracture resistance and failure modes of premolar partial coverage restorations10.1016/S0022-3913(13)60374-1 ↗
25. Evaluation of thickness of CAD/CAM fabricated zirconia cores by digital microscope10.3233/THC-171144 ↗
26. A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics10.1002/1097-4636(2000)53:4<297::AID-JBM3>3.0.CO;2-G ↗
27. Fatigue resistance of monolithic CAD/CAM ceramic crowns on human premolars10.1016/j.ceramint.2016.07.029 ↗
28. Static and fatigue mechanical behavior of three dental CAD/CAM ceramics10.1016/j.jmbbm.2016.01.023 ↗
29. Numerical fatigue analysis of premolars restored by CAD/CAM ceramic crowns10.1016/j.dental.2018.03.017 ↗
30. Ultra-thin occlusal veneers bonded to enamel and made of ceramic or hybrid materials exhibit load-bearing capacities not different from conventional restorations10.1016/j.jmbbm.2018.09.041 ↗
31. Fracture strength of CAD/CAM composite and composite-ceramic occlusal veneers10.1016/j.jpor.2014.01.001 ↗
32. Maximum biteforces as a basis for the design of dental restorations
33. Fatigue resistance and microleakage of CAD/CAM ceramic and composite molar crowns10.1111/j.1532-849X.2011.00773.x ↗
34. Mechanical properties of composite resin blocks for CAD/CAM10.4012/dmj.2014-208 ↗
35. An up to 16-year prospective study of 304 porcelain veneers
36. Comparison of mechanical properties of three machinable ceramics with an experimental fluorophlogopite glass ceramic10.1016/j.prosdent.2015.02.024 ↗
37. Effects of thickness, processing technique, and cooling rate protocol on the flexural strength of a bilayer ceramic system10.1016/j.dental.2013.07.019 ↗
38. Load-bearing properties of minimal-invasive monolithic lithium disilicate and zirconia occlusal onlays: finite element and theoretical analyses10.1016/j.dental.2013.04.004 ↗
39. Load-bearing capacities of ultra-thin occlusal veneers bonded to dentin10.1016/j.jmbbm.2019.04.006 ↗
40. Effect of preparation design for all-ceramic restoration on maxillary premolar: a 3D finite element study10.1016/j.jpor.2018.04.002 ↗
41. Immediate dentin sealing: a fundamental procedure for indirect bonded restorations10.1111/j.1708-8240.2005.tb00103.x ↗
42. The case for moderate "guided prep" indirect porcelain veneers in the anterior dentition. The pendulum of porcelain veneer preparations: from almost no-prep to over-prep to no-prep
43. Influence of overlay restorative materials and load cusps on the fatigue resistance of endodontically treated molars
44. Simulated fatigue resistance of composite resin versus porcelain CAD/CAM overlay restorations on endodontically treated molars
45. In vitro fatigue resistance of CAD/CAM composite resin and ceramic posterior occlusal veneers10.1016/S0022-3913(10)60111-4 ↗
46. Modeling of ultrathin occlusal veneers10.1016/j.dental.2012.04.002 ↗
47. From artisanal to CAD-CAM blocks: state of the art of indirect composites10.1177/0022034516634286 ↗
48. Silane adhesion mechanism in dental applications and surface treatments: a review10.1016/j.dental.2017.09.002 ↗
49. Survival rate of resin and ceramic inlays, onlays, and overlays: a systematic review and meta-analysis10.1177/0022034516652848 ↗
50. Influence of antagonist material on fatigue and fracture resistance of zirconia crowns10.1055/s-0040-1708228 ↗
51. Accuracy and precision of 3 intraoral scanners and accuracy of conventional impressions: a novel in vivo analysis method10.1016/j.jdent.2017.12.006 ↗
52. Influence of thermal and mechanical cycling on the flexural strength of ceramics with titanium or gold alloy frameworks10.1016/j.dental.2007.06.008 ↗
53. Surface conditioning and bonding protocol for polymer-infiltrated ceramic: how and why?
54. Effect of temperature on post-cure polymerization of bulk-fill composites10.1016/j.jdent.2014.08.004 ↗
55. Petticrew · 2008
56. A prospective ten-year clinical trial of porcelain veneers
57. A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part I: single crowns10.1111/j.1600-0501.2007.01467.x ↗
58. Bond strength of universal adhesives: a systematic review and meta-analysis10.1016/j.jdent.2015.04.003 ↗
59. Effect of impact velocity and specimen stiffness on contact forces in a weight-controlled chewing simulator10.1016/j.dental.2011.09.007 ↗
60. The role of resin cement on bond strength of glass-fiber posts luted into root canals: a systematic review and meta-analysis of in vitro studies10.2341/13-070-LIT ↗
61. Influence of restoration thickness and dental bonding surface on the fracture resistance of full-coverage occlusal veneers made from lithium disilicate ceramic10.1016/j.dental.2015.04.017 ↗
62. Novel-design ultra-thin CAD/CAM composite resin and ceramic occlusal veneers for the treatment of severe dental erosion10.1016/S0022-3913(11)60035-8 ↗
63. Influence of different load application devices on fracture resistance of restored premolars10.1590/S0103-64402012000500003 ↗
64. Fracture strength of minimally prepared all-ceramic CEREC crowns after simulating 5 years of service10.1016/j.dental.2013.03.019 ↗
65. Surface treatment protocols in the cementation process of ceramic and laboratory-processed composite restorations: a literature review10.1111/j.1708-8240.2005.tb00119.x ↗
66. Polymer-infiltrated ceramic CAD/CAM inlays and partial coverage restorations: 3-year results of a prospective clinical study over 5 years10.1007/s00784-017-2293-x ↗
67. Changes in surface characteristics of two different resin composites after 1 year water storage: an SEM and AFM study10.1002/sca.21317 ↗
68. Aspects of bonding between resin luting cements and glass ceramic materials10.1016/j.dental.2014.01.017 ↗
69. Full-mouth adhesive rehabilitation of a severely eroded dentition: the three-step technique. Part 1
70. Full-mouth adhesive rehabilitation of a severely eroded dentition: the three-step technique. Part 2
71. Full-mouth adhesive rehabilitation of a severely eroded dentition: the three-step technique. Part 3
72. Effect of food/oral-simulating liquids on dynamic mechanical thermal properties of dental nanohybrid light-cured resin composites10.1016/j.dental.2013.04.013 ↗
73. Aspects of adhesion tests on resin-glass ceramic bonding10.1016/j.dental.2017.06.013 ↗
74. Effects of artificial aging and progression of cracks on thin occlusal veneers using SD-OCT
75. Influence of various bonding techniques on the fracture strength of thin CAD/CAM-fabricated occlusal glass-ceramic veneers10.1016/j.jmbbm.2017.08.016 ↗