journal article·2021-02Open access

Comparison of conventional ceramic laminate veneers, partial laminate veneers and direct composite resin restorations in fracture strength after aging

Marco M.M. Gresnigt, Mari M. Sugii, Karin B.F.W. Johanns, Stephan A.M. van der Made

Abstract

OBJECTIVES: The objectives of this study were to test the fracture strength in vitro of laminate veneers, partial laminate veneers and composite restorations after aging and analyze the failure mode. METHODS: Forty extracted, sound human teeth were selected and divided into four groups: 1) Control group (CG); 2) Conventional Laminate Veneer (CLV); 3) Partial Laminate Veneer (PLV); 4) Direct Composite Resin (DCR). Laminate veneer preparations with incisal overlap were made in group CLV whereas only incisal preparations were made with a 1 mm bevel in group PLV and DCR. The indirect restorations were luted with a resin composite and the DCR group was restored with a direct resin composite restoration. The restored teeth were subsequently aged by thermocycling (20.000 cycles, 5-55 degrees C). Subsequently, the fracture strength was tested by a load to failure test at 135° on the incisal edge. A failure analysis was performed using light microscopy. The results were analyzed using Shapiro-Wilk and Kruska-Wallis test. RESULTS: After thermocycling, one sample from group CLV presented a premature adhesive failure and was excluded. Three restorations from groups PLV and DCR presented small cracks but were taken to the fracture test. After aging mean fracture load + SD (N) were: Group DCR (n = 10): 385 ± 225; Group CG (n = 10): 271 ± 100; Group PLV (n = 10): 266 ± 69; Group CLV (n = 9): 264 ± 66. Fracture strength means from groups CLV and PLV did not differ statistically from each other nor from control (p = 0.05). In the group CLV the root fracture was the most occurring fracture. In groups PLV and DCR, material cohesive failures and a mix (adhesive, tooth and material cohesive) failures were most observed. SIGNIFICANCE: This in vitro study showed for the first time that partial laminate veneers can exhibit fracture strength values similar to direct composite restorations or conventional ceramic laminate veneers. All three restorative procedures presented clinically acceptable values of fracture strength. Even though three samples from groups PLV and three from DCR presented small cracks after thermocycling, these cracks do not appear to have a negative effect on the fracture strength.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Anusavice · 2013 · vol. 12
2. Ceramic laminate veneers: effect of preparation design and ceramic thickness on fracture resistance and marginal quality in vitro10.1007/s00784-019-03136-z ↗
3. Restoring a single anterior tooth: solutions to a dental dilemma10.14219/jada.archive.2004.0126 ↗
4. Clinical evaluation on porcelain laminate veneers bonded with light-cured composite: results up to 7 years10.1007/s00784-011-0593-0 ↗
5. The clinical success of all-ceramic restorations10.14219/jada.archive.2008.0361 ↗
6. Tooth structure removal associated with various preparation designs for anterior teeth10.1067/mpr.2002.124094 ↗
7. Farias-Neto · 2015
8. Single tooth bite forces in healthy young adults10.1046/j.0305-182X.2003.01179.x ↗
9. Randomized clinical trial on indirect resin composite and ceramic laminate veneers: up to 10-year findings10.1016/j.jdent.2019.06.001 ↗
10. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
11. Resin composite restorative materials10.1111/j.1834-7819.2010.01296.x ↗
12. A three-dimensional finite element study on anterior laminate veneers with different incisal preparations10.1016/j.prosdent.2013.09.023 ↗
13. Porcelain veneers: dentin bonding optimization and biomimetic recovery of the crown
14. Effect of luting composite shrinkage and thermal loads on the stress distribution in porcelain laminate veneers10.1016/S0022-3913(99)70278-7 ↗
15. Energy dissipation capacities of CAD-CAM restorative materials: a comparative evaluation of resilience and toughness10.1016/j.prosdent.2018.05.003 ↗
16. The 5-year clinical performance of direct composite additions to correct tooth form and position. I. Esthetic qualities10.1007/s007840050003 ↗
17. Flexural strength and modulus of elasticity of different types of resin-based composites10.1590/S1806-83242007000100003 ↗
18. Evaluation of fracture strength of ceramics containing small surface defects introduced by focused ion beam10.3390/ma11030457 ↗
19. CAD/CAM ceramic fragments in anterior teeth: a clinical report10.1111/jerd.12342 ↗
20. Investigation of stress distribution in roots restored with different crown materials and luting agents10.4012/dmj.27.229 ↗
21. Fracture frequency and longevity of fractured resin composite, polyacid-modified resin composite, and resin-modified glass ionomer cement class IV restorations: an up to 14 years of follow-up10.1007/s00784-009-0287-z ↗
22. Computer-aided designed/computer-assisted manufactured composite resin versus ceramic single-tooth restorations: a 3-year clinical study
23. [Treatment of crown fractured incisors: reattachment instead of restoration?]