journal article·2017-01

Using a chewing simulator for fatigue testing of metal ceramic crowns

S.D. Heintze, A. Eser, D. Monreal, V. Rousson

Publisher page

Abstract

Objective Dynamic loading is a more important predictor for the clinical longevity of ceramic crowns than static loading. However, dynamic loading machines are costly and mostly have only one test station. The SD Mechatronik Chewing Simulator (formerly Willytec) may be a cost-effective alternative to evaluate the fatigue resistance of metal ceramic crowns. Method Four metal ceramic materials were tested on lower first molar crowns: GC InitiaI, Creation (Willy Geller), IPS InLine (Ivoclar Vivadent) and the new low-fusion IPS Style Ceram (Ivoclar Vivadent). The ceramic material was manually layered on frames made of the nickel-chromium alloy 4all (Ivoclar Vivadent) by using a silicone mould. The crowns were adhesively luted to PMMA dies. Dynamic loading was carried out with a SD Mechatronik Chewing Simulator using additional bars with weights. A steel antagonist (Ø 4mm) with 40mm/s downward speed hit the disto-buccal cusp of the crown with minimal impulse while sliding for a distance of 0.7mm. The starting load was 250N. The forces at each load level had been verified with a 3D force sensor (Kistler). Four crowns per group and load were submitted to four decreasing load levels for 200,000 cycles with a resulting simulation frequency of 0.9Hz and simultaneous thermocycling (5°C/55°C) until all four crowns no longer showed chippings. Statistical analyses had been carried out using an exponential, a Weibull and a lognormal model. The fatigue resistance was defined as the maximal load for which one would observe less than 1% failure after 200,000 cycles. In addition to the fatigue testing of the molar crowns, simulations of finite element method (FEM) were conducted in order to investigate the influence of the mismatch of the thermal expansion coefficient (CTE) between the PMMA die and the molar crown on the fatigue resistance. Results The 3D-force measurements revealed that the summarised forces were very similar to the force of the dead weights that were put on the bars. The failure modes consisted of cracks and small and big chippings. Chi-square test and Gamma revealed no statistically significant differences between the four test materials in relation to the failure mode. At 250N all materials showed chippings within the ceramic or down to the metal frame, while at lower loads there were differences. The estimated fatigue resistance was 68N for GC Initial, 88N for Creation, 96N for IPS Style Ceram, and 105N for IPS InLine, when using a Weibull model and considering all possible events. Furthermore, FEM simulations revealed that the maximum values of the maximum principal stress were 90 MPa for the thermocycling and 225 MPa for the external load. Conclusion The SD Mechatronik Chewing Simulator is an adequate and cost-effective tool to test layered PFM crowns for fatigue resistance. The test method and the chewing simulator can be used for ceramic on metal, ceramic on zirconia and monolithic ceramic materials.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Standardizing failure, success, and survival decisions in clinical studies of ceramic and metal-ceramic fixed dental prostheses10.1016/j.dental.2011.09.012 ↗
2. Physical properties of dental materials
3. Resin composites: strength of the bond to dentin versus surface energy parameters10.1016/j.dental.2004.12.004 ↗
4. The clinical performance of porcelain-fused-to-metal precious alloy single crowns: chipping, recurrent caries, periodontitis, and loss of retention10.11607/ijp.3440 ↗
5. Bilandžić · 2009
6. Fatigue and damage accumulation of veneer porcelain pressed on Y-TZP10.1016/j.jdent.2009.12.004 ↗
7. Burnham · 1998
8. Porcelain-fused-to-metal versus zirconia-based ceramic restorations10.14219/jada.archive.2009.0316 ↗
9. A clinical comparison of zirconia, metal and alumina fixed-prosthesis frameworks veneered with layered or pressed ceramic: a three-year report10.14219/jada.archive.2010.0076 ↗
10. Laboratory simulation of Y-TZP all-ceramic crown clinical failures10.1177/0022034509333968 ↗
11. Fatigue testing of two porcelain-zirconia all-ceramic crown systems10.1016/j.dental.2009.03.009 ↗
12. Long-term clinical study of porcelain-fused-to-gold restorations10.1016/0022-3913(84)90217-8 ↗
13. A clinical evaluation of cobalt–chromium metal-ceramic fixed partial dentures and crowns: a three- to seven-year retrospective study10.1016/S0022-3913(07)60032-8 ↗
14. Initial versus final fracture of metal-free crowns, analyzed via acoustic emission10.1016/j.dental.2008.04.010 ↗
15. Biting and chewing in overdentures, full dentures, and natural dentitions10.1177/00220345000790071501 ↗
16. Chewing movements in relation to border movements at the first molar10.1016/0022-3913(81)90220-1 ↗
17. Monolithic CAD/CAM lithium disilicate versus veneered Y-TZP crowns: comparison of failure modes and reliability after fatigue
18. Effect of veneering techniques on damage and reliability of Y-TZP trilayers
19. How to qualify and validate wear simulation devices and methods10.1016/j.dental.2006.02.002 ↗
20. Fatigue resistance of denture teeth10.1016/j.jmbbm.2015.08.034 ↗
21. Survival of zirconia- and metal-supported fixed dental prostheses: a systematic review
22. ISO, 2007. Dentistry-implants-dynamic fatigue test for endosseous dental implants. International Standard DIN EN ISO No. 14801.
23. Kalbfleisch · 2002
24. Cyclic fatigue testing of denture teeth for bulk fracture10.1016/j.dental.2013.07.001 ↗
25. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
26. The slippery slope: critical perspectives on in vitro research methodologies10.1016/j.dental.2011.09.001 ↗
27. Wear of composite resin veneering materials in a dual-axis chewing simulator10.1046/j.1365-2842.1999.00416.x ↗
28. Clinical risk factors related to failures with zirconia-based restorations: an up to 9-year retrospective study10.1016/j.jdent.2013.10.009 ↗
29. Effect of sample thickness on bite force studied with a multiple-point sheet sensor10.1046/j.1365-2842.2003.01248.x ↗
30. Materials design in the performance of all-ceramic crowns10.1016/j.biomaterials.2003.09.050 ↗
31. Fracture strength of all-ceramic crowns with varying core elastic moduli
32. Six-year clinical performance of lithium disilicate fixed partial dentures
33. Survival of glass-ceramic materials and involved clinical risk: variables affecting long-term survival
34. Nelson · 1990 · 493
35. A 5-year retrospective study of cobalt–chromium-based single crowns inserted in a private practice
36. Five-year results of a prospective randomised controlled clinical trial of posterior computer-aided design-computer-aided manufacturing ZrSiO4-ceramic crowns10.1111/joor.12075 ↗
37. A four-year prospective clinical evaluation of zirconia and metal–ceramic posterior fixed dental prostheses
38. All-ceramic or metal–ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part II: multiple-unit FDPs10.1016/j.dental.2015.02.013 ↗
39. A prospective 10-year study of metal ceramic single crowns and fixed dental prosthesis retainers in private practice settings10.1016/S0022-3913(13)60034-7 ↗
40. Practice-based clinical evaluation of metal–ceramic and zirconia molar crowns: 3-year results10.1111/joor.12018 ↗
41. Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures10.1016/j.dental.2005.04.024 ↗
42. Randomized controlled clinical trial of zirconia-ceramic and metal-ceramic posterior fixed dental prostheses (FDPs): 3-year follow-up
43. All-ceramic or metal–ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part I: Single crowns (SCs)10.1016/j.dental.2015.02.011 ↗
44. Off-axis sliding contact reliability and failure modes of veneered alumina and zirconia10.1016/j.dental.2009.01.093 ↗
45. The fracture resistance of all-ceramic crowns on supporting structures with different elastic moduli
46. Feedback control during mastication of solid food textures – a clinical-experimental study10.1016/S0022-3913(98)70134-9 ↗
47. A 5-year retrospective study of cobalt–chromium-based fixed dental prostheses10.11607/ijp.3024 ↗
48. Evaluation of zirconium-oxide-based ceramic single-unit posterior fixed dental prostheses (FDPs) generated with two CAD/CAM systems compared to porcelain-fused-to-metal single-unit posterior FDPs: a 5-year clinical prospective study10.1111/j.1532-849X.2011.00825.x ↗
49. Völkel · 2010
50. Six-year follow-up of titanium and high-gold porcelain-fused-to-metal fixed partial dentures10.1046/j.1365-2842.1999.00373.x ↗
51. The up to 25-year survival and clinical performance of 2340 high gold-based metal-ceramic single crowns10.11607/ijp.3136 ↗
52. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
53. Zöchbauer · 2011