journal article·2020-04

One-step ceramic primer as surface conditioner: Effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations

Kiara Serafini Dapieve, Renan Vaz Machry, Rafaela Oliveira Pilecco, Cornelis Johannes Kleverlaan, Gabriel Kalil Rocha Pereira, Andressa Borin Venturini, Luiz Felipe Valandro

Publisher page

Abstract

The aim of the study was to evaluate the effect of a ceramic primer and its increased passive application on the fatigue performance of adhesively cemented lithium disilicate simplified restorations. Ceramic discs (Ø = 10 mm; thickness = 1.0 mm) were submitted to an in-lab simulation of CAD/CAM milling and allocated into 8 groups (n = 15), considering 2 factors: "surface treatment"- PRIMER, only coupling agent application (Monobond N); HF5+PRIMER, 5% hydrofluoric acid and coupling agent; E&P 20s + 40s and E&P 20s+5min, ceramic etching/priming (Monobond Etch & Prime, E&P) for 20 s of active application followed by 40 s or 5 min of passive application, respectively; and "aging condition"- baseline, storage for 24 h to 5 days; aged, storage for 90 days +12,000 thermal cycles. Adhesive cementation (Multilink N) was performed onto epoxy discs (Ø = 10 mm; thickness = 2 mm) and the cemented assemblies were subjected to step-stress fatigue tests (initial load of 200 N; step-size of 50 N; 10,000 cycles per step; 20 Hz). The results showed that the groups had similar fatigue performance in the baseline condition (except for E&P 20s+5min: 940.0 N; 123,000 cycles > PRIMER: 786.7 N; 92,333 cycles). When aged, the PRIMER group presented the worst fatigue performance (480.8 N; 31,154 cycles) compared to the other groups (810.0-840.0 N; 97,000-103,000 cycles). In addition, only the PRIMER treatment showed unstable fatigue performance (baseline > aged). Therefore, ceramic surface treatment promoting micromechanical interlocking and chemical bonds is mandatory for stable fatigue performance of adhesively cemented lithium disilicate restorations. The one-step ceramic primer/conditioner promoted similar fatigue performance to the 5% hydrofluoric acid + coupling agent, but increased E&P etching time did not improve the fatigue behavior.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Study of thermocycling effect on the bond strength between an aluminous ceramic and a resin cement10.1590/S1678-77572005000100011 ↗
2. Tensile stress in glass-ceramic crowns: effect of flaws and cementation voids
3. Resin cements formulated with thio-urethanes can strengthen porcelain and increase bond strength to ceramics10.1016/j.jdent.2018.04.002 ↗
4. Resin-ceramic bonding: a review of the literature10.1067/mpr.2003.50 ↗
5. The effect of resin bonding on long-term success of high-strength ceramics10.1177/0022034517729134 ↗
6. Microtensile bond strength of a resin cement to feld pathic ceramic after different etching and silanization regimens in dry and aged conditions10.1016/j.dental.2006.11.011 ↗
7. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
8. Response of composite resins to preheating and the resulting strengthening of luted feldspar ceramic10.1016/j.dental.2019.07.021 ↗
9. Mechanical performance of Y-TZP monolithic ceramic after grinding and aging: survival estimates and fatigue strength10.1016/j.jmbbm.2018.07.041 ↗
10. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
11. Stability and reactivity of γ-ΜPTMS silane in some commercial primer and adhesive formulations10.1016/j.dental.2018.05.006 ↗
12. Silane reactivity and resin bond strength to lithium disilicate ceramic surfaces10.1016/j.dental.2019.05.002 ↗
13. Size and shape of the human first permanent molar: a Fourier analysis of the occlusal and equatorial outlines10.1002/(SICI)1096-8644(199903)108:3<281::AID-AJPA4>3.0.CO;2-# ↗
14. The strengthening mechanism of resin cements on porcelain surfaces10.1177/154405910608500313 ↗
15. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
16. Long term water storage deteriorates bonding of composite resin to alumina and zirconia short communication10.2174/1874210601307010123 ↗
17. Porcelain laminate veneers bonded to etched enamel
18. Simplified cementation of lithium disilicate crowns: retention with various adhesive resin cement combinations10.1016/j.prosdent.2017.07.012 ↗
19. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
20. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
21. Hydrofluoric acid burns: a review10.1016/0305-4179(95)93254-H ↗
22. Aspects of silane coupling agents and surface conditioning in dentistry: an overview10.1016/j.dental.2012.02.009 ↗
23. Survival of Dicor glass-ceramic dental restorations over 16 years. Part III. effect of luting agent and tooth or tooth-substitute core structure10.1067/mpr.2001.119415 ↗
24. Cements and adhesives for all-ceramic restorations
25. Bonding of resin composites to etchable ceramic surfaces – an insight review of the chemical aspects on surface conditioning10.1111/j.1365-2842.2005.01569.x ↗
26. Silane adhesion mechanism in dental applications and surface treatments: a review10.1016/j.dental.2017.09.002 ↗
27. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns: multi-physics FEA modeling and monotonic testing10.1016/j.dental.2012.04.033 ↗
28. Physicochemical and morphological characterization of a glass ceramic treated with different ceramic primers and post-silanization protocols10.1016/j.dental.2019.05.003 ↗
29. Survival rate of resin and ceramic inlays, onlays, and overlays: a systematic review and meta-analysis10.1177/0022034516652848 ↗
30. Possible hazardous effects of hydrofluoric acid and recommendations for treatment approach: a review10.1007/s00784-011-0636-6 ↗
31. Bonding of restorative materials to dentin with various luting agents10.2341/10-236-L ↗
32. How does hydrofluoric acid etching affect the cyclic load-to-failure of lithium disilicate restorations?10.1016/j.jmbbm.2018.07.040 ↗
33. Effect of hydrofluoric acid concentration and etching time on bond strength to lithium disilicate glass ceramic10.2341/16-215-L ↗
34. Internal adjustments decrease the fatigue failure load of bonded simplified lithium disilicate restorations10.1016/j.dental.2018.05.015 ↗
35. Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: conventional ceramic etching vs etch & prime one-step primer10.1016/j.dental.2018.04.012 ↗
36. CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: fatigue performance and ceramic surface characteristics10.1016/j.jmbbm.2019.03.005 ↗
37. Early clinical performance of resin cements in glass-ceramic posterior restorations in adult vital teeth: a systematic review and meta-analysis
38. Ceramic strengthening by tuning the elastic moduli of resin-based luting agents10.1016/j.dental.2017.01.002 ↗
39. Strengthening of porcelain provided by resin cements and flowable composites10.2341/15-025-L ↗
40. Fatigue failure load of resin-bonded simplified lithium disilicate glass-ceramic restorations: effect of ceramic conditioning methods
41. Silanes and metal pretreatments
42. Aspects of adhesion tests on resin-glass ceramic bonding10.1016/j.dental.2017.06.013 ↗
43. Effect of etching time and resin bond on the flexural strength of IPS e.max Press glass ceramic10.1016/j.dental.2014.08.373 ↗
44. Effect of hydrofluoric acid etching duration on the roughness and flexural strength of a lithium disilicate-based glass ceramic10.1590/S0103-64402011000100008 ↗