Improving stress corrosion cracking behavior of AZ31 alloy with conformal thin titania and zirconia coatings for biomedical applications

M. Peron, A. Bin Afif, A.L. Dadlani, F. Berto, J. Torgersen

Abstract

Magnesium and its alloys have been widely studied as materials for temporary implant devices. However, corrosion-assisted cracking phenomena such as stress corrosion cracking (SCC) continue to prevent their mainstream use. For the first time, we explore the SCC susceptibility of Atomic Layer Deposition (ALD) coated AZ31 alloys in Simulated Body Fluid (SBF). Conformal 100 nm coatings of titania and zirconia were deposited on standard dogbone specimens and subjected to slow strain rate tests at 3.5 10-6 s-1 and a temperature of 37 °C. Remarkably, the SCC susceptibility index IUTS was reduced by 6% and 40% and the Iε was reduced by more than 70% and 76% with a titania and zirconia coating, respectively. Potentiodynamic polarization, hydrogen evolution and fracture behavior of the samples revealed the drastic corrosion reduction to be the main reason for the susceptibility reduction. We discuss the observed SCC behavior of our samples in light of the coatings’ electrochemical activities, wettabilities, surface integrities and mechanical properties. This straightforward conformal surface treatment can be useful as a workaround for one of the major bottlenecks of biomedical Mg based implants and hence provides a possible pathway for making them more commonplace in the field.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Titanium Alloys Microstructure and Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (84)

Show source-provided references
1. Effects of microstructure on the short fatigue crack initiation and propagation characteristics of biomedical α/β titanium alloys10.1007/s11661-000-0222-z ↗
2. The effect of wettability on corrosion resistance of oxide films produced by SILAR method on magnesium, aluminum and copper substrates10.1016/j.surfcoat.2016.03.011 ↗
3. Corrosion fatigue of biomedical metallic alloys: mechanisms and mitigation10.1016/j.actbio.2011.09.012 ↗
4. ASTM International, ASTM-E466-96
5. The pathology of total joint arthroplasty.II. Mechanisms of implant failure10.1007/s002560050552 ↗
6. Microbially-influenced corrosion: damage to prostheses, delight for bacteria10.1177/039139880602900415 ↗
7. Stress corrosion cracking of rare-earth containing magnesium alloys ZE41, QE22 and Elektron 21 (EV31A) compared with AZ8010.1016/j.msea.2007.07.070 ↗
8. Biocorrosion properties of Ti–3Cu alloy in F ion-containing solution and acidic solution and biocompatibility10.1007/s12598-019-01202-9 ↗
9. Photochemical atomic layer deposition and etching10.1016/j.surfcoat.2016.02.046 ↗
10. Influence of a MAO + PLGA coating on biocorrosion and stress corrosion cracking behavior of a magnesium alloy in a physiological environment10.1016/j.corsci.2018.12.005 ↗
11. In-vitro characterization of stress corrosion cracking of aluminium-free magnesium alloys for temporary bio-implant applications10.1016/j.msec.2014.06.018 ↗
12. (Christoph) Leyens · 2003
13. Conformality in atomic layer deposition: current status overview of analysis and modelling10.1063/1.5060967 ↗
14. Zirconia and its biomedical applications
15. Mechanical compatibility of noncemented hip prostheses with the human femur10.1016/S0883-5403(06)80102-6 ↗
16. The influence of stem size and extent of porous coating on femoral bone resorption after primary cementless hip arthroplasty10.1097/00003086-198806000-00002 ↗
17. Calcium phosphate cements as bone drug delivery systems: a review10.1016/j.jconrel.2006.04.007 ↗
18. Wettability and surface free energy of zirconia ceramics and their constituents10.1023/A:1004767914895 ↗
19. Atomic layer deposition for biosensing applications10.1016/j.bios.2018.09.038 ↗
20. Design strategy for new biodegradable Mg–Y–Zn alloys for medical applications10.3139/146.110157 ↗
21. H. Harianawala, M. Kheur, S. Kheur, T. Sethi, A. Bal, M. Burhanpurwala, F. Sayed, Biocompatibility of Zirconia, n.d.
22. Thermal expansion coefficient of yttria stabilized zirconia for various yttria contents10.1016/j.ssi.2004.08.021 ↗
23. In vitro corrosion behavior of Ti-O film deposited on fluoride-treated Mg–Zn–Y–Nd alloy10.1016/j.apsusc.2011.11.116 ↗
24. http://share.iofbonehealth.org/EU-6-Material/Reports/IOF%20Report_EU.pdf, (n.d). http://share.iofbonehealth.org/EU-6-Material/Reports/IOF Report_EU.pdf (accessed November 20, 2019).
25. Construction of TiO2/silane nanofilm on AZ31 magnesium alloy for controlled degradability and enhanced biocompatibility10.1007/s12598-018-1187-7 ↗
26. Thermal expansion of anatase and rutile between 300 and 575 K using synchrotron powder X-ray diffraction10.1154/1.2790965 ↗
27. Relationship between interfacial reaction and adhesion at PVD TiO2 film-metal (Ti or Al) interfaces10.1016/0257-8972(93)90231-C ↗
28. Corrosion of metal orthopaedic implants10.2106/00004623-199802000-00015 ↗
29. Metal degradation products: a cause for concern in metal-metal bearings?10.1097/01.blo.0000096810.78689.62 ↗
30. A review of stress-corrosion cracking and corrosion fatigue of magnesium alloys for biodegradable implant applications10.1007/s11837-015-1366-z ↗
31. Stress corrosion cracking and corrosion fatigue characterisation of MgZn1Ca0.3 (ZX10) in a simulated physiological environment10.1016/j.jmbbm.2016.09.033 ↗
32. Stress corrosion cracking of an extruded magnesium alloy (ZK21) in a simulated body fluid10.1016/j.engfracmech.2018.09.002 ↗
33. In vitro degradation and mechanical integrity of calcium-containing magnesium alloys in modified-simulated body fluid10.1016/j.biomaterials.2008.02.003 ↗
34. Apatite formation on TiO2 in simulated body fluid10.1016/S0022-0248(01)01782-1 ↗
35. Correlation between pre-operative periprosthetic bone density and post-operative bone loss in THA can be explained by strain-adaptive remodelling10.1016/S0021-9290(99)00041-X ↗
36. Effect of target density and its morphology on TiO2 thin films grown on Si(100) by PLD10.1016/S0169-4332(99)00269-X ↗
37. How useful is SBF in predicting in vivo bone bioactivity?10.1016/j.biomaterials.2006.01.017 ↗
38. Anodic electrodeposition of MgO coatings to improve corrosion resistance in vivo
39. Sol-gel coatings to improve the corrosion resistance of magnesium (Mg) alloys
40. Influence of surface morphology on corrosion and electronic behavior10.1016/j.actamat.2005.09.017 ↗
41. Corrosion behavior of the composite ceramic coating containing zirconium oxides on AM30 magnesium alloy by plasma electrolytic oxidation10.1016/j.corsci.2011.07.037 ↗
42. A combined coating strategy based on atomic layer deposition for enhancement of corrosion resistance of AZ31 magnesium alloy10.1016/j.apsusc.2017.11.032 ↗
43. Improvement to the corrosion resistance of Ti-based implants using hydrothermally synthesized nanostructured anatase coatings10.3390/ma7010180 ↗
44. Chemical and electrochemical characterization of TiO2/Al2O3 atomic layer depositions on AZ-31 magnesium alloy10.1007/s11998-011-9372-8 ↗
45. Reversible wettability control of TiO2 surface by light irradiation10.1016/S0039-6028(02)01551-0 ↗
46. Hydroxyapatite coating containing multi-walled carbon nanotubes on AZ31 magnesium: mechanical-electrochemical degradation in a physiological environment10.1016/j.ceramint.2018.02.015 ↗
47. Properties of TiO 2 thin films deposited by rf reactive magnetron sputtering on biased substrates10.1016/j.apsusc.2016.08.125 ↗
48. Electrochemical estimation of the corrosion rate of magnesium/aluminium alloys10.1155/2010/953850 ↗
49. Mg and its alloys for biomedical applications: exploring corrosion and its interplay with mechanical failure10.3390/met7070252 ↗
50. Effect of Zirconia ALD coating on stress corrosion cracking of AZ31 alloy in simulated body fluid
51. Stress corrosion cracking behavior of zirconia ALD–coated AZ31 alloy in simulated body fluid
52. Enhancement of stress corrosion cracking of AZ31 magnesium alloy in simulated body fluid thanks to cryogenic machining10.1016/j.jmbbm.2019.103429 ↗
53. Peron · 2020
54. The effect of Equal Channel Angular Pressing on the stress corrosion cracking susceptibility of AZ31 alloy in simulated body fluid10.1016/j.jmbbm.2020.103724 ↗
55. Comparing physiologically relevant corrosion performances of Mg AZ31 alloy protected by ALD and sputter coated TiO210.1016/j.surfcoat.2020.125922 ↗
56. Corrosion behavior of metallic materials in biomedical applications
57. Corrosion behavior of metallic materials in biomedical applications
58. Comparison of degradation behavior and the associated bone response of ZK60 and PLLA in vivo10.1002/jbm.a.34795 ↗
59. Role of chlorides on pitting and hydrogen embrittlement of Mg–Mn wrought alloy10.1016/j.corsci.2013.05.030 ↗
60. L. Rimondini, L. Cerroni, A. Carrassi, P. Torricelli, Bacterial colonization of zirconia ceramic surfaces: an in vitro and in vivo study., Int. J. Oral Maxillofac. Implants 17 (n.d.)793–8. http://www.ncbi.nlm.nih.gov/pubmed/12507238 (accessed January 23, 2020).
61. Corrosion fatigue fracture of magnesium alloys in bioimplant applications: a review10.1016/j.engfracmech.2014.08.009 ↗
62. Comparing cold spray with thermal spray coating technologies
63. Control of biodegradation of biocompatable magnesium alloys10.1016/j.corsci.2007.01.001 ↗
64. An hydrogen evolution method for the estimation of the corrosion rate of magnesium alloys
65. Polymers in oral insulin delivery
66. Characterisation of anodic oxide films on zirconium formed in sulphuric acid: XPS and corrosion resistance investigations10.1007/s10008-016-3369-2 ↗
67. Magnesium and its alloys as orthopedic biomaterials: a review10.1016/j.biomaterials.2005.10.003 ↗
68. Environmentally-induced cracking of magnesium10.1016/0010-938X(84)90017-9 ↗
69. Determinants of stress shielding: design versus materials versus interface
70. Fatigue of biomaterials: a review10.1016/S0142-1123(00)00052-9 ↗
71. Comparison of the corrosion behaviour of AZ31B magnesium alloy under immersion test and potentiodynamic polarization test in NaCl solution10.1016/j.jma.2014.01.004 ↗
72. Cohesive energy, properties, and formation energy of transition metal alloys10.1007/s11106-008-0006-3 ↗
73. Maintenance of proximal cortical bone with use of a less stiff femoral component in hemiarthroplasty of the hip without cement. An investigation in a canine model at six months and two years10.2106/00004623-199709000-00013 ↗
74. APATITE-FORMING ability OF titania gels with different structures
75. The mechanism of bone remodeling and resorption around press-fitted THA stems10.1016/0021-9290(93)90001-U ↗
76. Bioactive titania gel layers formed by chemical treatment of Ti substrate with a H2O2/HCl solution10.1016/S0142-9612(01)00254-X ↗
77. Biodegradable magnesium‐based implants in orthopedics—a general review and perspectives10.1002/advs.201902443 ↗
78. A critical review of the Stress Corrosion Cracking (SCC) of magnesium alloys10.1002/adem.200500071 ↗
79. Stress corrosion cracking in magnesium alloys: characterization and prevention10.1007/s11837-007-0104-6 ↗
80. Wolff · 1986
81. Hot forming characteristics of magnesium alloy AZ31 and three-dimensional FE modeling and simulation of the hot splitting spinning process
82. Atomic layer deposited ZrO2 nanofilm on Mg-Sr alloy for enhanced corrosion resistance and biocompatibility10.1016/j.actbio.2017.06.015 ↗
83. Preparation, microstructure and photocatalytic activity of the porous TiO2 anatase coating by sol-gel processing10.1023/A:1008703719929 ↗
84. Vitro study on Mg–Sn–Mn alloy as biodegradable metals10.1016/j.jmst.2014.04.005 ↗