Grinding, polishing and glazing of the occlusal surface do not affect the load-bearing capacity under fatigue and survival rates of bonded monolithic fully-stabilized zirconia simplified restorations
Source abstract
Abstract
This study aims to evaluate the effect of distinct surface treatments (grinding, polishing and glaze) of the occlusal surface of fully-stabilized zirconia (FSZ) simplified restorations bonded onto epoxy resin on the fatigue behavior of the restorations. Disc shaped specimens of FSZ (IPS e.max Zircad MT Multi) were produced (Ø = 10 mm and 0.8 mm in thickness) and randomly allocated into 5 groups, considering the factor 'surface treatment' of the occlusal surface: Ctrl - as-sintered; Gr - ground with coarse diamond bur; Gr + Pol- grinding + polishing with two-step polishing system; Gr + Gl - grinding + glaze application; Gr + Pol + Gl - grinding + polishing + glaze application. Next, the FSZ intaglio surface was air-abraded with 45 μm aluminum oxide powder for 10 s at 15 mm of distance under 2 bar pressure and the discs were adhesively cemented (Multilink Automix) onto its dentin analogue pair (Ø = 10 mm; thickness = 2.7 mm). Finally, the step-stress fatigue test was executed (load ranging from 200 to 1300 N; step-size of 100N; 10,000 cycles per step, 20 Hz). In addition, surface topography, roughness, phase transformation and fractography analyses were performed. Grinding altered the topographical pattern introducing defects into the material surface and increasing roughness. Polishing and glaze application led to a smoothening effect, reducing surface defects and statistically decreasing roughness. However, the effect on roughness of polishing and glaze was statistically similar. No phase transformation was observed, thus only cubic and tetragonal phases were detected. No surface treatment had a deleterious effect regarding the fatigue failure load, number of cycles for failure and survival rates. All failures (cracks) started on the bonding surface. Thus, polishing and glaze are indicated to reduce surface roughness, despite not leading to differences in terms of fatigue performance.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Temporomandibular Joint Disorders
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Resin elasticity and the strengthening of all-ceramic restorations10.1177/154405910708600606 ↗
2. Tensile stress in glass-ceramic crowns: effect of flaws and cementation voids
3. Does air particle abrasion affect the flexural strength and phase transformation of Y-TZP? A systematic review and meta-analysis10.1016/j.dental.2016.03.021 ↗
4. Two-body wear performance of dental colored zirconia after different surface treatments10.1016/j.prosdent.2016.02.006 ↗
5. Flexural strength and failure modes of layered ceramic structures10.1016/j.dental.2011.09.008 ↗
6. FEM and von mises analysis on prosthetic crowns structural elements: evaluation of different applied materials
7. Effect of finishing and polishing on the surface roughness and gloss of feldspathic ceramic for chairside CAD/CAM systems10.2341/15-174-L ↗
8. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
9. Microstructural analysis and reliability of monolithic zirconia after simulated adjustment simulation protocols10.1016/j.dental.2017.04.024 ↗
10. Collins · 1993
11. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
12. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
13. Does finishing and polishing of restorative materials affect bacterial adhesion and biofilm formation? A systematic review10.2341/17-073-L ↗
14. Influence of cooling rate on zirconia/veneer interfacial adhesion10.1016/j.actbio.2010.06.026 ↗
15. Surface micro-morphology, phase transformation, and mechanical reliability of ground and aged monolithic zirconia ceramic10.1016/j.jmbbm.2016.10.008 ↗
16. Surface roughness of zirconia for full-contour crowns after clinically simulated grinding and polishing10.1038/ijos.2014.34 ↗
17. Aging resistance of surface-treated dental zirconia10.1016/j.dental.2014.11.018 ↗
18. Crystallographic and morphological analysis of sandblasted highly translucent dental zirconia10.1016/j.dental.2017.12.008 ↗
19. ISO 6872 · 2015
20. ISO 4287 · 1997
21. Fracture surface analysis of dental ceramics; clinically failed restorations
22. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
23. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
24. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
25. Effects of surface treatments on the translucency, opalescence, and surface texture of dental monolithic zirconia ceramics10.1016/j.prosdent.2015.11.020 ↗
26. Effect of different grinding burs on the physical properties of zirconia10.4047/jap.2016.8.2.137 ↗
27. Effects of two surface finishes on the color of cemented and colored anatomic-contour zirconia crowns10.1016/j.prosdent.2015.12.012 ↗
28. Effects of different surface finishing protocols for zirconia on surface roughness and bacterial biofilm formation10.4047/jap.2019.11.1.41 ↗
29. Effect of glaze cooling rate on mechanical properties of conventional and pressed porcelain on zirconia10.1590/0103-6440201600709 ↗
30. Influence of the resin cement thickness on the fatigue failure loads of CAD/CAM feldspathic crowns10.1016/j.dental.2015.04.019 ↗
31. Effect of coarse grinding, overglazing, and 2 polishing systems on the flexural strength, surface roughness, and phase transformation of yttrium-stabilized tetragonal zirconia
32. Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: effect of ceramic thickness10.1016/j.dental.2018.03.004 ↗
33. Effects of opaque and porcelain surface texture on the color of ceramometal restorations
34. Clinically relevant fracture testing of all-ceramic crowns10.1016/j.dental.2013.04.026 ↗
35. Fractographic features of glass ceramic and zirconia-based dental restorations fractured during clinical function10.1111/eos.12127 ↗
36. The effect of a layer of resin luting agent on the biaxial flexure strength of two all-ceramic systems10.1016/j.prosdent.2005.02.012 ↗
37. Effect of grinding with diamond-disc and-bur on the mechanical behavior of a Y-TZP ceramic10.1016/j.jmbbm.2014.05.010 ↗
38. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
39. Lithium disilicate glass-ceramic vs translucent zirconia polycrystals bonded to distinct substrates: fatigue failure load, number of cycles for failure, survival rates, and stress distribution10.1016/j.jmbbm.2018.12.010 ↗
40. Mechanical behavior of yttria-stabilized tetragonal zirconia polycrystalline ceramic after different zirconia surface treatments10.1016/j.msec.2017.03.299 ↗
41. Wear performance of dental ceramics after grinding and polishing treatments10.1016/j.jmbbm.2012.03.002 ↗
42. Surface properties of monolithic zirconia after dental adjustment treatments and in vitro wear10.1016/j.jdent.2014.08.011 ↗
43. Hydrofluoric acid concentrations: effect on the cyclic load to failure of machined lithium disilicate restorations10.1016/j.dental.2018.06.028 ↗
44. Internal adjustments decrease the fatigue failure load of bonded simplified lithium disilicate restorations10.1016/j.dental.2018.05.015 ↗
45. Three generations of zirconia: from veneered to monolithic. Part I
46. Effect of different treatments on the flexural strength of fully versus partially stabilized monolithic zirconia10.1016/j.prosdent.2016.10.031 ↗
47. Fatigue failure load of feldspathic ceramic crowns after hydrofluoric acid etching at different concentrations
48. Effect of finishing and polishing on roughness and gloss of lithium disilicate and lithium silicate zirconia reinforced glass ceramic for CAD/CAM systems10.2341/16-381-L ↗
49. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
50. Influence of finishing/polishing on the fatigue strength, surface topography, and roughness of an yttrium-stabilized tetragonal zirconia polycrystals subjected to grinding10.1016/j.jmbbm.2019.02.013 ↗
51. Polishing of ground Y-TZP ceramic is mandatory for improving the mechanical behavior.10.1590/0103-6440201802044 ↗
52. Load-bearing capacity under fatigue and survival rates of adhesively cemented yttrium-stabilized zirconia polycrystal monolithic simplified restorations10.1016/j.jmbbm.2018.11.009 ↗