Abstract

Total hip replacement is the most effective treatment for late stage osteoarthritis. However, adverse local tissue reactions (ALTRs) have been observed in patients with modular total hip implants. Although the detailed mechanisms of ALTRs are still unknown, fretting corrosion and the associated metal ion release from the CoCrMo femoral head at the modular junction has been reported to be a major factor. The purpose of this study is to increase the fretting corrosion resistance of the CoCrMo alloy and the associated metal ion release by applying hard coatings to the surface. Cathodic arc evaporation technique (arc-PVD) was used to deposit TiSiN and ZrN hard coatings on CoCrMo substrates. The morphology, chemical composition, crystal structures and residual stress of the coatings were characterized by scanning electron microscopy, energy dispersive X-ray spectroscopy, and X-ray diffractometry. Hardness, elastic modulus, and adhesion of the coatings were measured by nano-indentation, nano-scratch test, and the Rockwell C test. Fretting corrosion resistance tests of coated and uncoated CoCrMo discs against Ti6Al4V spheres were conducted on a four-station fretting testing machine in simulated body fluid at 1Hz for 1 million cycles. Post-fretting samples were analyzed for morphological changes, volume loss and metal ion release. Our analyses showed better surface finish and lower residual stress for ZrN coating, but higher hardness and better scratch resistance for TiSiN coating. Fretting results demonstrated substantial improvement in fretting corrosion resistance of CoCrMo with both coatings. ZrN and TiSiN decreased fretting volume loss by more than 10 times and 1000 times, respectively. Both coatings showed close to 90% decrease of Co ion release during fretting corrosion tests. Our results suggest that hard coating deposition on CoCrMo alloy can significantly improve its fretting corrosion resistance and could thus potentially alleviate ALTRs in metal hip implants.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (81)

Show source-provided references
1. Influence of Ti–TiN multilayer PVD-coatings design on residual stresses and adhesion10.1016/j.matdes.2015.03.007 ↗
2. Nanocomposite Ti-Si-N coatings deposited by reactive dc magnetron sputtering for biomedical applications10.1111/j.1551-2916.2011.05029.x ↗
3. Trunnion corrosion: what surgeons need to know in 201810.1302/0301-620X.100B1.BJJ-2017-0569.R1 ↗
4. Characterization of multi-principal-element (TiZrNbHfTa)N and (TiZrNbHfTa)C coatings for biomedical applications10.1016/j.jmbbm.2012.02.020 ↗
5. Fretting corrosion accelerates crevice corrosion of modular hip tapers10.1002/jab.770060104 ↗
6. Budynas · 2011 · 122
7. Influence of bias voltages on the structure and wear properties of TiSiN coating synthesized by cathodic arc plasma evaporation10.1016/j.tsf.2007.07.087 ↗
8. Mechanical and tribological properties of nanocomposite TiSiN coatings10.1016/j.surfcoat.2009.11.034 ↗
9. Corrosion resistance of ZrN films on AISI 304 stainless steel substrate10.1016/S0257-8972(02)00882-4 ↗
10. Corrosion between the components of modular femoral hip prostheses10.1302/0301-620X.74B4.1624507 ↗
11. Corrosion at the head-neck taper as a cause for adverse local tissue reactions after total hip arthroplasty10.2106/JBJS.K.01352 ↗
12. Adverse local tissue reaction arising from corrosion at the femoral neck-body junction in a dual-taper stem with a cobalt-chromium modular neck10.2106/JBJS.L.01042 ↗
13. Improvement of CoCr alloy characteristics by Ti-based carbonitride coatings used in orthopedic applications
14. Improving the properties of titanium nitride by incorporation of silicon10.1016/S0257-8972(98)00560-X ↗
15. Characteristics of different cathodic arc deposition coatings on CoCrMo for biomedical applications10.1016/j.jmbbm.2019.04.026 ↗
16. Adverse reactions to metal on polyethylene implants: highly destructive lesions related to elevated concentration of cobalt and chromium in synovial fluid10.1002/jbm.a.36057 ↗
17. Mechanisms of adverse local tissue reactions to hip implants10.3389/fbioe.2019.00176 ↗
18. A computational approach to fretting wear prediction at the head-stem taper junction of total hip replacements10.1016/j.wear.2015.06.016 ↗
19. The effect of N, C, Cr, and Nb content on silicon nitride coatings for joint applications10.3390/ma13081896 ↗
20. Serum metal levels for diagnosis of adverse local tissue reactions secondary to corrosion in metal-on-polyethylene total hip arthroplasty10.1016/j.arth.2017.04.016 ↗
21. A mechanistic understanding of the wear coefficient: from single to multiple asperities contact10.1016/j.jmps.2018.02.015 ↗
22. Tribological study of TiN monolayer and TiN/CrN (multilayer and superlattice) on Co–Cr alloy10.1016/j.wear.2015.02.010 ↗
23. Biotribological study of multi-nano-layers as a coating for total hip prostheses10.1016/j.wear.2016.12.043 ↗
24. Fretting-corrosion of materials used as orthopaedic implants10.1016/j.wear.2004.11.027 ↗
25. In vivo corrosion of modular hip prosthesis components in mixed and similar metal combinations. The effect of crevice, stress, motion, and alloy coupling10.1002/jbm.820271210 ↗
26. Intergranular corrosion-fatigue failure of cobalt-alloy femoral stems. A failure analysis of two implants10.2106/00004623-199401000-00014 ↗
27. Corrosion at the neck-stem junction as a cause of metal ion release and pseudortumour formation10.1302/0301-620X.94B7.29122 ↗
28. An ASTM standard for quantitative scratch adhesion testing of thin, hard ceramic coatings10.1111/j.1744-7402.2005.02043.x ↗
29. Corrosion protection of titanium by deposition of niobium thin films10.1016/S0257-8972(99)00321-7 ↗
30. Deposition of TiSiN coatings by arc ion plating process10.1016/j.apsusc.2007.10.079 ↗
31. Orthopedic implant fretting corrosion10.1515/CORRREV.2003.21.2-3.183 ↗
32. Wear analysis of a retrieved hip implant with titanium nitride coating10.1016/S0883-5403(97)90164-9 ↗
33. He · 2009 · 249
34. The fretting corrosion resistance of PVD surface-modified orthopedic implant alloys10.1002/1097-4636(2001)58:2<156::AID-JBM1002>3.0.CO;2-H ↗
35. Development of superlattice CrN/NbN coatings for joint replacements deposited by high power impulse magnetron sputtering10.1007/s10856-016-5751-0 ↗
36. Presence of corrosion products and hypersensitivity-associated reactions in periprosthetic tissue after aseptic loosening of total hip replacements with metal bearing surfaces10.1016/j.actbio.2008.07.032 ↗
37. Wear and corrosion protection of 316-L femoral implants by deposition of thin films10.1016/S0257-8972(01)01321-4 ↗
38. The individual and socioeconomic impact of osteoarthritis10.1038/nrrheum.2014.44 ↗
39. Properties of superhard nc-TiN/a-BN and nc-TiN/a-BN/a-TiB2 nanocomposite coatings prepared by plasma induced chemical vapor deposition10.1016/j.surfcoat.2005.01.003 ↗
40. How useful is SBF in predicting in vivo bone activity?10.1016/j.biomaterials.2006.01.017 ↗
41. Corrosion of a hip stem with a modular neck taper junction: a retrieval study of 16 cases10.1016/j.arth.2008.09.009 ↗
42. Retrieval analysis of titanium nitride (TiN) coated prosthetic femoral heads articulating with polyethylene10.1016/j.jmbbm.2015.10.012 ↗
43. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
44. CoCrMo surface modifications affect biocompatibility, adhesion, and inflammation in human osteoblasts10.1038/s41598-020-58742-9 ↗
45. An introduction to thin film processing using high-power impulse magnetron sputtering10.1557/jmr.2012.8 ↗
46. Comparative study of the tribological behaviour of superhard nanocomposite coatings nc-TiN/a-Si3N4 with TiN10.1016/j.surfcoat.2004.05.007 ↗
47. Adverse reactions to metal debris occur with all types of hip replacement not just metal-on-metal hips: a retrospective observational study of 3340 revisions for adverse reactions to metal debris from the National Joint Registry for England, Wales, Northe10.1186/s12891-016-1329-8 ↗
48. Corrosion of modular hip prostheses10.1302/0301-620X.73B4.2071637 ↗
49. Improvement of the tribological behaviour of PVD nanostratified TiN/CrN coatings — an explanation10.1016/j.surfcoat.2006.08.013 ↗
50. Why does titanium alloy wear cobalt chrome alloy despite lower bulk hardness: a nanoindentation study?10.1016/j.tsf.2013.06.020 ↗
51. Relationships between hardness, Young's modulus and elastic recovery in hard nanocomposite coatings10.1016/S0257-8972(01)01714-5 ↗
52. Corrosion and fretting corrosion studies of medical grade CoCrMo alloy in a clinically relevant simulated body fluid environment10.1007/s11661-015-2834-3 ↗
53. Intergranular pitting corrosion of CoCrMo biomedical implant alloy10.1002/jbm.b.33067 ↗
54. Trunnionosis: a pain in the neck10.5312/wjo.v4.i4.161 ↗
55. Mechanical and tribological behavior of silicon nitride and silicon carbon nitride coatings for total joint replacements10.1016/j.jmbbm.2013.05.002 ↗
56. Atypical pseudotumour after metal-on-polyethylene total hip arthroplasty causing deep venous thrombosis10.5301/HIP.2011.8839 ↗
58. Corrosion resistance of Ti–6Al–4V alloy with nitride coatings in Ringer's solution10.1016/j.corsci.2012.10.005 ↗
59. CoCrMo alloys ions release behavior by TiNbN coating: an in vitro study10.1007/s10544-019-0417-6 ↗
60. Chromium (III) hydrolysis constants and solubility of chromium(III) hydroxide10.1021/ic00250a002 ↗
61. Chromium(III) hydroxide solubility in the aqueous Na-OH-H2PO4-HPO4-PO4-H2O system: a thermodynamic model10.1007/s10953-004-7137-z ↗
62. High power pulsed magnetron sputtering: a review on scientific and engineering state of the art10.1016/j.surfcoat.2009.11.013 ↗
63. Increased blood cobalt and chromium after total hip replacement10.1081/CLT-100102463 ↗
64. Biocompatibility and corrosion resistance in biological media of hard ceramic coatings sputter deposited on metal implants10.1016/0921-5093(91)90595-E ↗
65. Trunnionosis: the latest culprit in adverse reactions to metal debris following hip arthroplasty10.1007/s00256-014-1978-3 ↗
66. Nano‐adhesion and friction of multi‐asperity contact: a molecular dynamics simulation study10.1002/sia.5797 ↗
67. Influence of substrate heating and nitrogen flow on the composition, morphological and mechanical properties of SiNx coatings aimed for joint replacements10.3390/ma10020173 ↗
68. A comparative study of titanium nitride (TiN), titanium oxy nitride (TiON) and titanium aluminum nitride (TiAlN), as surface coatings for bio implants10.1016/j.surfcoat.2011.05.004 ↗
69. Microabrasion–corrosion of cast CoCrMo alloy in simulated body fluids10.1016/j.triboint.2008.05.005 ↗
70. Fretting corrosion of CoCrMo and Ti6Al4V interfaces10.1016/j.biomaterials.2012.04.015 ↗
71. Comparison of diamond‐like‐carbon and alumina‐oxide articulating with polyethylene in total hip arthroplasty
72. 1991
73. Electrical properties of high-temperature oxides, borides, carbides, and nitrides10.1007/BF00351591 ↗
74. CoCrMo metal release in metal-on- highly crosslinked polyethylene hip implants10.1002/jbm.b.34470 ↗
75. Adverse local tissue reactions in metal-on-polyethylene total hip arthroplasty due to trunnion corrosion: the risk of misdiagnosis10.1302/0301-620X.97B8.34682 ↗
76. Structure, electrical and chemical properties of zirconium nitride films deposited by dc reactive magnetron sputtering10.1007/s003390050522 ↗
77. Corrosion behavior of ZrN/Zr coated biomedical AZ91 magnesium alloy10.1016/j.surfcoat.2009.02.074 ↗
78. Mechanical properties of nano-structured Ti-Si-N films synthesized by cathodic arc evaporation10.1016/j.jallcom.2006.12.124 ↗
79. Mechanical and tribological properties of multilayered TiSiN/CrN coatings synthesized by a cathodic arc deposition process10.1016/j.surfcoat.2007.09.004 ↗
80. Canadian Institute for Health Information, 2018. Hip and Knee Replacements in Canada, 2016-2017 Canadian Joint Replacement Registry Annual Report. https://secure.cihi.ca/free_products/cjrr-annual-report-2018-en.pdf. (Accessed 6 June 2019).
81. National Joint Registry for England, 2018. Wales, Northern Ireland and the Isle of Man. National joint Registry 15th annual report . https://www.hqip.org.uk/wp-content/uploads/2018/11/NJR-15th-Annual-Report-2018.pdf, 2018s , 6 June 2019.