Effect of tribochemical silica coating or multipurpose products on bonding performance of a CAD/CAM resin-based material
Source abstract
Abstract
Objectives Nanocomposite ceramics have been widely used in clinical practice; however, a standard, recommended bonding protocol has not been determined yet. The present study aimed to evaluate application of tribochemical silica coating or multipurpose products on bonding performance of a CAD/CAM resin-based material (known as nanocomposite ceramic). Materials and methods Nanocomposite ceramic specimens were fabricated and assigned into 11 groups to build bonded specimens (n = 15) according to surface treatments (none; air particle abrasion with 50-μm alumina followed by application of a silane coupling agent or a universal adhesive; tribochemical silica coating followed by application of a silane coupling agent or a universal adhesive) and resin luting cements (conventional resin cement, RelyX Veneer; self-adhesive resin cement RelyX Unicem) used. Micro-shear bond strength (μ-SBS) was measured after 24-h water storage or ageing with 10,000 thermocycles plus additional 90-d water storage. Surface roughness after alumina air abrasion and tribochemical silica coating were determined using a profilometer. Surface morphology and element variation were observed by using a scanning electron microscope (SEM)/energy dispersion spectrum (EDS). X-ray photoelectron spectroscopy (XPS) was used to characterize nanocomposite ceramic powders conditioned with silane coupling agent or the universal adhesive used in the μ-SBS test. The nanocomposite ceramic plates received alumina air abrasion, tribochemical silica coating, or without, were determined using X-ray diffraction (XRD). Results Nanocomposite ceramic treated with alumina air abrasion achieved the highest surface roughness, followed by those treated with tribochemical silica coating. Newly formed Si-O-Si bonds on the nanocomposite ceramic surface were detected by XPS after treatment with silane coupling agent or universal adhesive, and a Zr-O-P bond was detected after treating with universal adhesive. μ-SBS was significantly affected by bond strategies and ageing. Ageing by thermocycling and water storage significantly decreased μ-SBS. μ-SBS values derived by use of a universal adhesive or self-adhesive resin cement alone were no lower than the values derived by use of a silane coupling agent alone. Pre-silanization further enhanced the bonding improvement of universal adhesive or self-adhesive resin cement. However, tribochemical silica coating failed to provide higher μ-SBS compared with alumina air abrasion. XRD detected no monoclinic zirconia phase after alumina air abrasion or tribochemical silica coating, suggesting that these two roughening methods did not lead to phase transformation of zirconia fillers. Conclusions Combination of presilanization and universal adhesives improve resin bonding of nanocomposite ceramics. Tribochemical silica coating is not superior to alumina air abrasion for pretreated nanocomposite ceramics.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Bonding to zirconia using a new surface treatment10.1111/j.1532-849X.2010.00575.x ↗
2. Characterization of the adsorption of omega-(thiophene-3-yl alkyl) phosphonic acid on metal oxides with AR-XPS10.1007/s00216-004-2634-x ↗
3. An investigation into the role of core porcelain thickness and lamination in determining the flexural strength of in‐ceram dental materials10.1111/j.1532-849X.2011.00707.x ↗
4. Wettability of silane-treated glass slides as determined from x-ray photoelectron spectroscopy10.1006/jcis.1995.9942 ↗
5. Can the application of multi-mode adhesive be a substitute to silicatized/silanized Y-TZP ceramics?10.1590/0103-6440201801862 ↗
6. Effect of different surface treatments on bond strength of resin cement to a CAD/CAM restorative material
7. Shear bond strength of different luting cements to an aluminum oxide containing glass ceramic core material10.1016/j.dental.2003.10.011 ↗
8. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
9. Effect of dentin surface modification on the microtensile bond strength of self-adhesive resin cements10.1111/j.1532-849X.2012.00890.x ↗
10. Effects of silane coupling agents and solutions of different polarity on pmma bonding to alumina10.4012/dmj.2012-040 ↗
11. Bonding of primed zirconia ceramics: evidence of chemical bonding and improved bond strengths
12. The effects of water on degradation of the zirconia-resin bond10.1016/j.jdent.2017.04.004 ↗
13. Shear bond strength of resin bonded ceramic after different try-in procedures10.1016/0300-5712(94)90012-4 ↗
14. The effect of surface treatments on the bond strength between CAD/CAM blocks and composite resin10.1111/jopr.12322 ↗
15. Bonding to CAD/CAM composites: an interfacial fracture toughness approach
16. Bond strength of novel CAD/CAM restorative materials to self-adhesive resin cement: the effect of surface treatments
17. Influence of surface treatments on bond strength of metal and ceramic brackets to a novel CAD/CAM hybrid ceramic material10.1007/s10266-014-0188-8 ↗
18. Adhesive luting of new CAD/CAM materials
19. Surface treatment agent for dental metals using a thiirane monomer and a phosphoric acid monomer10.4012/dmj.21.156 ↗
20. Effect of curing mode on shear bond strength of self-adhesive cement to composite blocks10.3390/ma9030210 ↗
21. In vitro evaluation of the wear resistance of composite resin blocks for CAD/CAM10.4012/dmj.2014-293 ↗
22. Effects of mechanical and chemical pretreatments of zirconia or fiber posts on resin cement bonding10.1371/journal.pone.0129690 ↗
23. Synthesis of amorphous porous zirconium phosphonate materials: tuneable from micropore to mesopore sizes10.1039/C4RA03970J ↗
24. Aspects of silane coupling agents and surface conditioning in dentistry: an overview10.1016/j.dental.2012.02.009 ↗
25. Bonding of resin composites to etchable ceramic surfaces - an insight review of the chemical aspects on surface conditioning10.1111/j.1365-2842.2005.01569.x ↗
26. Silane adhesion mechanism in dental applications and surface treatments: a review10.1016/j.dental.2017.09.002 ↗
27. In vitro fatigue resistance of CAD/CAM composite resin and ceramic posterior occlusal veneers10.1016/S0022-3913(10)60111-4 ↗
28. Hydrolytic stability of composite repair bond10.1111/j.1600-0722.2007.00475.x ↗
29. Microtensile bond strength and micromorphologic analysis of surface-treated resin nanoceramics10.4047/jap.2016.8.4.275 ↗
30. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
31. Evaluation of different surface treatments on fiber post cemented with a self-adhesive system10.1016/j.msec.2017.03.141 ↗
32. Resin-composite blocks for dental CAD/CAM applications
33. Fracture strength and hardness of different computer-aided design/computer-aided manufacturing inlays10.4103/njcp.njcp_58_17 ↗
34. Evaluation of five CAD/CAM materials by microstructural characterization and mechanical tests: a comparative in vitro study10.1186/s12903-017-0458-2 ↗
35. Effect of the silicone disclosing procedure on the shear bond strength of composite cements to ceramic restorations10.1067/mpr.2003.1 ↗
36. Comparison of resin bonding improvements to zirconia between one-bottle universal adhesives and tribochemical silica coating, which is better?10.1016/j.dental.2015.12.014 ↗
37. Effectiveness and stability of silane coupling agent incorporated in 'universal' adhesives10.1016/j.dental.2016.07.002 ↗
38. In-vitro dimensional changes of self-adhesive and conventional resin cements10.1016/j.dental.2013.08.130 ↗