Tuning strain-induced γ-to-ε martensitic transformation of biomedical Co–Cr–Mo alloys by introducing parent phase lattice defects
Source abstract
Abstract
In this study, we examined the effect of pre-existing dislocation structures in a face-centered cubic γ-phase on strain-induced martensitic transformation (SIMT) to produce a hexagonal close-packed ε-phase in a hot-rolled biomedical Co-Cr-Mo alloy. The as-rolled microstructure was characterized by numerous dislocations as well as stacking faults and deformation twins. SIMT occurred just after macroscopic yielding in tensile deformation. Using synchrotron X-ray diffraction line-profile analysis, we successfully captured the nucleation of ε-martensite during tensile deformation in terms of structural evolution in the surrounding γ-matrix: many dislocations that were introduced into the γ-matrix during the hot-rolling process were consumed to produce ε-martensite, together with strong interactions between dislocations in the γ-matrix. As a result, the SIMT behavior during tensile deformation was accelerated through the consumption of these lattice defects, and the nucleation sites for the SIMT ε-phase transformed into intergranular regions upon hot rolling. Consequently, the hot-rolled Co-Cr-Mo alloy simultaneously exhibited an enhanced strain hardening and a high yield strength. The results of this study suggest the possibility of a novel approach for controlling the γ → ε SIMT behavior, and ultimately, the performance of the alloy in service by manipulating the initial dislocation structures.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · High Entropy Alloys Studies · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Mechanical testing of spinal instrumentation10.1097/00003086-198802000-00015 ↗
2. Review of wear mechanisms in hip implants: paper I - general10.1016/j.matdes.2003.11.010 ↗
3. Stress induced martensite transformation in Co–28Cr–6Mo alloy during room temperature deformation10.1016/j.msea.2013.05.050 ↗
4. Room-temperature deformation and martensitic transformation of two Co-Cr-based alloys10.1007/s11661-018-4636-x ↗
5. Continuous atomic displacements and lattice distortion during fcc-bcc martensitic transformation10.1016/j.actamat.2015.06.010 ↗
6. Pin-on-disk wear behavior in a like-on-like configuration in a biological environment of high carbon cast and low carbon forged Co–29Cr–6Mo alloys10.1016/j.actamat.2006.10.005 ↗
7. Supra-ductile and high-strength manganese-TRIP/TWIP steels for high energy absorption purposes10.2355/isijinternational.43.438 ↗
8. High strength Fe−Mn−(Al, Si) TRIP/TWIP steels development — properties — application10.1016/S0749-6419(00)00015-2 ↗
9. Anomalous strengthening behavior of Co–Cr–Mo alloy single crystals for biomedical applications10.1016/j.scriptamat.2016.06.016 ↗
10. FIT2D: a multi-purpose data reduction, analysis and visualization program10.1107/S1600576716000455 ↗
11. Strain induced ε-martensite in a Co–Cr–Mo alloy: grain size effects10.1016/S0167-577X(99)00021-X ↗
12. Effect of pre-existing defects in the parent fcc phase on atomistic mechanisms during the martensitic transformation in pure Fe: a molecular dynamics study10.1016/j.actamat.2017.09.049 ↗
13. Strain-induced martensitic transformation near twin boundaries in a biomedical Co–Cr–Mo alloy with negative stacking fault energy10.1016/j.actamat.2012.11.041 ↗
14. Work hardening associated with ε-martensitic transformation, deformation twinning and dynamic strain aging in Fe–17Mn–0.6C and Fe–17Mn–0.8C TWIP steels10.1016/j.msea.2011.06.011 ↗
15. Metastable high-entropy dual-phase alloys overcome the strength–ductility trade-off10.1038/nature17981 ↗
16. A TRIP-assisted dual-phase high-entropy alloy: grain size and phase fraction effects on deformation behavior10.1016/j.actamat.2017.03.069 ↗
17. Microstructure and strength of commercial purity aluminium (AA 1200) cold-rolled to large strains10.1016/S1359-6454(02)00174-X ↗
18. Deformation induced FCC to HCP transformation in a Co–27Cr–5Mo–0.05C alloy10.1016/j.msea.2010.12.024 ↗
19. Meyers · 2009
20. Role of strain-induced martensitic transformation on extrusion and intrusion formation during fatigue deformation of biomedical Co–Cr–Mo–N alloys10.1016/j.actamat.2014.08.039 ↗
21. Evolution of cold-rolled microstructures of biomedical Co–Cr–Mo alloys with and without N doping10.1016/j.msea.2010.09.002 ↗
22. Cold-rolling behavior of biomedical Ni-free Co–Cr–Mo alloys: role of strain-induced ε martensite and its intersecting phenomena10.1016/j.jmbbm.2015.10.021 ↗
23. Texture evolution and mechanical anisotropy of biomedical hot-rolled Co–Cr–Mo alloy10.1016/j.jmbbm.2015.06.034 ↗
24. Strengthening of biomedical Co–Cr–Mo alloy by multipass “low-strain-per-pass” thermomechanical processing10.1016/j.actbio.2015.09.016 ↗
25. Development of new metallic alloys for biomedical applications10.1016/j.actbio.2012.06.037 ↗
26. Nishiyama · 1978
27. Microstructural characterization of high-manganese austenitic steels with different stacking fault energies10.1016/j.matchar.2011.05.011 ↗
28. The effect of contouring on fatigue strength of spinal rods: is it okay to re-bend and which materials are best?10.1016/j.jspd.2013.08.004 ↗
29. Formation of shear bands and strain-induced martensite during plastic deformation of metastable austenitic stainless steels10.1016/j.actamat.2007.07.015 ↗
30. Microstructural dependence of Fe-high Mn tensile behavior10.1007/BF02643961 ↗
31. The effect of dislocation contrast on x-ray line broadening: a new approach to line profile analysis10.1063/1.117951 ↗
32. The effect of dislocation contrast on X-Ray line profiles in untextured polycrystals10.1002/(SICI)1521-396X(199902)171:2<425::AID-PSSA425>3.0.CO;2-W ↗
33. Crystallite size distribution and dislocation structure determined by diffraction profile analysis: principles and practical application to cubic and hexagonal crystals10.1107/S0021889801003715 ↗
34. Theoretical aspects of kinematical X-ray diffraction profiles from crystals containing dislocation distributions
35. Ultrafine grain refinement of biomedical Co–29Cr–6Mo alloy during conventional hot-compression deformation10.1007/s11661-009-9879-0 ↗
36. Origin of significant grain refinement in Co–Cr–Mo alloys without severe plastic deformation10.1007/s11661-012-1303-5 ↗
37. Enhanced mechanical properties of As-forged Co–Cr–Mo–N alloys with ultrafine-grained structures10.1007/s11661-012-1288-0 ↗
38. Analysis of the fracture mechanism of Ti–6Al–4V alloy rods that failed clinically after spinal instrumentation surgery10.1097/BRS.0000000000000881 ↗
39. Manufacturing of high-strength Ni-free Co–Cr–Mo alloy rods via cold swaging10.1016/j.jmbbm.2015.12.032 ↗
40. Stacking-fault strengthening of biomedical Co–Cr–Mo alloy via multipass thermomechanical processing10.1038/s41598-017-10305-1 ↗