Wear and corrosion behaviour of nanocrystalline TaN, ZrN, and TaZrN coatings deposited on biomedical grade CoCrMo alloy
Source abstract
Abstract
TaZrN coatings were synthesized directly on biomedical grade CoCrMo using radio-frequency magnetron co-sputtering. The mechanical properties, adhesion, wear, and corrosion resistance of the TaZrN coatings on the Cobalt alloy were assessed to determine their potential for hip joint replacement applications. The results indicate the TaZrN coatings are highly adhesive and have a nanocrystalline structure with a Hardness and Young's modulus of 19 GPa and 297 GPa, respectively. The TaZrN coatings showed a 3% lower wear rate of the polyethylene counterpart and an icorr value 274 times lower than the uncoated CoCrMo alloy. The excellent wear and corrosion resistance of the TaZrN coating suggest that it is a promising coating material for CoCrMo alloy to improve the lifetime of hip joint implants.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (67)
Show source-provided references
1. Electronic structure and mechanical properties of ternary ZrTaN alloys studied by ab initio calculations and thin-film growth experiments10.1103/PhysRevB.90.144107 ↗
2. Structural properties and corrosion resistance of tantalum nitride coatings produced by reactive DC magnetron sputtering10.1039/C6RA17869C ↗
3. Characterization of tantalum zirconium nitride sputter-deposited nanocrystalline coatings10.1016/j.surfcoat.2004.03.044 ↗
4. Electronic and optical properties of Ta1−xZrxN films: experimental and ab initio studies10.1116/1.1946710 ↗
5. Tribological investigation of zirconium nitride/silver nanocomposite structures10.1016/j.surfcoat.2005.11.135 ↗
6. Laboratory wear tests and clinical observations of the penetration of femoral heads into acetabular cups in total replacement hip joints10.1016/0043-1648(85)90049-3 ↗
7. Laboratory wear tests and clinical observations of the penetration of femoral heads into acetabular cups in total replacement hip joints10.1016/0043-1648(85)90050-X ↗
8. The coefficient of thermal expansion of zirconium nitride10.1107/S0365110X58000724 ↗
9. Migration of metal and polyethylene particles from articular prostheses may generate lymphadenopathy with histiocytosis10.1002/(SICI)1097-4636(199602)30:2<157::AID-JBM4>3.0.CO;2-Q ↗
10. Magnetron sputter deposited tantalum and tantalum nitride thin fi lms : an analysis of phase , hardness and composition10.1016/j.tsf.2013.09.055 ↗
11. The transpassive dissolution mechanism of highly alloyed stainless steels10.1016/S0010-938X(02)00073-2 ↗
12. Biocompatibility and antibacterial properties of zirconium nitride coating on titanium abutments: an in vitro study10.1371/journal.pone.0199591 ↗
13. Mechanical properties and oxidation resistance of reactively sputtered Ta1-xZrxNy thin films10.1016/j.surfcoat.2015.08.051 ↗
14. Effects of surface coating on reducing friction and wear of orthopaedic implants10.1088/1468-6996/15/1/014402 ↗
15. Corrosion resistance of ZrN films on AISI 304 stainless steel substrate10.1016/S0257-8972(02)00882-4 ↗
16. Ceramic bearing surfaces in total artificial joints: resistance to third body wear damage from bone cement particles10.3109/03091909109009970 ↗
17. Wear and corrosion characteristics of nano-crystalline tantalum nitride coatings deposited on CoCrMo alloy for hip joint applications10.1016/j.matchar.2021.111516 ↗
18. The role of counterface imperfections in the wear of polyethylene10.1016/0043-1648(87)90036-6 ↗
19. Primary uncemented harris-galante acetabular components in patients 50 Years old or younger10.1097/01.blo.0000142286.73328.28 ↗
20. Ceramic bearings for total hip arthroplasty have high survivorship at 10 years10.1007/s11999-011-2076-7 ↗
21. Development of a Ta/TaN/TaNx(Ag)y/TaN nanocomposite coating system and bio-response study for biomedical applications10.1016/j.vacuum.2017.08.020 ↗
22. Effect of nitrogen flow ratio on nano-mechanical properties of tantalum nitride thin film10.1016/j.jallcom.2017.05.159 ↗
23. The influence of scratches to metallic counterfaces on the wear of ultra-high molecular weight polyethylene10.1243/PIME_PROC_1995_209_353_02 ↗
24. Tribological, tribocorrosion and wear mechanism studies of TaZrN coatings deposited by magnetron sputtering on TiAlV alloy10.3390/coatings8090295 ↗
25. Status of surface modification techniques for artificial hip implants10.1080/14686996.2016.1240575 ↗
26. Tribological performance of the biological components of synovial fluid in artificial joint implants10.1088/1468-6996/16/4/045002 ↗
27. Influence of nitrogen vacancy concentration on mechanical and electrical properties of rocksalt zirconium nitride films10.1007/s40195-017-0636-x ↗
28. Retrospective lifetime estimation of failed and explanted diamond-like carbon coated hip joint balls10.1016/j.actbio.2012.04.016 ↗
29. Tribological study of a mono and multilayer coating of TaZrN/TaZr produced by magnetron sputtering on AISI-316L stainless steel10.1016/j.triboint.2018.10.034 ↗
30. Recent updates for biomaterials used in total hip arthroplasty10.1186/s40824-018-0144-8 ↗
31. 2006 · 1
32. 2020 · 1
33. The role of cement in the long term performance and premature failure of charnley low friction arthroplasties10.1243/EMED_JOUR_1986_015_007_02 ↗
34. A review of UHMWPE wear-induced osteolysis: the role for early detection of the immune response10.1038/boneres.2016.14 ↗
35. Magnetron sputtering: a review of recent developments and applications10.1016/S0042-207X(99)00189-X ↗
36. Examination of failed retrieved temporomandibular joint (TMJ) implants10.1016/j.actbio.2016.01.001 ↗
37. Aggressive 3rd-body wear challenge to highly crosslinked polyethylene: a hip simulator model10.1016/j.wear.2009.01.029 ↗
38. The influence of nitrogen on the morphology of ZrN coatings deposited by magnetron sputtering10.1016/j.apsusc.2020.146508 ↗
39. Sputtering yields of metals for Ar + and Ne + ions with energies from 50 to 600 ev10.1063/1.1736012 ↗
40. Biomedical properties of tantalum nitride films synthesized by reactive magnetron sputtering10.1016/S0040-6090(01)01448-1 ↗
41. Leyland · 2000 · vol. 246 · 1
42. CoCrMo metal-on-metal hip replacements10.1039/C2CP42968C ↗
43. Migration of wear debris of polyethylene depends on bone microarchitecture10.1002/jbm.b.31341 ↗
44. Mechanical and corrosive characteristics of Ta/TaN multilayer coatings10.1016/j.vacuum.2012.05.024 ↗
45. Endosteal erosion in association with stable uncemented femoral components10.2106/00004623-199072070-00011 ↗
46. Tribocorrosion response in biological environments of multilayer TaN films deposited by HPPMS10.1016/j.surfcoat.2015.11.012 ↗
47. Preferred orientation, phase transition and hardness for sputtered zirconium nitride films grown at different substrate biases10.1016/j.surfcoat.2010.10.060 ↗
48. Neutron diffraction analysis of cubic tantalum nitride
49. Nanostructured diamondlike carbon thin films for medical applications10.1016/j.msec.2005.01.026 ↗
50. Titanium nitride ceramic film against polyethylene. A 48 million cycle wear test
51. The inverse Hall–Petch effect in nanocrystalline ZrN coatings10.1016/j.surfcoat.2011.01.021 ↗
52. Chapter 13 - corrosion and Mott-Schottky probe of chromium nitride coatings exposed to saline solution for engineering and biomedical applications
53. Surface performances of PVD ZrN coatings in biological environments10.1080/17515831.2018.1553820 ↗
54. Wear and corrosion properties of in-situ grown zirconium nitride layers for implant applications10.1016/j.surfcoat.2017.11.064 ↗
55. Periprosthetic bone loss in total hip arthroplasty. Polyethylene wear debris and the concept of the effective joint space10.2106/00004623-199274060-00006 ↗
56. Protective coating of zinc and zinc alloys for industrial applications
57. Improving fretting corrosion resistance of CoCrMo alloy with TiSiN and ZrN coatings for orthopedic applications10.1016/j.jmbbm.2020.104233 ↗
58. Daimler benz adhesion test
59. New insights into fretting corrosion products from modular total hip replacement revision
60. Comparison of mechanical and tribological properties of nitride and oxynitride coatings based on chrome and zirconium obtained by cathodic arc evaporation10.3103/S1068366619020156 ↗
61. Osteolysis in alloarthroplasty of the hip: the role of ultra-high molecular weight polyethylene wear particles10.1097/00003086-199009000-00013 ↗
62. Corrosion behavior of ZrN/Zr coated biomedical AZ91 magnesium alloy10.1016/j.surfcoat.2009.02.074 ↗
63. The microstructure and mechanical properties of tantalum nitride coatings deposited by a plasma assisted bias sputtering deposition process10.1016/j.surfcoat.2016.09.015 ↗
64. Yan · 2013
65. Yang · 2016 · vol. 303 · 32
66. Zunjarrao · 2008 · vol. 28 · 79
67. Survival of hard-on-hard bearings in total hip arthroplasty: a systematic review10.1007/s11999-010-1658-0 ↗