journal article·2019-11

Low-fusing porcelain glaze application does not damage the fatigue strength of Y-TZP

Camila Pauleski Zucuni, Gabriel Kalil Rocha Pereira, Kiara Serafini Dapieve, Marilia Pivetta Rippe, Marco Cícero Bottino, Luiz Felipe Valandro

Publisher page

Abstract

This study evaluated and compared the effects of two glaze application methods (brush and spray) on the fatigue strength and surface characteristics (topography and roughness) of a translucent yttrium stabilized partially tetragonal zirconia polycrystal ceramic (Y-TZP) prior to and after grinding. Disc-shaped specimens of translucent Y-TZP (Vita YZ-HT; Vita-Zahnfabrik) were processed (ISO 6872-2015) and randomly allocated into 6 groups, according to the surface treatments performed on the tensile surface: Ctrl - as-sintered (no treatment); Gr - grinding with a diamond bur (181 μm-grit; #3101G); Br - glaze obtained from a powder-liquid mix and applied by brush (Vita Akzent; Vita Zahnfabrik); Sp - glaze application via spray (Vita Akzent Plus; Vita Zahnfabrik); Gr + Br and Gr + Sp - association of grinding + respective glaze method. Analyses of surface roughness (Ra and Rz), fatigue strength (staircase method), surface topography and fractography were carried out. The as-sintered condition had the smoothest surface, while grinding led to the rougher and more heterogeneous topography. Both glaze application methods showed a potential for topography evenness (smoothening effect), while the glaze spray method led to thinner layers of material, showing a limitation in reducing the roughness compared to the brush method. No deleterious effect on fatigue strength of the Y-TZP could be observed, as the glaze-spray application on the as-sintered surface showed the highest values. Fractography depicted two distinct fracture origin regions: from defects in the surface/sub-surface region for the Ctrl and Gr groups; and at the zirconia-glaze layer interface for Br, Sp, Gr + Br and Gr + Sp. The clinical relevance of this work is that the tested glaze application methods did not damage the fatigue strength of the tested Y-TZP.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Effect of zirconia type on its bond strength with different veneer ceramics10.1111/j.1532-849X.2008.00306.x ↗
2. Machining variability impacts on the strength of a ‘chairside’ CAD-CAM ceramic10.1016/j.dental.2012.04.017 ↗
3. Fatigue behavior of Y-TZP ceramic after surface treatments10.1016/j.jmbbm.2015.11.042 ↗
4. Can low-fusing glass application affect the marginal misfit and bond strength of Y-TZP crowns?10.1590/1807-3107bor-2018.vol32.0034 ↗
5. Anusavice · 2003
6. Extended glaze firing on ceramics for hard machining: crack healing, residual stresses, optical and microstructural aspects10.1016/j.dental.2016.12.002 ↗
7. Survival rate of mono-ceramic and ceramic-core CAD/CAM generated anterior crowns over 2–5 years10.1111/j.1600-0722.2004.00119.x ↗
8. Flexural strength and failure modes of layered ceramic structures10.1016/j.dental.2011.09.008 ↗
9. Effect of finishing and polishing on the surface roughness and gloss of feldspathic ceramic for hairside CAD/CAM systems10.2341/15-174-L ↗
10. Fracture energy of class-alumina interfaces via the bimaterial bend test10.1111/j.1151-2916.1997.tb02808.x ↗
11. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
12. Microstructural analysis and reliability of monolithic zirconia after simulated adjustment protocols10.1016/j.dental.2017.04.024 ↗
13. Collins · 1993
14. Thermal compatibility of dental ceramic systems using cylindrical and spherical geometries10.1016/j.dental.2007.08.008 ↗
15. Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structures10.1016/S0109-5641(03)00010-1 ↗
16. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
17. Effects of non-planarity on the mixed mode fractureresistance of biomaterial interfaces10.1016/0001-6160(89)90017-5 ↗
18. Effect of the bonding strategy on the tensile retention of full-contour zirconia crowns10.1016/j.ijadhadh.2018.06.006 ↗
19. Effect of surface roughness on flexural strength of veneer ceramics10.1177/154405910308201207 ↗
20. Glaze firing and hydrofluoric acid etching: do these procedures affect the flexural strength of aleucite glass-ceramic10.1016/j.dental.2015.04.005 ↗
21. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
22. The effects of finishing and polishing techniques on surface roughness and color stability of nanocomposites10.1016/j.jdent.2012.07.005 ↗
23. Surfacemicro-morphology, phase transformation, and mechanical reliability of ground andaged monolithic zirconia ceramic10.1016/j.jmbbm.2016.10.008 ↗
24. Surface roughness of zirconia for full-contour crowns after clinically simulated grinding and polishing10.1038/ijos.2014.34 ↗
25. Geometrical product specifications (GPS)–surface texture: profile method, terms definitions and surface texture parameters
26. ISO 6872 · 2015
27. Fracture surface analysis of dental ceramics: clinically failed restorations
28. Clinical outcomes of monolithic zirconia crowns with CAD/CAM technology. A 1-year follow-up prospective clinical study of 65 patients10.3390/ijerph15112523 ↗
29. Effect of glazing on flexural strength of full-contour zirconia
30. Effects of two surface finishes on the color of cemented and colored anatomic-contour zirconia crowns10.1016/j.prosdent.2015.12.012 ↗
31. An in vitro study to identify a ceramic polishing protocol effecting smoothness superior to glazed surface10.1007/s13191-013-0313-3 ↗
32. Fracture mechanics principles10.1016/0109-5641(95)80044-1 ↗
33. Effect of grinding with diamond-disc and-bur on the mechanical behavior of a Y-TZPceramic10.1016/j.jmbbm.2014.05.010 ↗
34. Fatigue limit of polycrystalline zirconium oxide ceramics: effect of grinding and low-temperature aging10.1016/j.jmbbm.2016.01.006 ↗
35. Mechanical behavior of yttria-stabilized tetragonal zirconia polycrystalline ceramic after different zirconia surface treatments10.1016/j.msec.2017.03.299 ↗
36. Cycle-dependent in vitro wear performance of dental ceramics after clinical surface treatments10.1016/j.jmbbm.2015.08.009 ↗
37. Prochnow · Dent. Mater. · 2018 · 34 · e25510.1016/j.dental.2018.06.028 ↗
38. Influence of surface treatment on the in-vitro fracture resistance of zirconia-based all-ceramic anterior crows10.1016/j.dental.2015.10.003 ↗
39. Three generations of zirconia: from veneered to monolithic. Part I
40. The use of slow heating and slow cooling regimens to strengthen porcelain fused to zirconia10.1016/S0022-3913(12)60050-X ↗
41. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction10.1111/j.1151-2916.1984.tb19614.x ↗
42. Low-fusing porcelain glaze application on 3Y-TZP surfaces can enhance zirconia-porcelain adhesion10.1590/0103-6440201601014 ↗
43. Fatigue strength of yttria-stabilized zirconia polycrystals: effects of grinding, polishing, glazing, and heat treatment10.1016/j.jmbbm.2017.06.016 ↗
44. Load-bearing capacity under fatigue and survival rates of adhesively cemented yttrium-stabilized zirconia polycrystal monolithic simplified restorations10.1016/j.jmbbm.2018.11.009 ↗