Influence of sandblasting and acid etching on fatigue properties of ultra-fine grained Ti grade 4 for dental implants
Source abstract
Abstract
Commercially pure Ti is a typical material for dental implants. Besides oral environmental effects, implants are seriously mechanically loaded during the lifetime. Mechanical resistance of coarse and ultra-fine grained Ti grade 4 was investigated. Significant grain size refinement resulting in the 65% increase of the proof stress is reported. The fatigue endurance limit increased from 523 MPa to 698 MPa due to grain refinement. The influence of sandblasting combined with acid etching on fatigue damage of both material states was analyzed. The surface treatment was proven as detrimental to the fatigue properties of both material states, due to reduction of the fatigue initiation stage. Nevertheless, the fatigue endurance limit of the surface-treated ultra-fine grained material remained higher than the fatigue endurance limit of the coarse-grained material without surface treatment. Reported results confirm better mechanical resistance of ultra-fine grained materials for dental implants in the comparison with coarse-grain one.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. In vivo evaluation of micro-rough and bioactive titanium dental implants using histometry and pull-out tests10.1016/j.jmbbm.2011.05.005 ↗
2. Brittle coating effects on fatigue cracks behavior in Ti alloys10.1016/j.ijfatigue.2019.04.017 ↗
3. Fretting-corrosion behavior on dental implant connection in human saliva10.1016/j.jmbbm.2019.02.025 ↗
4. Fatigue behaviour of light alloys with ultrafine grain structure produced by severe plastic deformation: an overview10.1016/j.ijfatigue.2009.06.022 ↗
5. Fatigue crack propagation in UFG Ti grade 4 processed by severe plastic deformation10.1016/j.ijfatigue.2017.01.028 ↗
6. Effect of shotpeening on sliding wear and tensile behavior of titanium implant alloys10.1016/j.matdes.2013.11.052 ↗
7. Three-dimensional and chemical changes on the surface of a 3-year clinically retrieved oxidized titanium dental implant10.1016/j.jmbbm.2014.02.020 ↗
8. Cleavage cracking of ductile-metal substrates induced by brittle coating fracture10.1016/j.actamat.2018.04.017 ↗
9. Brittle film-induced cracking of ductile substrates10.1016/j.actamat.2015.07.059 ↗
10. Enhancement of fatigue and corrosion properties of pure Ti by sandblasting10.1016/j.msea.2006.04.024 ↗
11. Bone regeneration into side openings and hollow inner channel of a dental implant10.1016/j.jmbbm.2019.103416 ↗
12. Fatigue strength of ultrafine-grained pure Ti after severe plastic deformation10.1016/j.scriptamat.2006.01.042 ↗
13. Surface treatments of titanium dental implants for rapid osseointegration10.1016/j.dental.2006.06.025 ↗
14. Formation of bioactive hydroxyapatite-containing titania coatings on CP-Ti 4+ alloy generated by plasma electrolytic oxidation10.1016/j.surfcoat.2019.02.030 ↗
15. Enhancement of mechanical properties of grade 4 titanium by equal channel angular pressing with billet encapsulation10.1016/j.matlet.2013.09.118 ↗
16. Lütjering · 2007
17. Effect of bulk microstructure of commercially pure titanium on surface characteristics and fatigue properties after surface modification by sand blasting and acid-etching10.1016/j.jmbbm.2015.11.035 ↗
18. Continuous production of pure titanium with ultrafine to nanocrystalline microstructure10.3390/ma13020336 ↗
19. Comprehensive evaluation of the properties of ultrafine to nanocrystalline grade 2 titanium wires10.3390/ma11122522 ↗
20. Effect of surface treatments on the fatigue life of titanium for biomedical applications10.1016/j.jmbbm.2010.03.006 ↗
21. Effect of commercial purity levels on the mechanical properties of ultrafine-grained titanium10.1016/j.msea.2010.11.021 ↗
22. Enhanced fatigue strength of commercially pure Ti processed by severe plastic deformation10.1016/j.msea.2008.07.075 ↗
23. Sha · 2009
24. Improved osseointegration of long-term stored SLA implant by hydrothermal sterilization10.1016/j.jmbbm.2015.08.038 ↗
25. Mechanical and biological behavior of ultrafine-grained Ti alloy aneurysm clip processed using high-pressure torsion10.1016/j.jmbbm.2017.02.002 ↗
26. Cyclic behavior of ultrafine-grain titanium produced by severe plastic deformation10.1016/S0921-5093(01)01262-X ↗
27. Effect of microstructure on the fatigue properties of Ti–6Al–4V titanium alloys10.1016/j.matdes.2012.10.059 ↗