Influence of the foundation substrate on the fatigue behavior of bonded glass, zirconia polycrystals, and polymer infiltrated ceramic simplified CAD-CAM restorations
Source abstract
Abstract
This study evaluated the influence of distinct substrates on the mechanical fatigue behavior of adhesively cemented simplified restorations made of glass, polycrystalline or polymer infiltrated-ceramics. CAD/CAM ceramic blocks (feldspathic - FEL; lithium disilicate - LD; yttria-stabilized zirconia - YZ; and polymer-infiltrated ceramic network - PICN) were shaped into discs (n = 15, Ø = 10 mm; thickness = 1.0 mm), mimicking a simplified monolithic restoration. After, they were adhesively cemented onto different foundation substrates (epoxy resin - ER; or Ni-Cr metal alloy - MA) of the same shape (Ø = 10 mm; thickness = 2.0 mm). The assemblies were subjected to fatigue testing using a step-stress approach (200N-2800 N; step-size of 200 N; 10,000 cycles per step; 20 Hz) upon the occurrence of a radial crack or fracture. The data was submitted to two-way ANOVA (α = 0.05) to analyze differences considering 'ceramic material' and 'type of substrate' as factors. In addition, a survival analysis (Kaplan Meier with Mantel-Cox log-rank post-hoc tests; α = 0.05) was conducted to obtain the survival probability during the steps in the fatigue test. Fractographic and finite element (FEA) analyzes were also conducted. The factors 'ceramic material', 'type of substrate' and the interaction between both were verified to be statistically significant (p < .001). All evaluated ceramics presented higher fatigue failure load (FFL), cycles for failure (CFF) and survival probabilities when cemented to the metallic alloy substrate. Among the restorative materials, YZ and LD restorations presented the best fatigue behavior when adhesively cemented onto the metallic alloy substrate, while FEL obtained the lowest FFL and CFF for both substrates. The LD, PICN and YZ restorations showed similar fatigue performance considering the epoxy resin substrate. A more rigid foundation substrate improves the fatigue performance of adhesively cemented glass, polycrystalline and polymer infiltrated-ceramic simplified restorations.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Fatigue behavior of ultrafine tabletop ceramic restorations10.1016/j.dental.2018.06.017 ↗
2. Substrate masking ability of bilayer and monolithic ceramics used for complete crowns and the effect of association with an opaque resin-based luting agent10.1016/j.jpor.2019.01.005 ↗
3. Fracture rates and lifetime estimations of CAD/CAM all-ceramic restorations10.1177/0022034515608187 ↗
4. Bonfante · 2016
5. Mechanical properties of polymer-infiltrated-ceramic-network materials10.1016/j.dental.2013.01.002 ↗
6. 5-Year follow-up of A prospective clinical study on various types of core restorations
7. CAD-FEA modeling and analysis of different full crown monolithic restorations10.1016/j.dental.2018.06.024 ↗
8. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
9. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
10. Effect of supporting substrate on the failure behavior of a polymer-infiltrated ceramic network material10.1016/j.prosdent.2018.08.008 ↗
11. Effect of a metal primer on the bond strength of the resin-metal interface10.1590/S1678-77572004000200006 ↗
12. Fatigue performance of distinct CAD/CAM dental ceramics10.1016/j.jmbbm.2019.103540 ↗
13. ISO 6872 · 2015
14. Influence of different surface treatments of nickel chrome metal alloy and types of metal primer monomers on the tensile bond strength of a resin cement10.1016/j.sdentj.2019.03.006 ↗
15. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
16. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
17. Fracture-surface analysis of dental ceramics10.1016/0022-3913(89)90075-9 ↗
18. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
19. Comparison of the mechanical properties of translucent zirconia and lithium disilicate10.1016/j.prosdent.2017.08.004 ↗
20. Fatigue resistance of simplified CAD – CAM restorations : foundation material and ceramic thickness effects on the fatigue behavior of partially- and fully-stabilized zirconia10.1016/j.dental.2021.01.001 ↗
21. Load-bearing capacities of ultra-thin occlusal veneers bonded to dentin10.1016/j.jmbbm.2019.04.006 ↗
22. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns : multi-physics FEA modeling and monotonic testing10.1016/j.dental.2012.04.033 ↗
23. Effect of different loading pistons on stress distribution of a CAD/CAM silica-based ceramic: CAD-FEA modeling and fatigue survival analysis10.1016/j.jmbbm.2019.03.011 ↗
24. Fracture resistance of monolithic zirconia molar crowns with reduced thickness10.3109/00016357.2015.1007479 ↗
25. Fracture strength of ceramic monolithic crown systems of different thickness10.2334/josnusd.57.255 ↗
26. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
27. Lithium disilicate glass-ceramic vs translucent zirconia polycrystals bonded to distinct substrates: fatigue failure load, number of cycles for failure, survival rates, and stress distribution10.1016/j.jmbbm.2018.12.010 ↗
28. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
29. Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: conventional ceramic etching vs etch & prime one-step primer10.1016/j.dental.2018.04.012 ↗
30. Dental ceramics: a review of new materials and processing methods10.1590/1807-3107bor-2017.vol31.0058 ↗
31. Three generations of zirconia: from veneered to monolithic. Part I
32. HF etching of CAD/CAM materials: influence of HF concentration and etching time on shear bond strength10.1186/s13005-019-0206-8 ↗
33. Fracture surface characterization of clinically failed all-ceramic crowns10.1177/00220345940730120601 ↗
34. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
35. Influence of ceramic material, thickness of restoration and cement layer on stress distribution of occlusal veneers10.1590/1807-3107bor-2018.vol32.0118 ↗
36. Journal of the Mechanical Behavior of Biomedical Materials Accelerated loading frequency does not influence the fatigue behavior of polymer infiltrated ceramic network or lithium disilicate glass-ceramic restorations10.1016/j.jmbbm.2020.103905 ↗
37. The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs10.1016/j.dental.2018.01.010 ↗
38. Fatigue performance of adhesively cemented glass-, hybrid- and resin-ceramic materials for CAD/CAM monolithic restorations10.1016/j.dental.2019.01.013 ↗
39. Stress fatigue: basic principles and prosthodontic implications
40. Load-bearing capacity of lithium disilicate and ultra-translucent zirconias10.1016/j.jmbbm.2018.08.023 ↗
41. Dental ceramics for restoration and metal veneering10.1016/j.cden.2017.06.005 ↗
42. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
43. Fracture-resistant monolithic dental crowns10.1016/j.dental.2015.12.010 ↗
44. Influence of material thickness on fractural strength of CAD/CAM fabricated ceramic crowns10.4012/dmj.2016-296 ↗
45. Grinding, polishing and glazing of the occlusal surface do not affect the load-bearing capacity under fatigue and survival rates of bonded monolithic fully-stabilized zirconia simplified restorations10.1016/j.jmbbm.2019.103528 ↗