Mechanical energy dissipation in natural ceramic composites
Source abstract
Abstract
Ceramics and glasses, in their monolithic forms, typically exhibit low fracture toughness values, but rigid natural marine ceramic and glass composites have shown remarkable resistance to mechanical failure. This has been observed in load-extension behavior by recognizing that the total area under the curve, notably the part beyond the yield point, often conveys substantial capacity to carry mechanical load. The mechanisms underlying the latter observations are proposed as defining factors for toughness that provide resistance to failure, or capability to dissipate energy, rather than fracture toughness. Such behavior is exhibited in the spicules of glass sponges and in mollusk shells. There are a number of similarities in the manner in which energy dissipation takes place in both sponges and mollusks. It was observed that crack diversion, a new form of crack bridging, creation of new surface area, and other important energy-dissipating mechanisms occur and aid in "toughening". Crack tolerance, key to energy dissipation in these natural composite materials, is assisted by promoting energy distribution over large volumes of loaded specimens by minor components of organic constituents that also serve important roles as adhesives. Viscoelastic deformation was a notable characteristic of the organic component. Some of these energy-dissipating modes and characteristics were found to be quite different from the toughening mechanisms that are utilized for more conventional structural composites. Complementary to those mechanisms found in rigid natural ceramic/organic composites, layered architectures and very thin organic layers played major roles in energy dissipation in these structures. It has been demonstrated in rigid natural marine composites that not only architecture, but also the mechanical behavior of the individual constituents, the nature of the interfaces, and interfacial bonding play important roles in energy dissipation. Additionally, the controlling effects of thin organic layers have been observed in other natural ceramic composite structures, such as teeth and bones, indicating that a variety of similar energy dissipating mechanisms in natural ceramic composites may operate as means to resist failure.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Calcium Carbonate Crystallization and Inhibition · Bone Tissue Engineering Materials · Building materials and conservation
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Fibrillar organic phases and their roles in rigid biological composites10.1016/j.jmbbm.2015.01.011 ↗
2. Biological structures mitigate catastrophic fracture through various strategies10.1007/s10704-005-3949-0 ↗
3. A novel biomimetic material duplicating the structure and mechanics of natural nacre10.1557/jmr.2011.65 ↗
4. Bioinspired design and assembly of platelet reinforced polymer films10.1126/science.1148726 ↗
5. Fracture mechanics of protein materials10.1016/S1369-7021(07)70208-0 ↗
6. Flaw tolerance in a viscoelastic strip10.1115/1.4007864 ↗
7. A mechanism for the control of crack propagation in all-brittle systems
8. Courtney · 2000 · 280
9. The design of mineralised hard tissues for their mechanical functions10.1242/jeb.202.23.3285 ↗
10. Biological composites
11. Sacrificial bonds heal bone10.1038/414699a ↗
12. Artful interfaces within biological materials10.1016/S1369-7021(11)70056-6 ↗
13. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
14. Nature's hierarchical materials10.1016/j.pmatsci.2007.06.001 ↗
15. Fritz, M., Treccani, L., Heinemann, F., Grathwohl, G., 2011. Synthetic Nacre, Method of Manufacture and Apparatus therefor, European Patent EP 1835053 B1.
16. Gordon · 1968 · 119
17. Green · 1998 · 229
18. Gruner · 2004
19. Three-dimensional-printing of bio-inspired composites
20. Hull · 1996
21. Comparison of nacre with other ceramic composites10.1007/BF00587670 ↗
22. Influence of moisture on the mechanical behavior of a natural composite10.1016/j.actbio.2009.12.006 ↗
23. Jones · 1975
24. Ker · 1977
25. Bioinspired design criteria for damage-resistant materials with periodically varying microstructure10.1002/adfm.201100443 ↗
26. Lawn · 1998 · 208
27. Mayer, G., Trejo, R., Lara-Curzio, E., Rodriguez, M., Tran, K., Song, H., Ma, W.H., 2005a. Lessons for new classes of inorganic/organic composites from the spicules and skeleton of the sea sponge Euplectella aspergillum. In: Proceedings of the Symp. on Mechanical Properties of Bioinspired and Biological Materials. Materials Research Society, Warrendale, PA, V.844, pp. 79–86.10.1557/PROC-844-Y4.2 ↗
28. Rigid biological systems as models for synthetic composites10.1126/science.1116994 ↗
29. New toughening concepts for ceramic composites from rigid natural materials10.1016/j.jmbbm.2010.08.001 ↗
30. Rigid biological composite materials: structural examples for biomimetic design10.1007/BF02412144 ↗
31. Biological materials: structure and mechanical properties10.1016/j.pmatsci.2007.05.002 ↗
32. Bioorganic/inorganic hybrid com- position of sponge spicules: matrix of the giant spicules and of the comitalia of the deep sea hexactinellid monorhaphis10.1016/j.jsb.2007.10.009 ↗
33. On the strength and stiffness of planar reinforced plastic resins10.1002/pen.760100310 ↗
34. Biomimetic model of a sponge-spicular optical fiber-mechanical properties and structure10.1557/JMR.2001.0198 ↗
35. Does abalone nacre form by heteroepitaxial nucleation or by growth through mineral bridges?10.1021/cm960429i ↗
36. Staab · 1999 · 71–96 · 261
37. Mechanical properties of bioinspired bicontinuous nanocomposites10.1016/j.commatsci.2013.04.012 ↗
38. Vogel · 2003 · 325
39. Wachtman · 2009 · 189
40. Mechanisms of toughening of a natural rigid composite10.1016/j.msec.2006.05.020 ↗
41. Effects of loading rate on the mechanical behavior of a natural rigid composite10.1016/j.actbio.2006.09.008 ↗
42. Deformation mechanisms in nacre10.1557/JMR.2001.0340 ↗
43. The stomatopod dactyl club: a formidable damage-tolerant biological hammer10.1126/science.1218764 ↗
44. The interaction between polymeric structure, deformation, and fracture