Mechanism of tribofilm formation on Ti6Al4V oxygen diffusion layer in a simulated body fluid
Source abstract
Abstract
An Oxygen Diffusion Layer (ODL) was generated on the surface of Ti6Al4V alloy by thermal oxidation treatment. In vitro tests for cytotoxicity were performed in the presence of Ti6Al4V and the ODL samples with the culture of G292 Cells using MTT assay. The results showed a similar cell viability in the presence of the both samples. Wear behaviour of Ti6Al4V and the ODL samples was investigated in a phosphate buffered saline solution under a normal load of 30N at a sliding velocity of 0.1m/s. The worn surface and subsurface of the samples were studied using SEM, STEM, TEM, XPS, AFM, nano-hardness and surface profilometry. A bio-tribofilm was observed on the worn surface of the ODL. TEM studies showed that the tribofilm had an amorphous structure and contained oxygen and phosphorous as confirmed by XPS and EDS analysis. AFM images also revealed that the tribofilm consisted of compacted fine debris. The formation of the tribofilm on the ODL with higher hardness and strength resulted in a decrease of about 95% in the wear rate compared with Ti6Al4V alloy.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Titanium Alloys Microstructure and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. A 15-year study of osseointegrated implants in the treatment of the edentulous jaw10.1016/S0300-9785(81)80077-4 ↗
2. Tribological behavior of heat treated Ni-rich NiTi alloys10.1115/1.4004102 ↗
3. ASTM F2129-15, 2015. Standard Test Method for Conducting Cyclic Potentiodynamic Polarization Measurements to Determine the Corrosion Susceptibility of Small Implant.
4. Calcium phosphate-titanium composites for articulating surfaces of load-bearing implants10.1016/j.jmbbm.2015.11.022 ↗
5. Glow-discharge and furnace treatments of Ti-6Al-4V10.1016/j.surfcoat.2003.10.004 ↗
6. BS EN ISO 10993-5, 2009. Biological evaluation of medical devices-Part 5: Tests for in vitro cytotoxicity, Switzerland.
7. Orthopedic wear debris mediated inflammatory osteolysis is mediated in part by NALP3 inflammasome activation10.1002/jor.22190 ↗
8. Metallic implant biomaterials10.1016/j.mser.2014.10.001 ↗
9. Improved wear resistance of functional diamond like carbon coated Ti–6Al–4V alloys in an edge loading conditions10.1016/j.jmbbm.2016.04.004 ↗
10. Oxygen boost diffusion for the deep-case hardening of titanium alloys10.1016/S0921-5093(99)00697-8 ↗
11. Fischer-Cripps · 2011
12. Froes, F.H., 2015. Principles of Alloying Titanium, in: Titan. Phys. Metall. Process. Appl., 1st Edition, ASM International, Ohio, pp. 51–74.10.31399/asm.tb.tpmpa.t54480051 ↗
13. Ti based biomaterials, the ultimate choice for orthopaedic implants - A review10.1016/j.pmatsci.2008.06.004 ↗
14. Study of the corrosion behavior of titanium and some of its alloys for biomedical and dental implant applications10.1016/S0022-0728(99)00260-0 ↗
15. Biological responses of human mesenchymal stem cells to titanium wear debris particles10.1002/jor.22002 ↗
16. Characterization of surface film formed on titanium in electrolyte using XPS10.1016/0169-4332(92)90178-Z ↗
17. Hutchings · 1992
18. Deformation twins in pure titanium processed by equal channel angular pressing10.1016/S1359-6462(02)00513-4 ↗
19. Independent slip systems in crystals10.1080/14786436408225657 ↗
20. Effect of the oxygen content in solution on the static and cyclic deformation of titanium foams10.1007/s10856-009-3798-x ↗
21. Leyens, C.,Peters, M., eds., 2006. Structure and Properties of Titanium and Titanium Alloys, in: Titan. Titan. Alloy. Fundam. Appl., John Wiley & Sons. pp. 1–36. 〈http://dx.doi.org/10.1002/3527602119〉.10.1002/3527602119.ch1 ↗
22. Nanocrystallization mechanism of beta phase in Ti-6Al-4V subjected to severe plastic deformation10.1016/j.msea.2016.05.088 ↗
23. Titanium alloys in total joint replacement—a materials science perspective10.1016/S0142-9612(97)00146-4 ↗
24. Thermal oxidation of Ti6Al4V alloy and its biotribological properties under serum lubrication10.1016/j.triboint.2014.12.022 ↗
25. Manivasagam, G., Dhinasekaran, D., Rajamanickam, A., 2010. Biomedical Implants: Corrosion and its Prevention - A Review, 〈http://dx.doi.org/10.2174/1877610801002010040〉.10.2174/1877610801002010040 ↗
26. Tribo-layer and its role in dry sliding wear of Ti-6Al-4V alloy10.1016/j.wear.2012.11.063 ↗
27. Moulder · 1992
28. Recent titanium R&D for biomedical applications in japan10.1007/s11837-999-0091-x ↗
29. Tribocorrosion behaviour of laser cladded biomedical grade titanium alloy10.1002/maco.201408037 ↗
30. Electrochemical impedance spectroscopy study of the passive oxide film on titanium for implant application10.1016/0013-4686(95)00465-3 ↗
31. The crystallography and deformation modes of hexagonal close-packed metals
32. Metallic biomaterials10.1007/978-0-387-84872-3_2 ↗
33. Microstructure evolution and grain refinement of Ti-6Al-4V alloy by laser shock processing10.1016/j.apsusc.2015.11.192 ↗
34. The evolution of tribolayers during high temperature sliding wear10.1016/j.wear.2014.03.007 ↗
35. Strain hardening of titanium: role of deformation twinning10.1016/S1359-6454(03)00239-8 ↗
36. Strain hardening due to deformation twinning in alpha-titanium: mechanisms10.1007/s11661-006-0171-2 ↗
37. Severe plastic deformation (SPD) of titanium at near-ambient temperature10.1016/j.actamat.2006.03.056 ↗
38. Fretting corrosion behaviour of Ti-6Al-4V alloy in artificial saliva containing varying concentrations of fluoride ions10.1016/j.wear.2010.09.008 ↗
39. ARXPS and high energy XPS characterisation of titanium surfaces for medical implants10.1002/sia.2778 ↗
40. Surface engineering of Ti6Al4V surfaces for enhanced tribocorrosion performance in artificial seawater10.1016/j.matdes.2016.04.080 ↗
41. Microstructure and wear of in-situ Ti/(TiN + TiB) hybrid composite layers produced using liquid phase process10.1016/j.matchemphys.2014.12.026 ↗
42. Bio-corrosion behaviour of oxygen diffusion layer on Ti-6Al-4V during tribocorrosion10.1016/j.corsci.2017.08.031 ↗
43. Interstitial Oxygen diffusion hardening - A practical route for the surface protection of titanium10.1016/j.matchar.2011.10.012 ↗
44. Influence of grain size on deformation mechanisms: an extension to nanocrystalline materials10.1016/j.msea.2005.05.111 ↗