Effect of zirconia surface treatment, resin cement and aging on the load-bearing capacity under fatigue of thin simplified full-contour Y-TZP restorations
Source abstract
Abstract
This study investigated the effect of zirconia surface treatment (air-abrasion with aluminum oxide or tribochemical silica coating) and aging on the fatigue behavior of thin monolithic Y-TZP (yttria-stabilized tetragonal zirconia polycrystal) restorations cemented with 2 types of resin cements, containing or not containing MDP, to a dentin-like substrate. Y-TZP ceramic (Zenostar T, diameter (Ø) 10 mm, 0.7 mm thick) and dentin-like discs (Ø 10 mm, 2.8 mm thick) were assigned into eight groups according to three factors: 'zirconia surface treatment' (aluminum oxide particles air-abrasion 'AO'; or tribochemical silica coating via silica-coated aluminum trioxide particles air-abrasion + silanization 'SC'); 'MDP-containing resin cement' (with: Panavia F2.0, 'MDP'; or without: Multilink Automix, 'nMDP'); and 'aging' (baseline; or aged - 'AG':12,000 thermal cycles + 60 days water storage). Y-TZP intaglio surface was conditioned and dentin-like substrate was etched with hydrofluoric acid prior to bonding. Aging was performed in half of the specimens before the fatigue testing (Staircase, 20 Hz; 250,000 cycles). Fractographic and topographic characteristics were analyzed by stereomicroscope and SEM. Prior to aging, no significant difference was found between the two surface treatments, irrespective to the cement. Samples bonded with resin cement containing MDP had a significant reduction in their fatigue failure load when Y-TZP was air-abraded with aluminum oxide particles and subjected to aging (MDP-AO = 2050.71A; MDP-AO/AG = 1756.67B). Other studied conditions were not affected by aging. Topographic images revealed a rougher surface for aluminum oxide air-abrasion. Fractography supports all failures as a radial crack starting at the Y-TZP intaglio surface. Bonded thin simplified Y-TZP restorations had a high load-bearing capacity, regardless of the studied factors. The MDP-containing resin cement applied on aluminum oxide air-abraded zirconia surface was not enough to maintain the fatigue performance after aging, while higher stability to aging was achieved by treating with the tribochemical silica coating method. When using MDP-free resin cement, the surface treatment and the aging did not impact the fatigue performance.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Effect of conditioning methods on the microtensile bond strength of phosphate monomer-based cement on zirconia ceramic in dry and aged conditions10.1002/jbm.b.30908 ↗
2. Fatigue resistance of Y-TZP/porcelain crowns is not influenced by the conditioning of the intaglio surface10.2341/14-166-L ↗
3. Effect of grinding on subsurface modifications of pre-sintered zirconia under different cooling and lubrication conditions10.1016/j.jmbbm.2018.06.026 ↗
4. Study of thermocycling effect on the bond strength between an aluminous ceramic and a resin cement10.1590/S1678-77572005000100011 ↗
5. Fatigue testing of biomaterials and their interfaces10.1016/j.dental.2017.01.012 ↗
6. Long-term resin bonding to zirconia ceramic with a new universal primer10.1016/S0022-3913(11)60137-6 ↗
7. In vitro evaluation of shear bond strengths of resin to densely-sintered high-purity zirconium-oxide ceramic after long-term storage and thermal cycling10.1016/j.prosdent.2004.02.001 ↗
8. Short-term prospective clinical evaluation of monolithic and partially veneered zirconia single crowns10.1111/jerd.12270 ↗
9. Adhesive cementation promotes higher fatigue resistance to zirconia crowns10.2341/16-002-L ↗
10. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
11. The effects of water on degradation of the zirconia-resin bond10.1016/j.jdent.2017.04.004 ↗
12. Collins · 1993
13. Stability of the bond between two resin cements and an yttria-stabilized zirconia ceramic after six months of aging in water10.1016/j.prosdent.2013.12.003 ↗
14. Micro-Raman vibrational identification of 10-MDP bond to zirconia and shear bond strength analysis
15. The use of MDP-based materials for bonding to zirconia10.1016/j.prosdent.2014.01.016 ↗
16. A method for obtaining and analyzing sensitivity data10.1080/01621459.1948.10483254 ↗
17. Size and shape of the human first permanent molar: a Fourier analysis of the occlusal and equatorial outlines10.1002/(SICI)1096-8644(199903)108:3<281::AID-AJPA4>3.0.CO;2-# ↗
18. Does luting strategy affect the fatigue behavior of bonded Y-TZP ceramic?
19. Monolithic zirconia crowns in the aesthetic zone in heavy grinders with severe tooth wear - an observational case-series10.1016/j.jdent.2018.01.013 ↗
20. A radiographic assessment of enamel thickness in human maxillary incisors10.1016/S0003-9969(98)00061-2 ↗
21. Durable bonding to mechanically and/or chemically pre-treated dental zirconia10.1016/j.jdent.2012.10.017 ↗
22. ISO 4049 · 2009
23. ISO 6872 · 2015
24. Fracture surface analysis of dental ceramics: clinically failed restorations
25. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
26. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
27. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
28. Resin bonding to oxide ceramics for dental restorations10.1163/156856109X432721 ↗
29. Bonding to oxide ceramics—laboratory testing versus clinical outcome10.1016/j.dental.2014.06.007 ↗
30. A prospective study of the incidence of asymptomatic pulp necrosis following crown preparation10.1111/iej.12340 ↗
31. Recent trends in surface treatment methods for bonding composite cement to zirconia: a Review
32. Comparison of the mechanical properties of translucent zirconia and lithium disilicate10.1016/j.prosdent.2017.08.004 ↗
33. Three-dimensional finite element analysis of weakened roots restored with different cements in combination with titanium alloy posts10.1097/00029330-200602020-00007 ↗
34. Effect of thermocycling on bond strength of luting cements to zirconia ceramic10.1016/j.dental.2005.04.016 ↗
35. Effect of silica coating combined to a MDP-based primer on the resin bond to Y-TZP ceramic10.1002/jbm.b.31684 ↗
36. Sorption and solubility of luting cements in different solutions10.4012/dmj.27.702 ↗
37. Effects of airborne-particle abrasion protocol choice on the surface characteristics of monolithic zirconia materials and the shear bond strength of resin cement10.1016/j.ceramint.2015.09.104 ↗
38. Consecutive case series of monolithic and minimally veneered zirconia restorations on teeth and implants: up to 68 months10.11607/prd.2270 ↗
39. Effect of primer-cement systems with different functional phosphate monomers on the adhesion of zirconia to dentin10.1016/j.jmbbm.2018.08.003 ↗
40. Chemical interaction mechanism of 10-MDP with zirconia10.1038/srep45563 ↗
41. Ultrasonic cleaning of silica-coated zirconia influences bond strength between zirconia and resin luting material10.4012/dmj.27.842 ↗
42. Survival-rate analysis of surface treated dental zirconia (Y-TZP) ceramics10.1007/s10856-014-5217-1 ↗
43. A 5-year retrospective study of survival of zirconia single crowns fitted in a private clinical setting10.1016/j.jdent.2012.02.011 ↗
44. Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers' instructions of the cements only10.1007/s00784-007-0151-y ↗
45. Early bond strength of two resin cements to Y-TZP ceramic using MPS or MPS/4-META silanes10.1007/s10266-010-0144-1 ↗
46. Effect of air-particle abrasion protocols on the biaxial flexural strength, surface characteristics and phase transformation of zirconia after cyclic loading10.1016/j.jmbbm.2013.01.005 ↗
47. Adhesion to zirconia used for dental restorations: a systematic review and meta-analysis
48. Fatigue limit of polycrystalline zirconium oxide ceramics: effect of grinding and low-temperature aging10.1016/j.jmbbm.2016.01.006 ↗
49. A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part I: single crowns10.1111/j.1600-0501.2007.01467.x ↗
50. The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study10.1016/j.prosdent.2006.08.010 ↗
51. Mechanical properties of dental zirconia ceramics changed with sandblasting and heat treatment10.4012/dmj.27.408 ↗
52. Fatigue behavior in water of Y-TZP zirconia ceramics after abrasion with 30 μm silica-coated alumina particles10.1016/j.dental.2010.10.003 ↗
53. ADM guidance-ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
54. Ceramic strengthening by tuning the elastic moduli of resin-based luting agents10.1016/j.dental.2017.01.002 ↗
55. Strengthening of porcelain provided by resin cements and flowable composites10.2341/15-025-L ↗
56. Ultrathin monolithic zirconia veneers: reality or future? Report of a clinical case and one-year follow-up10.2341/16-350-T ↗
57. Air-particle abrasion on zirconia ceramic using different protocols: effects on biaxial flexural strength after cyclic loading, phase transformation and surface topography10.1016/j.jmbbm.2013.04.018 ↗
58. CAD/CAM ceramic restorative materials for natural teeth10.1177/0022034518779759 ↗
59. Roughness, surface energy, and superficial damages of CAD/CAM materials after surface treatment10.1007/s00784-018-2365-6 ↗
60. Surface and intra-pulpal temperature rises during tooth bleaching: an in vitro study10.1038/sj.bdj.4812558 ↗
61. Bonding of composite cements to zirconia: a systematic review and meta-analysis of in vitro studies10.1016/j.jmbbm.2018.02.008 ↗
62. Microtensile bond strength of a resin cement to silica-coated and silanized In-Ceram Zirconia before and after aging
63. Biaxial flexure tests of ceramic substrates
64. Stress fatigue: basic principles and prosthodontic implications
65. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods10.1016/j.dental.2005.11.040 ↗
66. Comparison of resin bonding improvements to zirconia between one-bottle universal adhesives and tribochemical silica coating, which is better?10.1016/j.dental.2015.12.014 ↗
67. Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin10.1016/j.dental.2009.08.008 ↗
68. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
69. Damage accumulation and fatigue life of particle-abraded ceramics
70. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗