journal article·2019-02

Load-bearing capacity under fatigue and survival rates of adhesively cemented yttrium-stabilized zirconia polycrystal monolithic simplified restorations

Camila Pauleski Zucuni, Andressa Borin Venturini, Catina Prochnow, Gabriel Kalil Rocha Pereira, Luiz Felipe Valandro

Publisher page

Abstract

This study evaluated the fatigue failure load, number of cycles for failure and survival probability of 2nd and 3rd generation yttrium-stabilized zirconia (YSZ) adhesively cemented to a dentin analogue substrate. Disc-shaped specimens (n = 10; Ø = 10 mm; thickness = 1.0 mm) were produced from four 2nd generation YSZs (Lava Plus, 3M ESPE; Vita In-Ceram YZ-HT, VITA Zahnfabrik; Zirlux FC, Ivoclar Vivadent; Katana ML-HT, Kuraray) and two 3rd generation YSZs (Katana UTML and Katana STML, Kuraray). Each YSZ disc was adhesively cemented (Multilink Automix System) onto its dentin analogue pair (epoxy resin, Ø = 10 mm; thickness = 2.5 mm). Fatigue tests were conducted through step-stress approach (load ranging from 400 to 2600 N; step-size of 200 N; 20,000 cycles per step, 20 Hz) and the obtained data were analyzed using Kaplan Meier and Mantel-Cox tests. Surface topography and phase transformation (m-, t-, and c-phases) inspections after particle air-abrasion of the YSZs were performed, as well as fractographic analysis of the failed specimens. Second-generation zirconia materials presented higher fatigue failure load, number of cycles for failure, and survival probability than 3rd generation. Similar topographical characteristics of the YSZs could be noted. Phase transformation (t- to m-phase) after YSZ air-abrasion was only observed for 2nd generation materials. All failures started from the surface/sub-surface defects located at the cementation interface. 2nd generation zirconia presented higher load-bearing capacity under cyclic loading than 3rd generation materials.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Resin elasticity and the strengthening of all-ceramic restorations10.1177/154405910708600606 ↗
2. Fatigue resistance of Y-TZP/porcelain crowns is not influenced by the conditioning of the intaglio surface10.2341/14-166-L ↗
3. Does air particle abrasion affect the flexural strength and phase transformation of Y-TZP? A systematic review and meta-analysis10.1016/j.dental.2016.03.021 ↗
4. Adhesive cementation promotes higher fatigue resistance to zirconia crowns10.2341/16-002-L ↗
5. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
6. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
7. Ageing kinetics and strength of airborne-particle abraded 3Y-TZP ceramics10.1016/j.dental.2017.04.014 ↗
8. Mechanical performance of Y-TZP monolithic ceramic after grinding and aging: survival estimates and fatigue strength10.1016/j.jmbbm.2018.07.041 ↗
9. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
10. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
11. Size and shape of the human first permanent molar: a Fourier analysis of the occlusal and equatorial outlines10.1002/(SICI)1096-8644(199903)108:3<281::AID-AJPA4>3.0.CO;2-# ↗
12. Loading frequencies up to 20 Hz as an alternative to accelerate fatigue strength tests in a Y-TZP ceramic10.1016/j.jmbbm.2016.01.008 ↗
13. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
14. Effect of accelerated aging on the fracture toughness of zirconias10.1016/j.prosdent.2015.08.020 ↗
15. Crystallographic and morphological analysis of sandblasted highly translucent dental zirconia10.1016/j.dental.2017.12.008 ↗
16. Aging resistance of surface-treated dental zirconia10.1016/j.dental.2014.11.018 ↗
17. ISO 6872-2015, 2015. Dentistry – Ceramic Materials. International Organization for Standardization.
18. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
19. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
20. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
21. Effect of grain size on the monoclinic transformation, hardness, roughness and modulus of aged partially stabilized zirconia10.1016/j.dental.2015.09.014 ↗
22. In vitro fatigue resistance of CAD/CAM composite resin and ceramic posterior occlusal veneers10.1016/S0022-3913(10)60111-4 ↗
23. Fatigue failure load of two resin-bonded zirconia-reinforced lithium silicate glass-ceramics: effect of ceramic thickness10.1016/j.dental.2018.03.004 ↗
24. Effects of airborne-particle abrasion protocol choice on the surface characteristics of monolithic zirconia materials and the shear bond strength of resin cement10.1016/j.ceramint.2015.09.104 ↗
25. Quantitative study of bite force during sleep associated bruxism10.1046/j.1365-2842.2001.00692.x ↗
26. The effect of a layer of resin luting agent on the biaxial flexure strength of two all-ceramic systems10.1016/j.prosdent.2005.02.012 ↗
27. Structural ceramic nanocomposites: a review of properties and powders' Synthesis methods10.3390/nano5020656 ↗
28. Nanomechanics of Hall–Petch relationship in nanocrystalline materials10.1016/j.pmatsci.2009.03.008 ↗
29. Effect of grinding with diamond-disc and-bur on the mechanical behavior of a Y-TZP ceramic10.1016/j.jmbbm.2014.05.010 ↗
30. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
31. Zirconia as a ceramic biomaterial, a review10.1016/S0142-9612(98)00010-6 ↗
32. How does hydrofluoric acid etching affect the cyclic load-to-failure of lithium disilicate restorations?10.1016/j.jmbbm.2018.07.040 ↗
33. Optical properties of zirconia ceramics for esthetic dental restorations: a systematic review10.1016/j.prosdent.2017.07.009 ↗
34. Dental ceramics: an update10.4103/0972-0707.73379 ↗
35. Three generations of zirconia: from veneered to monolithic. Part I
36. Three generations of zirconia: from veneered to monolithic. Part II
37. Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: conventional ceramic etching vs etch & prime one-step primer10.1016/j.dental.2018.04.012 ↗
38. Optical properties and light irradiance of monolithic zirconia at variable thicknesses10.1016/j.dental.2015.06.016 ↗
39. Effect of different treatments on the flexural strength of fully versus partially stabilized monolithic zirconia10.1016/j.prosdent.2016.10.031 ↗
40. Surface and intra-pulpal temperature rises during tooth bleaching: an in vitro study10.1038/sj.bdj.4812558 ↗
41. The effect of ceramic surface treatment on bonding to densely sintered alumina ceramic10.1016/j.prosdent.2004.12.002 ↗
42. The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs10.1016/j.dental.2018.01.010 ↗
43. Load-bearing capacity of lithium disilicate and ultra-translucent zirconias10.1016/j.jmbbm.2018.08.023 ↗
44. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗