journal article·2022-11

Zirconia fixed dental prostheses fabricated by 3D gel deposition show higher fracture strength than conventionally milled counterparts

Kerstin Rabel, Julian Nold, Daniela Pehlke, James Shen, Anže Abram, Andraž Kocjan, Siegbert Witkowski, Ralf-Joachim Kohal

Publisher page

Abstract

Zirconia restorations, which are fabricated by additive 3D gel deposition and do not require glazing like conventional restorations, were introduced as "self-glazed" zirconia restorations into dentistry. This in vitro investigation characterized the surface layer, microstructure and the fracture and aging behavior of "self-glazed" zirconia (Y-TZPSG) three-unit fixed dental prostheses (FDP) and compared them to conventionally CAD/CAM milled and glazed controls (Y-TZPC-FDPs). For this purpose, the FDPs were analyzed by (focused ion beam) scanning electron microscopy, laserscanning microscopy, energy dispersive X-ray spectroscopy, X-ray diffraction and a dynamic and static loading test. For the latter, half of the samples of each material group (n = 16) was subjected to 5 million cycles of thermocyclic loading (98N) in an aqueous environment in a chewing simulator. Afterwards, all FDPs were loaded to fracture. Y-TZPSG-FDPs demonstrated a comparable elemental composition but higher surface microstructural homogeneity and fracture strength compared to Y-TZPC-FDPs. Microstructural flaws within the FDPs' surfaces were identified as fracture origins. The high fracture strength of the Y-TZPSG-FDPs was attributed to a finer-grained microstructure with fewer surface flaws compared to the Y-TZPC-FDPs which showed numerous flaws in the glaze overlayer. A decrease in fracture strength after dynamic loading from 5165N to 4507N was observed for the Y-TZPSG-FDPs, however, fracture strength remained statistically significantly above the one measured for Y-TZPC-FDPs (before chewing simulation: 1923N; after: 2041N). Within the limits of this investigation, it can therefore be concluded that Y-TZPSG appears to be stable for clinical application suggesting further investigations to prove clinical applicability.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Assessment of novel long-lasting ceria-stabilized zirconia-based ceramics with different surface topographies as implant materials10.1002/adfm.201702512 ↗
2. Distinct cell functions of osteoblasts on UV-functionalized titanium-and zirconia-based implant materials are modulated by surface topography10.1089/ten.tec.2012.0695 ↗
3. Biaxial flexure strength and low temperature degradation of Ce-TZP/Al2O3 nanocomposite and Y-TZP as dental restoratives10.1002/jbm.b.31131 ↗
4. Suitability of 3D printed pieces of nanocrystalline zirconia for dental applications10.1016/j.dental.2020.01.006 ↗
5. The influence of yttrium-segregation-dependent phase partitioning and residual stresses on the aging and fracture behaviour of 3Y-TZP ceramics10.1016/j.actbio.2017.08.014 ↗
6. What future for zirconia as a biomaterial?10.1016/j.biomaterials.2005.07.034 ↗
7. Critical effect of cubic phase on aging in 3 mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗
8. Ceramics for medical applications: a picture for the next 20 years10.1016/j.jeurceramsoc.2008.08.025 ↗
9. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
10. The tetragonal‐monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
11. Esthetic appearances of anatomic contour zirconia crowns made by additive wet deposition and subtractive dry milling: a self-controlled clinical trial10.1016/j.prosdent.2019.02.016 ↗
12. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
13. Osseointegration of zirconia implants compared with titanium: an in vivo study10.1186/1746-160X-4-30 ↗
14. Effect of feldspar porcelain coating upon the wear behavior of zirconia dental crowns10.1016/j.wear.2012.10.016 ↗
15. Ceramic steel?
16. Structure and thermomechanical properties of partially stabilized zirconia in the CaO‐ZrO2 system10.1111/j.1151-2916.1972.tb11241.x ↗
17. Zirconia based dental ceramics: structure, mechanical properties, biocompatibility and applications10.1039/C6DT03484E ↗
18. Zirconia and its novel compositions: what do clinicians need to know?
19. Biocompatibility of zirconia
20. Stability of tetragonal ZrO2 particles in ceramic matrices10.1111/j.1151-2916.1982.tb09946.x ↗
21. A comparison of the marginal fit and mechanical properties of a zirconia dental crown using CAM and 3DSP10.1108/RPJ-03-2018-0053 ↗
22. Concerns of hydrothermal degradation in CAD/CAM zirconia10.1177/0022034509354193 ↗
23. Zirconia ceramics: clinical and biological aspects in dentistry
24. Loaded custom-made zirconia and titanium implants show similar osseointegration: an animal experiment10.1902/jop.2004.75.9.1262 ↗
25. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
26. Three-dimensional trueness and margin quality of monolithic zirconia restorations fabricated by additive 3D gel deposition10.1016/j.jpor.2020.01.002 ↗
27. Self-glazed zirconia reducing the wear to tooth enamel10.1016/j.jeurceramsoc.2015.11.029 ↗
28. Cubic‐formation and grain‐growth mechanisms in tetragonal zirconia polycrystal10.1111/j.1151-2916.2003.tb03483.x ↗
29. Nanoroughening of sandblasted 3Y-TZP surface by alumina coating deposition for improved osseointegration and bacteria reduction10.1016/j.jeurceramsoc.2019.05.051 ↗
30. Influence of grain size and veneer firing process on the flexural strength of zirconia ceramics10.1111/j.1600-0722.2012.00958.x ↗
31. The effect of mechanical fatigue and accelerated ageing on fracture resistance of glazed monolithic zirconia dental bridges10.1016/j.jeurceramsoc.2017.04.048 ↗
32. Zirconia biocompatibility in animal studies - a systematic review10.4028/www.scientific.net/DDF.376.12 ↗
33. Quinn · 2007
34. Controlling osteoblast morphology and proliferation via surface micro-topographies of implant biomaterials10.1038/s41598-020-69685-6 ↗
35. Fatigue and wear behaviour of zirconia materials10.1016/j.jmbbm.2020.103970 ↗
36. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part I: single crowns (SCs)10.1016/j.dental.2015.02.011 ↗
37. On the behaviour of zirconia-based dental materials: a review10.1016/j.jmbbm.2021.104861 ↗
38. Fractography of self-glazed zirconia with improved reliability10.1016/j.jeurceramsoc.2017.03.008 ↗
39. Wear performance of self-glazed zirconia crowns with different amount of occlusal adjustment after 6 months of clinical use10.1080/17436753.2018.1477567 ↗
40. Comparison of four monolithic zirconia materials with conventional ones: contrast ratio, grain size, four-point flexural strength and two-body wear10.1016/j.jmbbm.2015.11.040 ↗
41. Computer-aided design and fabrication of dental restorations: current systems and future possibilities10.14219/jada.archive.2006.0389 ↗
42. Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures10.1016/j.actbio.2008.12.016 ↗
43. The application potential of self-glazed zirconia crowns confirmed by easy grinding and polishing of the enamel-like surface
44. Digital dentistry calls the change of ceramics and ceramic processes10.1080/17436753.2018.1511337 ↗
45. Friction and wear behaviors of dental ceramics against natural tooth enamel10.1016/j.jeurceramsoc.2012.03.021 ↗
46. Marginal adaptation of castable ceramic crowns10.1016/0022-3913(91)90408-O ↗
47. Fracture resistance of additively manufactured zirconia crowns when cemented to implant supported zirconia abutments: an in vitro study10.1111/jopr.13103 ↗
48. Current status on lithium disilicate and zirconia: a narrative review10.1186/s12903-019-0838-x ↗
49. Strength, toughness and aging stability of highly-translucent Y-TZP ceramics for dental restorations10.1016/j.dental.2016.09.025 ↗
50. Trade-off between fracture resistance and translucency of zirconia and lithium-disilicate glass ceramics for monolithic restorations10.1016/j.actbio.2019.04.043 ↗
51. Bonding of novel self-glazed zirconia dental ceramics10.1080/17436753.2018.1463935 ↗
52. Fatigue behaviours of the zirconia dental restorations prepared by two manufacturing methods10.1080/17436753.2017.1336365 ↗
53. Fatigue sensitivity of Y‐TZP to microscale sharp‐contact flaws10.1002/jbm.b.30174 ↗
54. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗