journal article·2022-10Open access

Effect of simulated brushing and disinfection on the surface roughness and color stability of CAD-CAM denture base materials

Gülce Çakmak, Mustafa Borga Donmez, Canan Akay, Sevda Atalay, Marcella Silva de Paula, Martin Schimmel, Burak Yilmaz

Abstract

To evaluate the effect of simulated brushing and chemical disinfection on the surface roughness and color stability of CAD-CAM denture base materials and to compare with those of a heat-cured denture base material. Disk-shaped specimens (Ø 10mm × 2 mm) were prepared from 3 CAD-CAM denture base resins (AvaDent, Ava; Merz M-PM, Merz; Polident d.o.o, Poli) and a heat-cured polymethylmethacrylate resin (Promolux, Conv) (n = 30). After polishing, baseline surface roughness (Ra) and color coordinates were measured. The measurements were repeated after 20000 cycles of simulated brushing, and the specimens were divided into 3 groups according to disinfection protocol (distilled water, 1% sodium hypochlorite (NaOCl), and effervescent tablet) (n = 10). After 9 cleaning cycles over a period of 20 days, Ra and color coordinates were remeasured. Color differences (ΔE00) were calculated by using CIEDE2000 formula. One-way analysis of variance (ANOVA) and pairwise t-tests were used to analyze Ra and ΔE00 data, while repeated measures ANOVA test was used to compare baseline, after brush, and after disinfection Ra values (α = 0.05). Brushing did not affect the Ra values of tested materials (P ≥ .08). Both before and after brushing, Merz and Conv had higher Ra values than Poli and Ava (P < .001). Among disinfectants, effervescent tablet led to the lowest Ra for Merz (P = .003) and the highest Ra for Poli (P ≤ .039). Only NaOCl resulted in significant differences among the Ra of materials (P < .001), as Merz and Conv had higher Ra values than Poli (P ≤ .002). Repeated measures ANOVA revealed that effervescent tablet disinfection of Merz led to lower Ra values than those of baseline and after brushing (P ≤ .042). After brushing, Ava and Conv had higher ΔE00 values compared with Merz and Poli (P ≤ .015). When compared with other disinfection protocols, effervescent tablet led to higher ΔE00 values for Merz and Poli (P < .001). Significant differences were observed among materials when NaOCl was used; Conv had higher ΔE00 values than Ava and Merz (P = .004). Brushing did not increase the surface roughness of materials. Disinfection protocol's effect on the surface roughness varied. The effect of brushing on the color of materials varied; color of Ava and Conv was affected from brushing more than the other materials. Color stability of materials varied depending on the disinfection protocol. Effervescent tablet caused higher color change with Merz and Poli compared with other disinfectants. NaOCl led to small color change for Poli, Ava, and Merz materials.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. A comparison of the surface properties of CAD/CAM and conventional polymethylmethacrylate (PMMA)10.1111/jopr.13033 ↗
2. Stainability of acrylic resin materials used in CAD-CAM and conventional complete dentures10.1016/j.prosdent.2019.07.004 ↗
3. Surface roughness analysis of prepolymerized CAD/CAM dental acrylic resins following combined surface treatments10.2478/msp-2021-0018 ↗
4. Power brushing and chemical denture cleansers induced color changes of pre-polymerized CAD/CAM denture acrylic resins10.1088/2053-1591/ac1e47 ↗
5. Color stability of 3D-printed denture resins: effect of aging, mechanical brushing and immersion in staining medium10.4047/jap.2021.13.3.160 ↗
6. Effect of aging and mechanical brushing on surface roughness of 3D printed denture resins: a profilometer and scanning electron microscopy analysis10.3233/THC-212974 ↗
7. Optical properties and surface roughness of prepolymerized poly(methyl methacrylate) denture base materials10.1016/j.prosdent.2018.03.001 ↗
8. Effects of denture cleansers on heat-polymerized acrylic resin: a five-year-simulated period of use10.1590/0103-6440201300120 ↗
9. Evaluation of flexural strength and surface properties of prepolymerized CAD/CAM PMMA-based polymers used for digital 3D complete dentures
10. Effect of different disinfection protocols on the surface properties of CAD-CAM denture base materials
11. Effect of toothbrush/dentifrice abrasion on weight variation, surface roughness, surface morphology and hardness of conventional and CAD/CAM denture base materials10.4012/dmj.2019-226 ↗
12. Surface roughness of acrylic resins used for denture base after chemical disinfection: a systematic review and meta-analysis10.1111/ger.12529 ↗
13. Effect of toothbrushes and denture brushes on heat-polymerized acrylic resins
14. Effects of the peracetic acid and sodium hypochlorite on the colour stability and surface roughness of the denture base acrylic resins polymerised by microwave and water bath methods10.1111/j.1741-2358.2012.00640.x ↗
15. Effect of artificial toothbrushing and water storage on the surface roughness and micromechanical properties of tooth-colored CAD-CAM materials10.1016/j.prosdent.2016.08.034 ↗
16. Effect of thermal cycling and disinfection on colour stability of denture base acrylic resin10.1111/j.1741-2358.2012.00676.x ↗
17. CAD/CAM complete denture resins: an in vitro evaluation of color stability10.1111/jopr.13246 ↗
18. Effect of repeated microwave disinfection on the surface hardness of a heat-cured denture base resin: an in vitro study10.4103/ccd.ccd_271_18 ↗
19. Evaluation of the color stability of temporary materials produced with CAD/CAM10.17219/dmp/126745 ↗
20. The effect of cleaning solutions on a denture base material: elimination of candida albicans and alteration of physical properties10.1111/jopr.12539 ↗
21. Effect of toothbrushing, chemical disinfection and thermocycling procedures on the surface microroughness of denture base acrylic resins10.1111/j.1741-2358.2011.00582.x ↗
22. Quantitative evaluation of the progressive wear of powered interproximal reduction systems after repeated use : an in vitro study10.1007/s00056-019-00200-x ↗
23. Cytotoxic potential of denture base and reline acrylic resins after immersion in disinfectant solutions10.1016/j.prosdent.2018.01.001 ↗
24. Effect of cleansers on denture base resins' structural properties
25. Color stability, surface roughness and flexural strength of an acrylic resin submitted to simulated overnight immersion in denture cleansers10.1590/0103-6440201302151 ↗
26. Long-term microwaving of denture base materials: effects on dimensional, color and translucency stability10.1590/1678-7757-2017-0536 ↗
27. Effect of denture cleansers on color stability, surface roughness, and hardness of different denture base resins10.4103/0972-4052.197940 ↗
28. Acrylic resins in the CAD/CAM technology: a systematic literature review10.17219/dmp/124697 ↗
29. Determining color difference thresholds in denture base acrylic resin10.1016/j.prosdent.2015.06.009 ↗
30. Complete denture hygiene solutions: antibiofilm activity and effects on physical and mechanical properties of acrylic resin10.1590/1678-7757-2020-0948 ↗
31. Effect of surface sealant agents on the surface roughness and color stability of denture base materials10.1016/j.prosdent.2016.03.007 ↗
32. Effect of denture cleaning on abrasion resistance and surface topography of polymerized CAD CAM acrylic resin denture base10.19082/4281 ↗
33. Adverse effects on PMMA caused by mechanical and combined methods of denture cleansing10.1590/0103-6440201300028 ↗
34. Abrasiveness of conventional and specific denture-cleansing dentifrices10.1590/S0103-64402012000200011 ↗
35. Time-lasting ceramic stains and glaze: a toothbrush simulation study10.1111/jerd.12590 ↗
36. Microbicidal effect of 405-nm blue LED light on Candida albicans and Streptococcus mutans dual-species biofilms on denture base resin10.1007/s10103-021-03323-z ↗
37. Activated charcoal toothpastes do not increase erosive tooth wear10.1016/j.jdent.2021.103677 ↗