Surface properties and flexural fatigue strength of an advanced lithium disilicate

Júlia Saccol Freitas, Luiza Freitas Brum Souza, Gabriel Kalil Rocha Pereira, Liliana Gressler May

Publisher page

Abstract

The aim of this study was to evaluate the surface properties and fatigue mechanical behavior of an advanced lithium disilicate ceramic in comparison to lithium disilicate and zirconia. First, discs (n = 15, diameter = 13.5 mm and thickness = 1.2 mm) were made from the following materials: 4Y-PSZ - 4% mol yttria-stabilized zirconia (IPS e.max ZirCAD A2); LD - lithium disilicate (IPS e.max CAD); ALD - advanced lithium disilicate (CEREC Tessera). The specimens were crystalized/sintered and subsequently analyzed by a rugosimeter (Mitutoyo SJ-410) to determine surface roughness (parameters Ra and Rz). Specimens were subjected to biaxial flexural fatigue testing using the step-test method (20 Hz; 10,000 cycles per step; initial stress of 200 MPa; and step size of 25 MPa) until specimen fracture. Statistical analyses included Shapiro-Wilk, Kruskal-Wallis, and post-hoc tests for roughness data, while survival analysis (Kaplan-Meier and Mantel-Cox) and reliability analysis (Weibull modulus) were applied to flexural fatigue strength data. Hardness (Vickers) results were submitted to analysis of variance (1-way ANOVA) and Tukey's test. Zirconia (4Y-PSZ) showed higher FFS, CFF (467 MPa and 115216 cycles) and survival compared to the other materials. ALD had the lowest FFS, CFF (215 MPa and 11,908 cycles) and survival. ALD showed lower Weibull modulus (m = 6.63 for FFS; m = 1.27 for CFF) than LD for FFS (m = 17.33), and lower than LD (m = 4.64) and 4Y-PSZ (m = 6.69) for CFF. ALD showed the lowest Ra (0.07 μm) and Rz (1.05 μm) values, while 4Y-PSZ (Ra = 0.22 μm; Rz = 1.91 μm) and LD (Ra = 0.21 μm; Rz = 2.17 μm) showed higher and similar values. Zirconia (4-YPSZ) was the hardest material, while lithia-based ceramics (LD and ALD) presented the lowest and similar hardness values. Fractures originated in surface defects in the tensile stress concentration region. ALD has lower flexural fatigue strength compared to the other tested materials, along with higher variability (lower structural reliability).
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Dental materials and restorations · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Clinical marginal and internal adaptation of maxillary anterior single all-ceramic crowns and 2-year randomized controlled clinical trial10.1111/jopr.12217 ↗
2. Assessment of the hardness of disks fabricated by zirconia reinforced lithium silicate glass ceramic; VITA suprinity and IPS e-max CAD
3. Fracture toughness and hardness evaluation of three pressable all-ceramic dental materials10.1016/S0300-5712(03)00025-3 ↗
4. Fracture toughness of two lithium disilicate dental glass ceramics10.1016/j.prosdent.2016.02.009 ↗
5. Extended glaze firing on ceramics for hard machining: crack healing, residual stresses, optical and microstructural aspects10.1016/j.dental.2016.12.002 ↗
6. Clinical performance of chairside monolithic lithium disilicate glass-ceramic CAD-CAM crowns10.1111/jerd.12531 ↗
7. Fatigue of restorative materials10.1177/10454411010120040501 ↗
8. Fracture rates and lifetime estimations of CAD/CAM allceramic restorations10.1177/0022034515608187 ↗
9. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
10. Translucency, color stability, and biaxial flexural strength of advanced lithium disilicate ceramic after coffee thermocyclin10.1111/jerd.12960 ↗
11. Emerging ceramic-based materials for dentistry10.1177/0022034514553627 ↗
12. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
13. Loading frequencies up to 20 Hz as an alternative to accelerate fatigue strength tests in a Y-TZP ceramic10.1016/j.jmbbm.2016.01.008 ↗
14. On the assignment of quartz-like LiAlSi2O6 - SiO2 solid solutions in dental lithium silicate glass-ceramics: virgilite, high quartz, low quartz or stuffed quartz derivatives?10.1016/j.dental.2022.07.009 ↗
15. 1997
16. 2015
17. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
18. Concurrent kinetics of crystallization and toughening in multicomponent biomedical SiO2-Li2O-P2O5-ZrO2 glass-ceramics10.1016/j.jnoncrysol.2020.120607 ↗
19. Wear resistance and abrasiveness of CAD-CAM monolithic materials10.1016/j.prosdent.2018.05.011 ↗
20. Load-bearing properties of minimal-invasive monolithic lithium disilicate and zirconia occlusal onlays: finite element and theoretical analyses10.1016/j.dental.2013.04.004 ↗
21. Polishing effects and wear performance of chairside CAD/CAM materials10.1007/s00784-018-2473-3 ↗
22. Surface properties of a new lithium disilicate glass-ceramic aftergrinding10.1007/s10856-021-06592-w ↗
23. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
24. Microstructural considerations for novel lithium disilicate glass ceramics: a review10.1111/jerd.12864 ↗
25. In-lab simulation of CAD/CAM milling of lithium disilicate glass-ceramic specimens: effect on the fatigue behavior of the bonded ceramic10.1016/j.jmbbm.2021.104604 ↗
26. Clinical survival of chair-side generated monolithic lithium disilicate crowns:10-year results10.1007/s00784-017-2271-3 ↗
27. Properties and clinical application of three types of dental glass-ceramics and ceramics for CAD-CAM technologies10.3390/ma3063700 ↗
28. In vitro mastication sim- ulation and wear test of virgilite and advanced lithium disilicate ceramics10.11607/ijp.7820 ↗
29. Fracture toughness testing of brittle materials10.1179/imr.1993.38.2.53 ↗
30. Clinical performance of two different CAD/CAM fabricated ceramic crowns: 2-year results10.1016/j.prosdent.2015.02.016 ↗
31. Machinability of lithium disilicate glass ceramicinin vitrodental diamond bur adjusting process10.1016/j.jmbbm.2015.08.003 ↗
32. CAD/CAM ceramic restorative materials for natural teeth10.1177/0022034518779759 ↗
33. Bonding behaviour of polytherketoneketone to methylmethacrylate- and dimethacrylate-based polymers
34. Effect of material characteristics and/or surface topography on biofilm development10.1111/j.1600-0501.2006.01353.x ↗
35. Brittleness index of machinable dental materials and its relation to the marginal chipping factor10.1016/j.jdent.2007.07.002 ↗
36. Biaxial flexure tests of ceramics substrates
37. Friction and wear behaviors of dental ceramics against natural tooth enamel10.1016/j.jeurceramsoc.2012.03.021 ↗
38. Wide applicability10.1115/1.4010337 ↗
39. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
40. Stress fatigue: basic principies and prosthodontic implications
41. Dental ceramics for restoration and metal veneering
42. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
43. A critical review of dental lithia-based glass–ceramics10.1177/00220345221142755 ↗