Soft machining-induced surface and edge chipping damage in pre-crystalized lithium silicate glass ceramics
Source abstract
Abstract
Soft machining is a key procedure in fabrication of high-strength lithium-based silicate glass ceramic (LS) restorations. This paper reports on the diamond machining-induced surface and edge chipping damage in two pre-crystalized LS materials: pre-crystallized lithium metasilicate/orthophosphate glass ceramic (Pre-LS, IPS e.max CAD) and pre-crystallized zirconia-containing lithium metasilicate glass ceramic (Pre-ZLS, Vita Suprinity). Indentation techniques were used to measure the material mechanical properties. Soft machining was conducted using a robotic controlled apparatus mimicking dental CAD/CAM machining processes at different removal rates and enabling in-process force measurement. Machined surface roughness was assessed using 3D confocal optical profilometry in terms of the average and maximum surface heights. Scanning electron microscopy was used to assess diamond tool and machined surface and edge morphology. Soft machining of both materials was dominated by brittle fracture mixed with localized ductile flow. However, the higher brittleness index of Pre-ZLS than Pre-LS yielded higher degrees of machining-induced conchoidal fractures in Pre-ZLS in comparison with irregular fractures in Pre-LS. Thus, much larger surface roughness and deeper edge chipping damage were produced in Pre-ZLS than Pre-LS. Machining forces for Pre-ZLS were significantly smaller than Pre-LS, due to the lower machinability index associated with a complex relation of the mechanical properties as well as less debris adhesion for Pre-ZLS than Pre-LS. Further, increased material removal rates resulted in significantly increased machining forces, maximum surface roughness and fracture, and edge chipping damage in both Pre-ZLS and Pre-LS materials. Therefore, optimization of soft machining processes needs to be practiced to achieve accepted surface and edge quality at balanced removal rates.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Advanced Surface Polishing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Fracture, roughness and phase transformation in CAD/CAM milling and subsequent surface treatments of lithium metasilicate/disilicate glass-ceramics10.1016/j.jmbbm.2017.06.015 ↗
2. Influence of CAD/CAM milling, sintering and surface treatments on the fatigue behavior of lithium disilicate glass ceramic10.1016/j.jmbbm.2020.104133 ↗
3. Advancements in CAD/CAM technology: options for practical implementation10.1016/j.jpor.2016.01.003 ↗
4. Influence of heat-treatment protocols on mechanical behavior of lithium silicate dental ceramics10.1111/ijac.13257 ↗
5. Edge chipping resistance and flexural strength of polymer infiltrated ceramic network and resin nanoceramic restorative materials10.1016/j.prosdent.2016.02.014 ↗
6. Crack-healing during two-stage crystallization of biomedical lithium (di)silicate glass-ceramics10.1016/j.dental.2019.05.013 ↗
7. Fracture rates and lifetime estimations of CAD/CAM all-ceramic restorations10.1177/0022034515608187 ↗
8. Report on fractures of trilayered all-ceramic fixed dental prostheses10.1016/j.csefa.2016.10.001 ↗
9. Chairside CAD/CAM materials. Part 1: measurement of elastic constants and microstructural characterization10.1016/j.dental.2016.10.009 ↗
10. Fracture toughness testing of biomedical ceramic-based materials using beams, plates and discs10.1016/j.jeurceramsoc.2018.08.012 ↗
11. Cracking of porcelain surfaces arising from abrasive grinding with a dental air turbine10.1111/j.1532-849X.2011.00760.x ↗
12. Machinability of CAD-CAM materials10.1016/j.prosdent.2016.09.022 ↗
13. Machinability: zirconia-reinforced lithium silicate glass ceramic versus lithium disilicate glass ceramic10.1016/j.jmbbm.2019.103435 ↗
14. Nucleation mechanisms in a SiO2-Li2O-P2O5-ZrO2 biomedical glass-ceramic: insights on crystallisation, residual glasses and Zr4+structural environment10.1016/j.jeurceramsoc.2021.12.009 ↗
15. Damage tolerance of indirect restorative materials (including PICN) after simulated bur adjustments10.1016/j.dental.2015.03.007 ↗
16. Grinding damage assessment for CAD-CAM restorative materials10.1016/j.dental.2016.12.004 ↗
17. How and when does fabrication damage adversely affect the clinical performance of ceramic restorations?10.1016/j.dental.2012.07.001 ↗
18. El-Meliegy · 2012
19. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
20. In-vitro wear of natural tooth surface opposed with zirconia reinforced lithium silicate glass ceramic after accelerated ageing10.1016/j.dental.2017.12.010 ↗
21. Phase characterization of lithium silicate biomedical glass-ceramics produced by two-stage crystallization10.1016/j.jnoncrysol.2019.01.027 ↗
22. Nucleation kinetics of lithium metasilicate in ZrO2-bearing lithium disilicate glasses for dental application10.1111/ijag.12011 ↗
23. Influence of CAD/CAM tool and material on tool wear and roughness of dental prostheses after milling10.1016/j.prosdent.2014.12.021 ↗
24. Ceramic dental biomaterials and CAD/CAM technology: state of the art10.1016/j.jpor.2014.07.003 ↗
25. Concurrent kinetics of crystallization and toughening in multicomponent biomedical SiO2-Li2O-P2O5-ZrO2 glass-ceramics10.1016/j.jnoncrysol.2020.120607 ↗
26. Grasping the lithium hype: insights into modern dental lithium silicate glass-ceramics10.1016/j.dental.2021.12.013 ↗
27. Inner marginal strength of CAD/CAM materials is not affected by machining protocol
28. Bioactive and inert dental glass-ceramics10.1002/jbm.a.35923 ↗
29. Survival rate of resin and ceramic inlays, onlays, and overlays: a systematic review and meta-analysis10.1177/0022034516652848 ↗
30. The effect of milling and postmilling procedures on the surface roughness of CAD/CAM materials10.1111/jerd.12326 ↗
31. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
32. Surface and bulk residual stresses in Li2O-2SiO2 glass-ceramics10.1016/j.jnoncrysol.2007.04.007 ↗
33. Indentation brittleness of ceramics: a fresh approach10.1023/A:1018671823059 ↗
34. Microstructure characterization and SCG of newly engineered dental ceramics10.1016/j.dental.2016.03.018 ↗
35. Performance of dental ceramics: challenges for improvements10.1177/0022034510391795 ↗
36. Strength-limiting damage in lithium silicate glass-ceramics associated with CAD-CAM10.1016/j.dental.2018.11.004 ↗
37. Surface morphology and fracture in handpiece adjusting of a leucite-reinforced glass ceramic with coarse diamond burs10.1016/j.msea.2011.11.058 ↗
38. Brittleness index of machinable dental materials and its relation to the marginal chipping factor10.1016/j.jdent.2007.07.002 ↗
39. Factors influencing development of residual stresses during crystallization firing in a novel lithium silicate glass-ceramic10.1016/j.dental.2019.03.002 ↗
40. Chairside CAD/CAM materials. Part 2: flexural strength testing10.1016/j.dental.2016.10.008 ↗
41. Responses of pre-crystallized and crystallized zirconia-containing lithium silicate glass ceramics to diamond machining10.1016/j.ceramint.2019.09.170 ↗
42. Maximum undeformed equivalent chip thickness for ductile-brittle transition of zirconia ceramics under different lubrication conditions10.1016/j.ijmachtools.2017.06.003 ↗