journal article·2022-10

Does adhesive luting promote improved fatigue performance of lithium disilicate simplified crowns?

Gratcheva Falcão Chiapinotto, Lucas Saldanha da Rosa, Nicola Scotti, Cornelis Johannes Kleverlaan, Luiz Felipe Valandro, Gabriel Kalil Rocha Pereira

Publisher page

Abstract

The present study aimed to determine the influence of adhesive luting on the fatigue mechanical properties of simplified lithium disilicate crowns luted to dentin analogues preparations, and to compare two different approaches of simulation of a non-adhesive luting procedure. To this end, 30 prosthetic preparations of glass fiber-filled epoxy resin used as dentin analogues were milled and lithium disilicate crowns were pressed (1.5 mm thickness), which were allocated into three different groups: resin cement (RC), resin cement isolated by paraffin oil (RCI) and zinc phosphate cement (ZP). For luting procedures, the ceramic crowns of the RC and RCI groups had their internal surface treated with 5% hydrofluoric acid and universal primer. Afterwards, a thin layer of paraffin oil was applied onto the ceramic crown intaglio surface in the RCI group. The dentin analogues were treated with 10% hydrofluoric acid, followed by primer application and luting as recommended by the manufacturer. No previous surface treatments were performed for the ZP group, and the cement was applied as recommended. The fatigue test was run under cyclic fatigue (load 400-2000 N, step-size 100 N, 15,000 cycles/step, frequency 20 Hz) until failure detection (radial crack) by transillumination. The fatigue failure load (FFL), number of cycles until failure (CFF), and survival rate in each testing step were recorded. The RC group presented a higher FFL, CFF and survival rate compared to the other groups (p < 0.001), which were statistically equal to each other (p > 0.05). Weibull analysis detected no difference between groups for the Weibull module. Therefore, loss of adhesion between the evaluated substrates induces a significant reduction in load-bearing capacity under fatigue of the lithium disilicate crowns, strengthening the strong-importance of long-lasting adhesion for crown's survival. In addition, different methods for the simulation of non-adhesive conditions induce the same performance in the explored outcomes, confirming that both are valid approaches for laboratory studies.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Evaluation of the radiopacity of luting cements by digital radiography: radiopacity of luting cements10.1111/j.1532-849X.2012.00936.x ↗
2. Influence of ceramic thickness and ceramic materials on fracture resistance of posterior partial coverage restorations10.2341/12-459-L ↗
3. To compare and evaluate the sorption and solubility of four luting cements after immersion in artificial saliva of different pH values10.4103/jpbs.JPBS_153_17 ↗
4. The effect of resin bonding on long-term success of high-strength ceramics10.1177/0022034517729134 ↗
5. One-step ceramic primer as surface conditioner: effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations10.1016/j.jmbbm.2020.103686 ↗
6. Masticatory efficiency and bite force in individuals with normal occlusion10.1016/j.archoralbio.2014.05.005 ↗
7. The effect of internal roughness and bonding on the fracture resistance and structural reliability of lithium disilicate ceramic10.1016/j.dental.2017.09.018 ↗
8. The effect of cement type and mixing on the bi-axial fracture strength of cemented aluminous core porcelain discs10.1016/S0109-5641(02)00006-4 ↗
9. Clinical results of lithium-disilicate crowns after up to 9 years of service10.1007/s00784-012-0700-x ↗
10. Slow crack growth and reliability of dental ceramics10.1016/j.dental.2010.10.025 ↗
11. Residual interface tensile strength of ceramic bonded to dentin after cyclic loading and aging10.1016/S0022-3913(08)60045-1 ↗
12. Dental cements for definitive luting: a review and practical clinical considerations
13. A clinically focused discussion of luting materials: luting materials10.1111/j.1834-7819.2010.01297.x ↗
14. Simplified cementation of lithium disilicate crowns: retention with various adhesive resin cement combinations10.1016/j.prosdent.2017.07.012 ↗
15. Predictions of cement microfracture under crowns using 3D-FEA10.1111/j.1532-849X.2000.00201.x ↗
16. A systematic review and meta analysis of the longevity of anterior and posterior all-ceramic crowns10.1016/j.jdent.2016.08.009 ↗
17. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
18. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
19. Comparison of the mechanical properties of translucent zirconia and lithium disilicate10.1016/j.prosdent.2017.08.004 ↗
20. The effect of adhesive failure and defects on the stress distribution in all-ceramic crowns10.1016/j.jdent.2018.05.020 ↗
21. Cements and adhesives for all-ceramic restorations
22. An up to 43-year longitudinal study of fixed prosthetic restorations retained with 4-META/MMA-TBB resin cement or zinc phosphate cement
23. Silane adhesion mechanism in dental applications and surface treatments: a review10.1016/j.dental.2017.09.002 ↗
24. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns: multi-physics FEA modeling and monotonic testing10.1016/j.dental.2012.04.033 ↗
25. Quantitative study of bite force during sleep associated bruxism10.1046/j.1365-2842.2001.00692.x ↗
26. Microleakage of various cementing agents for full cast crowns10.1016/j.dental.2004.07.009 ↗
27. Influence of cementation on in vitro performance, marginal adaptation and fracture resistance of CAD/CAM-fabricated ZLS molar crowns10.1016/j.dental.2015.08.154 ↗
28. CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: fatigue performance and ceramic surface characteristics10.1016/j.jmbbm.2019.03.005 ↗
29. Mechanical behavior of bovine periodontal ligament under tension-compression cyclic displacements10.1111/j.1600-0722.2006.00269.x ↗
30. Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures10.1016/j.actbio.2008.12.016 ↗
31. Retrospective survival analysis of 261 lithium disilicate crowns in a private general practice
32. The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs10.1016/j.dental.2018.01.010 ↗
33. Influence of Bioactive, Resin and Glass Ionomer luting cements on the fracture loads of dentin bonded ceramic crowns
34. Statistical failure analysis of adhesive resin cement bonded dental ceramics10.1016/j.engfracmech.2006.11.006 ↗
35. Fatigue of dental ceramics10.1016/j.jdent.2013.10.007 ↗
36. Rheological and mechanical properties of resin-based materials applied in dental restorations10.3390/polym13172975 ↗