journal article·2022-12

A mass balance analysis of the tribocorrosion process of titanium alloys using a single micro-asperity: Voltage and solution effects on plastic deformation, oxide repassivation, and ion dissolution

Annsley Mace, Jeremy L. Gilbert

Publisher page

Abstract

Within modular taper junctions of total hip implants (THA), nominally "smooth" metallic surfaces contain multiple micro-asperities that slide, are plastically deformed, have their oxide film surfaces disrupted and corrode during the fretting corrosion processes. In this work, a mass/volume balance approach is developed and used to assess the contribution of individual components of wear and corrosion to the entirety of the single-asperity tribocorrosion process for the popular THA alloy, Ti-6Al-4V. This analysis measures the total volume change (trough) in the surface due to low cycle single asperity fretting corrosion and compares it to the measured pileup volume which is comprised of plastic deformation, metal particles and oxide particles, plus the fretting current and the concentration of solution-bound species. A simple 17 μm spherical geometry diamond asperity was used and the trough volume, pileup volume, fretting currents and ion concentrations were measured to assess their contribution to the fretting corrosion process. The effects fretting in or out of solution (phosphate buffered saline), and the role of electrode potential, e.g., freely corroding or forced potential (-1.0 V, 0 V, and +1.0 V vs Ag/AgCl) were investigated. Under constant 30 mN loading, 100 cycles duration, 3 Hz cyclic frequency and 80 μm sliding amplitude, the volume abraded, fretting currents, ion release, and pileup volume were all recorded. Damage was analyzed and quantified using digital optical microscopy (DOM), atomic force microscopy (AFM), scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS), and inductive coupled plasma mass spectrometry (ICP-MS). The results were analyzed with ANOVA statistics (α = 0.05). The extent of wear damage (asperity trough volume) is as follows: air = Ecorr, air > -1.0 V = 0 V = +1.0 V. As the amount of pileup volume decreased between conditions, visible oxide generation increased, with V > 0 V having more oxide debris generation and air fretting resulting in the least oxide (and most plastic deformation). Ions in solution were not significant, accounting for less than 1% of the damage. Volume analysis showed trough volumes and pileup volumes were very close to one another and were dominated by plastic deformation. Synergy between wear and corrosion were not observed in this work.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Advanced materials and composites · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Whole blood titanium metal ion measurement reproducibility of two laboratories10.1016/j.plabm.2020.e00167 ↗
2. Passive layers and corrosion resistance of biomedical Ti-6Al-4V and β-Ti alloys10.3390/coatings11050487 ↗
3. Vanadium
4. Britannica
5. Study of overall and local electrochemical responses of oxide films grown on CoCr alloy under biological environments10.1016/j.bioelechem.2017.01.003 ↗
6. Fretting corrosion behavior of beta titanium alloys in simulated synovial fluid10.1016/j.wear.2011.05.010 ↗
7. Dry sliding and tribocorrosion behavior of hot pressed CoCrMo biomedical alloy compared with the cast CoCrMo and Ti6Al4V alloys10.1016/j.matdes.2013.05.032 ↗
8. A metal ion release study of CoCrMo exposed to corrosion and tribocorrosion conditions in simulated body fluids10.1016/j.wear.2014.12.030 ↗
9. Synergism between mechanical wear and corrosion on tribocorrosion of a titanium alloy in a ringer solution10.1016/j.jmrt.2018.11.004 ↗
10. Modelling the evolution of electrochemical current in potentiostatic conditions using an asperity-scale model of tribocorrosion10.1016/j.biotri.2019.02.003 ↗
11. A new asperity-scale mechanical model of tribocorrosive wear: synergistic effects of mechanical wear and corrosion10.1115/1.4041246 ↗
12. A metallic biomaterial tribocorrosion model linking fretting mechanics, currents, and potentials: model development and experimental comparison10.1002/jbm.b.34643 ↗
13. Anhydride-functional silane immobilized onto titanium surfaces induces osteoblast cell differentiation and reduces bacterial adhesion and biofilm formation10.1016/j.msec.2015.10.051 ↗
14. Correlation of serum metal ion levels with pathological changes of ARMD in failed metal-on-metal-hip-resurfacing arthroplasties10.1007/s00402-017-2723-x ↗
15. Biotribocorrosion of metal-on-metal hip replacements: how surface degradation can influence metal ion formation10.1016/j.triboint.2013.02.025 ↗
16. Electrochemical modeling of passivation phenomena in tribocorrosion10.1016/S0043-1648(99)00314-2 ↗
17. Modeling the tribocorrosion interaction in aqueous sliding conditions10.1016/S0301-679X(02)00058-0 ↗
18. Determination of aluminium-26 in biological materials by accelerator mass spectrometry10.1039/a702002c ↗
19. Fretting and fretting corrosion processes of Ti6Al4V implant alloy in simulated oral cavity environment10.3390/ma13071561 ↗
20. Asymptomatic" pseudotumors after metal-on-metal hip resurfacing arthroplasty: prevalence and metal ion study10.1016/j.arth.2010.05.030 ↗
21. Leal · 2014
22. Ten-year outcome of serum metal ion levels after primary total hip arthroplasty: a concise follow up of previous report10.2106/JBJS.L.00471 ↗
23. Fretting initiated crevice corrosion of 316LVM stainless steel in physiological phosphate buffered saline: potential and cycles to initiation10.1016/j.actbio.2019.07.051 ↗
24. Micro-asperity tribocorrosion of CoCrMo, Ti6Al4V, and 316 stainless steel in air and physiological solution: fretting of a single diamond tip10.1016/j.wear.2022.204332 ↗
25. Measurement of erosion - corrosion synergism with a slurry wear test apparatus10.1016/0043-1648(88)90095-6 ↗
26. Wear accelerated corrosion of passive metals in tribocorrosion systems10.1149/1.1838341 ↗
27. Friction and wear performance of titanium alloys against tungsten carbide under dry sliding and water lubrication10.1080/10402004.2012.729296 ↗
28. On the synergistic effects of abrasion and corrosion during wear10.1016/0043-1648(83)90138-2 ↗
29. The electrochemical behavior and passivity of titanium10.1149/1.2427492 ↗
30. Fretting corrosion of CoCrMo and Ti-6Al-4V interfaces10.1016/j.biomaterials.2012.04.015 ↗
31. Tapscott · 2022
32. Potential and frequency effects on fretting corrosion of Ti6Al4V and CoCrMo surfaces
33. In-situ electrochemical study of interaction of tribology and corrosion in artificial hip prosthesis simulators10.1016/j.jmbbm.2012.08.009 ↗
34. Investigation of wear behavior of titanium oxide films, produced by anodic oxidation, on commercially pure titanium in vacuum conditions10.1016/j.surfcoat.2010.08.079 ↗