journal article·2021-08

Surface treatments and its effects on the fatigue behavior of a 5% mol yttria partially stabilized zirconia material

Ana Carolina Cadore-Rodrigues, Pablo Soares Machado, Jivago Schumacher de Oliveira, Sérgio Luiz Jahn, Lucio Strazzabosco Dorneles, Marília Pivetta Rippe, Gabriel Kalil Rocha Pereira, Luiz Felipe Valandro

Publisher page

Abstract

This study evaluated the effect of distinct surface treatments on the fatigue behavior (biaxial flexural fatigue testing) and surface characteristics (topography and roughness) of a 5% mol yttria partially stabilized zirconia ceramic (5Y-PSZ). Disc-shaped specimens of 5Y-PSZ (IPS e.max ZirCAD MT Multi) were manufactured (ISO 6872-2015) and allocated into six groups (n = 15) considering the following surface treatments: Ctrl - no-treatment; GLZ - low-fusing porcelain glaze application; SNF - 5 nm SiO2 nanofilm; AlOx - aluminum oxide particle air-abrasion; SiC - silica-coated aluminum oxide particles (silica-coating); and 7%Si - 7% silica-coated aluminum oxide particles (silica-coating). The biaxial flexural fatigue tests were performed by the step-stress method (20Hz for 10,000 cycles) with a step increment of 50N starting at 100N and proceeding until failure detection. The samples were tested with the treated surface facing down (tensile stress side). Topography, fractography, roughness, and phase content assessments of treated specimens were performed. GLZ group presented the highest fatigue behavior, while AlOx presented the lowest performance, and was only similar to SiC and 7%Si. Ctrl and SNF presented intermediary fatigue behavior, and were also similar to SiC and 7%Si. GLZ promoted a rougher surface, Ctrl and SNF had the lowest roughness, while the air-abrasion groups presented intermediary roughness. No m-phase content was detected (only t and c phases were detected). In conclusion, the application of a thin-layer of low-fusing porcelain glaze, the deposition of silica nanofilms and the air-abrasion with silica-coated alumina particles had no detrimental effect on the fatigue behavior of the 5Y-PSZ, while the air-abrasion with alumina particles damaged the fatigue outcomes.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Bone Tissue Engineering Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Selective infiltration-etching technique for a strong and durable bond of resin cements to zirconia-based materials10.1016/S0022-3913(07)60123-1 ↗
2. Anusavice · 2003
3. Does air particle abrasion affect the flexural strength and phase transformation of Y-TZP? A systematic review and meta-analysis10.1016/j.dental.2016.03.021 ↗
4. Flexural strength and failure modes of layered ceramic structures10.1016/j.dental.2011.09.008 ↗
5. Cadore-Rodrigues · 2020 · vol. 22 · 149
6. Air-abrasion using new silica-alumina powders containing different silica concentrations: effect on the microstructural characteristics and fatigue behavior of a Y-TZP ceramic10.1016/j.jmbbm.2019.05.032 ↗
7. Can low-fusing glass application affect the marginal misfit and bond strength of Y-TZP crowns ?
8. The development and testing of glaze materials for application to the fit surface of dental ceramic restorations10.1016/j.dental.2008.09.004 ↗
9. Effects of tribochemical silica coating and alumina-particle air abrasion on 3Y-TZP and 5Y-TZP : evaluation of surface hardness
10. Phase transformation and subsurface damage in 3Y-TZP after sandblasting10.1016/j.dental.2013.03.005 ↗
11. Effect of sandblasting and residual stress on strength of zirconia for restorative dentistry applications10.1016/j.jmbbm.2013.09.004 ↗
12. Microstructural analysis and reliability of monolithic zirconia after simulated adjustment protocols10.1016/j.dental.2017.04.024 ↗
13. Comparison of alternative adhesive cementation concepts for zirconia ceramic: glaze layer vs zirconia primer
14. Denry · 2007 · vol. 4 · 299
15. Adhesion to Y-TZP ceramic: study of silica nanofilm coating on the surface of Y-TZP10.1002/jbm.b.33184 ↗
16. Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic10.1016/j.jdent.2004.07.001 ↗
17. Effect of blasting pressure, abrasive particle size and grade on phase transformation and morphological change of dental zirconia surface10.1016/j.surfcoat.2012.04.043 ↗
18. Damage tolerance of six dental zirconias with different translucencies
19. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
20. Effect of an internal coating technique on tensile bond strengths of resin cements to zirconia ceramics10.4012/dmj.28.446 ↗
21. Clinical outcomes of monolithic zirconia crowns with cad/cam technology. A 1-year follow-up prospective clinical study of 65 patients10.3390/ijerph15112523 ↗
22. Strength and aging resistance of monolithic zirconia: an update to current knowledge10.1016/j.jdsr.2019.09.002 ↗
23. The effect of surface grinding and sanblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
24. Effects of airborne-particle abrasion protocol choice on the surface characteristics of monolithic zirconia materials and the shear bond strength of resin cement10.1016/j.ceramint.2015.09.104 ↗
25. Adhesion to zirconia used for dental restorations: a systematic review and meta-analysis
26. Effect of particle deposition parameters on silica coating of zirconia using a chairside air-abrasion device
27. Effect of surface conditioning methods on the bond strength of luting cement to ceramics10.1016/S0109-5641(03)00019-8 ↗
28. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
29. Surface modification for enhanced silanation of zirconia ceramics10.1016/j.dental.2009.03.008 ↗
30. Piconi · 1999
31. Mechanical behavior of yttria-stabilized tetragonal zirconia polycrystalline ceramic after different zirconia surface treatments10.1016/j.msec.2017.03.299 ↗
32. Deposition of SiOx thin films on Y-TZP by reactive magnetron sputtering: influence of plasma parameters on the adhesion properties between Y-TZP and resin cement for application in dental prosthesis10.1590/S1516-14392011005000032 ↗
33. All-ceramic or metal-ceramic tooth-supported fixed dental prostheses (FDPs)? A systematic review of the survival and complication rates. Part I: single crowns (SCs)10.1016/j.dental.2015.02.011 ↗
34. Air-particle abrasion on zirconia ceramic using different protocols: effects on biaxial flexural strength after cyclic loading, phase transformation and surface topography10.1016/j.jmbbm.2013.04.018 ↗
35. Three generations of zirconia: from veneered to monolithic. Part I
36. Effect of different treatments on the flexural strength of fully versus partially stabilized monolithic zirconia10.1016/j.prosdent.2016.10.031 ↗
37. Tabatabaian · 2018
38. Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?10.1016/j.dental.2010.10.022 ↗
39. Fatigue performance of adhesively cemented glass-, hybrid- and resin-ceramic materials for CAD/CAM monolithic restorations10.1016/j.dental.2019.01.013 ↗
40. Flexural strength of a layered zirconia and porcelain dental all-ceramic system10.1016/j.prosdent.2005.05.007 ↗
41. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗
42. Damage accumulation and fatigue life of particle-abraded ceramics
43. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗
44. Low-fusing porcelain glaze application does not damage the fatigue strength of Y-TZP10.1016/j.jmbbm.2019.07.022 ↗
45. Grinding, polishing and glazing of the occlusal surface do not affect the load-bearing capacity under fatigue and survival rates of bonded monolithic fully-stabilized zirconia simplified restorations10.1016/j.jmbbm.2019.103528 ↗
46. Load-bearing capacity under fatigue and survival rates of adhesively cemented yttrium-stabilized zirconia polycrystal monolithic simplified restorations10.1016/j.jmbbm.2018.11.009 ↗