Objectives This study evaluated the repairability of three-dimensional printed (3DP) denture bases based on different conventional relining materials and aging. Material and methods The groups for surface characterization (surface-roughness and contact-angle measurements) were divided based on the denture base and surface treatment. Shear bond strength test and failure-mode analysis were conducted by a combination of three variables: denture base, relining materials, and hydrothermal aging (HA). The initial characterization involved quantifying the surface roughness (n = 10) and contact angle (n = 10) of denture base specimens with and without sandblasting (SB) treatment. Four relining materials (Kooliner [K], Vertex Self-Curing [V], Tokuyama Rebase II (Normal) [T], and Ufi Gel Hard [U]) were applied to 3DP, heat-cured (HC), and self-cured (SC) denture-base resin specimens. Shear bond strength (n = 15) and failure-mode analyses (n = 15) were performed before and after HA, along with evaluations of the fractured surfaces (n = 4). Statistical analyses were performed using a two-way analysis of variance (ANOVA) for surface characterization, and a three-way ANOVA was conducted for shear bond strength. Results The surface roughness peaked in HC groups and increased after SB. The 3DP group displayed significantly lower contact angles, which increased after treatment, similar to the surface roughness. The shear bond strength was significantly lower for 3DP and HC denture bases than for SC denture bases, and peaked for U at 10.65 ± 1.88 MPa (mean ± SD). HA decreased the shear bond strength relative to untreated samples. Furthermore, 3DP, HC, and SC mainly showed mixed or cohesive failures with V, T, and U. K, on the other hand, trended toward adhesive failures when bonded with HC and SC. Conclusion This study has validated the repairability of 3DP dentures through relining them with common materials used in clinical practice. The repairability of the 3DP denture base was on par with that of conventional materials, but it decreased after aging. Notably, U, which had a postadhesive application, proved to be the most effective material for repairing 3DP dentures.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Health and Care Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. Trends in computer-aided manufacturing in prosthodontics: a review of the available streams10.1155/2014/783948 ↗
2. Digital versus conventional impressions in fixed prosthodontics: a review10.1111/jopr.12527 ↗
3. Shear bond strength of two chemically different denture base polymers to reline materials10.1111/j.1532-849X.2009.00481.x ↗
4. A comparison of the surface and mechanical properties of 3D printable denture-base resin material and conventional polymethylmethacrylate (PMMA)10.1111/jopr.13491 ↗
5. A comparison of the surface properties of CAD/CAM and conventional polymethylmethacrylate (PMMA)10.1111/jopr.13033 ↗
6. Surface properties of polymer resins fabricated with subtractive and additive manufacturing techniques10.3390/polym13234077 ↗
7. Printing accuracy and flexural properties of different 3D-printed denture base resins10.3390/ma15072410 ↗
8. 3D printed complete removable dental prostheses: a narrative review10.1186/s12903-020-01328-8 ↗
9. Comparison of tensile bond strength of denture reline materials on denture bases fabricated with CAD-CAM technology10.1016/j.prosdent.2021.06.047 ↗
10. Bond strength and failure analysis of lining materials to denture resin10.1016/S0109-5641(99)00038-X ↗
11. The effect of water immersion on the shear bond strength between chairside reline and denture base acrylic resins10.1111/j.1532-849X.2007.00188.x ↗
12. Three-dimensional printing in contemporary fixed prosthodontics: a technique article10.1016/j.prosdent.2017.07.008 ↗
13. Wear resistance of 3D-printed denture tooth resin opposing zirconia and metal antagonists10.1016/j.prosdent.2019.09.004 ↗
14. Water sorption, solubility, and bond strength of two autopolymerizing acrylic resins and one heat-polymerizing acrylic resin10.1016/S0022-3913(98)70008-3 ↗
15. Post-processing of DLP-printed denture base polymer: impact of a protective coating on the surface characteristics, flexural properties, cytotoxicity, and microbial adhesion10.1016/j.dental.2022.11.008 ↗
16. 3D printing in dentistry10.1038/sj.bdj.2015.914 ↗
17. Comparative study of water sorption, solubility, and tensile bond strength of two soft lining materials10.1016/S0022-3913(00)70140-5 ↗
18. The effects of different surface treatments applied to milled PMMA denture base material on repair bond strength
19. The effect of food-simulating agents on the bond strength of hard chairside reline materials to denture base resin10.1111/jopr.12905 ↗
20. Physical, mechanical, and anti‐biofilm formation properties of CAD‐CAM milled or 3D printed denture base resins: in vitro analysis10.1111/jopr.13554 ↗
21. Repair bond strength of conventionally and digitally fabricated denture base resins to auto-polymerized acrylic resin: surface treatment effects in vitro10.3390/ma15249062 ↗
22. Physical properties of a new denture lining material containing a fluoroalkyl methacrylate polymer10.1016/j.prosdent.2006.05.012 ↗
23. Wettability of denture relining materials under water storage over time10.4047/jap.2009.1.1.1 ↗
24. Digital technology in fixed implant prosthodontics10.1111/prd.12164 ↗
25. An experimental study on hydrothermal degradation of cubic-containing translucent zirconia10.4047/jap.2020.12.5.265 ↗
26. Evaluation of the marginal fit of metal copings fabricated by using 3 different CAD-CAM techniques: milling, stereolithography, and 3D wax printer10.1016/j.prosdent.2019.09.002 ↗
27. Evaluation of adhesion of reline resins to the thermoplastic denture base resin for non-metal clasp denture10.4012/dmj.2013-121 ↗
28. Selective laser melting technique of Co-Cr dental alloys: a review of structure and properties and comparative analysis with other available techniques10.1111/jopr.12268 ↗
29. Denture liners: a systematic review relative to adhesion and mechanical properties10.1155/2019/6913080 ↗
30. Bonding strength between a hard chairside reline resin and a denture base material as influenced by surface treatment10.1046/j.1365-2842.2001.00786.x ↗
31. Water sorption, solubility, and tensile bond strength of resilient denture lining materials polymerized by different methods after thermal cycling10.1016/j.prosdent.2004.11.014 ↗
32. Repairability of a 3D printed denture base polymer: effects of surface treatment and artificial aging on the shear bond strength10.1016/j.jmbbm.2020.104227 ↗
33. Postpolymerization of a 3D-printed denture base polymer: impact of post-curing methods on surface characteristics, flexural strength, and cytotoxicity10.1016/j.jdent.2021.103856 ↗
34. A digital technique to replicate edentulous arches with functional borders and accurate maxillomandibular relationship for digital complete denture10.1111/jopr.13154 ↗
35. Effect of storage duration on the hardness and tensile bond strength of silicone- and acrylic resin-based resilient denture liners to a processed denture base acrylic resin10.1016/S0022-3913(08)60032-3 ↗
36. In vitro evaluation of the influence of repairing condition of denture base resin on the bonding of autopolymerizing resins10.1016/j.prosdent.2003.10.023 ↗
37. Effects of artificial tooth brushing and hydrothermal aging on the mechanical properties and color stability of dental 3D printed and CAD/CAM materials10.3390/ma14206207 ↗
38. 3D printing-encompassing the facets of dentistry10.3389/fbioe.2018.00172 ↗
39. Effects of repeated use of tungsten carbide burs on the surface roughness and contact angles of a CAD-CAM PMMA denture base resin10.1016/j.prosdent.2021.11.032 ↗
40. Effect of surface treatment on shear bond strength of relining material and 3D-printed denture base10.4047/jap.2022.14.4.262 ↗
41. Comparison of mechanical properties of 3D‐printed, CAD/CAM, and conventional denture base materials10.1111/jopr.13175 ↗
42. Digital dentistry: the new state of the art - is it disruptive or destructive?10.1016/j.dental.2019.08.103 ↗
43. Extended post-curing light exposure and sandblasting effects on surface hydrophobicity of 3D-printed denture base resin10.3390/prosthesis4010009 ↗
44. The effect of chemical surface treatments of different denture base resins on the shear bond strength of denture repair10.1016/j.prosdent.2005.05.024 ↗
45. Effect of thermal cycling on denture base and autopolymerizing reline resins10.1590/1679-775720130061 ↗
46. CAD-CAM complete denture resins: an evaluation of biocompatibility, mechanical properties, and surface characteristics10.1016/j.jdent.2021.103785 ↗
47. 3D printing with polymers: challenges among expanding options and opportunities10.1016/j.dental.2015.09.018 ↗
48. Comparison of shear bond strength of CAD/CAM and conventional heat-polymerized acrylic resin denture bases to auto-polymerized and heat-polymerized acrylic resins after aging10.4317/jced.59097 ↗
49. Complete denture wearing and fractures among edentulous patients treated in university clinics10.1111/j.1741-2358.2011.00551.x ↗
50. A review of 3D printing in dentistry: technologies, affecting factors, and applications10.1155/2021/9950131 ↗
51. Rapid prototyping technologies and their applications in prosthodontics, a review of literature
52. Tensile bond strength between soft liners and two chemically different denture base materials: effect of thermocycling10.1111/jopr.12296 ↗
53. The future of dental devices is digital10.1016/j.dental.2011.10.014 ↗
54. Effect of water storage on the shear strength and fatigue limit of the reline resin bond to denture base resins
55. Effective utilization of digital technology in complete denture fabrication10.2334/josnusd.21-0381 ↗
56. Bond strength of conventional, subtractive, and additive manufactured denture bases to soft and hard relining materials10.1016/j.dental.2021.02.018 ↗