Fretting corrosion behavior of Ti6Al4V alloy against zirconia-toughened alumina ceramic in simulated body fluid
Source abstract
Abstract
The fretting corrosion at the head-neck interface of artificial hip joints is an important reason for the failure of prostheses. The Ti6Al4V alloy-zirconia-toughened alumina (ZTA) ceramic combination has been widely used to make the head and neck of artificial hip joints. In this study, its fretting corrosion behavior in simulated body fluid was studied by electrochemical monitoring, surface morphology characterization, and chemical composition analysis. A running condition fretting map (RCFM) of load and displacement was established, including three regimes, namely partial slip regime (PSR), mixed fretting regime (MFR), and gross slip regime (GSR). The friction dissipation energy increased gradually from the PSR to MFR and GSR. In the PSR, the damage mechanisms were slight abrasive wear and tribocorrosion at the edge of contact area, as well as extremely slight adhesive wear at the center. In the MFR, the damage mechanisms were mainly adhesive wear, abrasive wear, and corrosive wear. In the GSR, the damage mechanism was serious abrasive wear, fatigue wear, and corrosive wear combined with slight adhesive wear. Finally, an ion-concentration map was created, displaying the material-loss transition of different displacements and loads. The material loss increased with the increased displacement, and increased first and then decreased with the increased load.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Mechanical stress and fatigue analysis · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Influence of fretting regimes on the tribocorrosion behaviour of Ti6Al4V in 0.9wt.% sodium chloride solution10.1016/j.wear.2003.11.003 ↗
2. Electrochemical effects on the fretting corrosion behaviour of Ti6Al4V in 0.9% sodium chloride solution10.1016/j.wear.2004.12.012 ↗
3. Realistic loads for testing hip implants
4. Effect of applied potential on the tribocorrosion behaviors of Monel K500 alloy in artificial seawater10.1016/j.triboint.2014.07.014 ↗
5. Corrosion at the head-neck taper as a cause for adverse local tissue reactions after total hip arthroplasty10.2106/JBJS.K.01352 ↗
6. Adverse local tissue reaction arising from corrosion at the femoral neck-body junction in a dual-taper stem with a cobalt-chromium modular neck10.2106/JBJS.L.01042 ↗
7. Fretting-corrosion behavior of β titanium alloys in simulated synovial fluid10.1016/j.wear.2011.05.010 ↗
8. Characterization of the fretting corrosion behavior, surface and debris from head-taper interface of two different modular hip prostheses10.1016/j.jmbbm.2016.04.036 ↗
9. Influence of molybdate ion and pH on the fretting corrosion of a CoCrMo – titanium alloy couple10.1016/j.biotri.2017.05.002 ↗
10. Assessing taper geometry, head size, head material, and their interactions in taper fretting corrosion of retrieved total hip arthroplasty implants10.1016/j.arth.2021.02.041 ↗
11. A finite element study on the mechanical response of the head-neck interface of hip implants under realistic forces and moments of daily activities: Part 1, level walking10.1016/j.jmbbm.2017.08.012 ↗
12. Wear modeling and the third body concept10.1016/j.wear.2006.10.011 ↗
13. The mechanism-based approach of understanding run-in and steady state: a gross-slip fretting experiment to fathom tribocorrosion of total hip taper junctions10.1016/j.biotri.2021.100165 ↗
14. Analysis of sliding behaviour for fretting loadings: determination of transition criteria10.1016/0043-1648(94)06582-9 ↗
15. Ti based biomaterials, the ultimate choice for orthopaedic implants – a review10.1016/j.pmatsci.2008.06.004 ↗
16. Metal sensitivity in patients with orthopedic implants10.1097/00124743-200108000-00004 ↗
17. The chemical form of metallic debris in tissues surrounding metal-on-metal hips with unexplained failure10.1016/j.actbio.2010.06.006 ↗
18. The influence of proteins on the fretting–corrosion behaviour of a Ti6Al4V alloy10.1016/j.wear.2006.03.032 ↗
19. Wear by plastic ratchetting10.1016/S0043-1648(97)00083-5 ↗
20. Fretting corrosion of Si3 N4 vs CoCrMo femoral heads on Ti-6Al-V trunnions10.1002/jor.24681 ↗
21. Analysis of energy dissipation in fretting corrosion experiments with materials used as hip prosthesis10.1016/j.wear.2012.07.014 ↗
22. Surface modification of CP-Ti to improve the fretting-corrosion resistance: thermal oxidation vs. anodizing10.1016/j.msec.2010.03.024 ↗
23. Fretting-corrosion mapping of CP-Ti in Ringer's solution10.1016/j.wear.2010.01.026 ↗
24. Reducing fretting-initiated crevice corrosion in hip simulator tests using a zirconia-toughened alumina femoral head10.1002/jbm.b.34062 ↗
25. Correlation of corrosion and biomechanics in the retrieval of a single modular neck total hip arthroplasty design: modular neck total hip arthroplasty system10.1016/j.arth.2014.06.009 ↗
26. Effects of displacement amplitude on fretting wear behaviors and mechanism of Inconel 600 alloy10.1016/j.wear.2013.04.027 ↗
27. Torsional fretting corrosion behaviours of Ti6Al4V alloys in Hank's simulated body fluid10.1080/1478422X.2019.1589675 ↗
28. A mass balance analysis of the tribocorrosion process of titanium alloys using a single micro-asperity: voltage and solution effects on plastic deformation, oxide repassivation, and ion dissolution10.1016/j.jmbbm.2022.105531 ↗
29. Hip implant modular junction: the role of CoCrMo alloy microstructure on fretting-corrosion10.1016/j.jmbbm.2022.105402 ↗
30. Elastic spheres in contact under varying oblique forces10.1115/1.4010702 ↗
31. Triboelectrochemical behaviour of a Si(3)N(4)-TiN ceramic composite and a titanium alloy commonly used in biomedical applications10.1016/j.wear.2008.07.005 ↗
32. The evolution of subsurface micro-structure and tribo-chemical processes in cocrmo-ti6al4v fretting-corrosion contacts: what lies at and below the surface?
33. Modular femoral stem-sleeve junction failure after primary total hip arthroplasty10.1016/j.arth.2008.09.006 ↗
34. An experimental study on the fretting corrosion behaviours of three material pairs at modular interfaces for hip joint implants10.3390/lubricants9020012 ↗
35. Mapping the fretting corrosion behaviors of 6082 aluminum alloy in 3.5% NaCl solution
36. Metal-induced apoptosis: mechanisms10.1016/j.mrfmmm.2003.07.015 ↗
37. Repeated metal ion measurements in patients with high risk metal-on-metal hip replacement10.1007/s00264-014-2300-7 ↗
38. Fretting-corrosion behavior in hip implant modular junctions: the influence of friction energy and pH variation10.1016/j.jmbbm.2016.05.024 ↗
39. Mapping the micro-abrasion mechanisms of CoCrMo: some thoughts on varying ceramic counterface diameter on transition boundaries in vitro10.3390/lubricants8070071 ↗
40. Potential presence of metals in patients treated with metal-metal coupling prostheses for hip arthroplasty at 7 and 10 years of follow-up10.1007/s00590-018-2129-7 ↗
41. Fretting corrosion behaviour of Ti–6Al–4V alloy in artificial saliva containing varying concentrations of fluoride ions10.1016/j.wear.2010.09.008 ↗
42. Interfacial compliance, energy dissipation, frequency effects, and long-term fretting corrosion performance of Ti-6Al-4V/CoCrMo interfaces10.1002/jbm.a.37299 ↗
43. Corrosion behaviour of biomedical Ti under simulated inflammation: exploring the relevance of grain refinement and crystallographic texture10.1016/j.corsci.2022.110238 ↗
44. Tribocorrosion investigation of 316L stainless steel: the synergistic effect between chloride ion and sulfate ion10.1088/2053-1591/ac1825 ↗
45. Influence of pH and corrosion inhibitors on the tribocorrosion of titanium in artificial saliva10.1016/j.wear.2006.03.031 ↗
46. Mechanical and electrochemical deterioration mechanisms in the tribocorrosion of Al alloys in NaCl and in NaNO3 solutions10.1016/j.corsci.2011.08.041 ↗
47. Moderated crevice corrosion susceptibility of Ti6Al4V implant material due to albumin-corrosion interaction10.1016/j.jmst.2021.09.006 ↗
48. Characterization of electrolytic ZrO2 coating on Co–Cr–Mo implant alloys of hip prosthesis10.1016/S0142-9612(00)00133-2 ↗
49. Reducing taper fretting corrosion in artificial hip joints using a PEEK femoral head10.1007/s11665-021-05766-5 ↗
50. Local cellular responses to metallic and ceramic nanoparticles from orthopedic joint arthroplasty implants10.2147/IJN.S248848 ↗
51. A review of the bio-tribology of medical devices10.1007/s40544-021-0512-6 ↗
52. Progress in fretting maps10.1016/j.triboint.2006.02.001 ↗
53. In vitro fretting crevice corrosion damage of CoCrMo alloys in phosphate buffered saline: debris generation, chemistry and distribution10.1016/j.actbio.2020.07.052 ↗