Abstract
Objectives The purpose of this study was to study the effects on Young's modulus and conversion degree of variations in polymerization conditions during the 3-point bending test of composite samples in accordance with the ISO 4049 standard. Methods Three nanocomposites were used in the 3-point bending test based on the conditions described in the ISO 4049 standard. Samples of 2 mm × 2 mm x 25 mm were fabricated and tested with a different number of irradiation points and irradiation time. Conversion degree of the samples were also measured by micro-Raman spectroscopy and correlated with the Young's modulus values obtained for each one. Results The variations in curing protocol during specimen's realization influenced the Young's modulus and degree of conversion of all composites. These two properties correlated well. The ISO 4049 standard defines the conditions for performing the properties tests of composites to allow reproducibility and comparison of different studies. Concerning the 3-point bending test, even a minimal change in the state causes differences in the results obtained. The standard should thus clarify the tools that can be used when producing samples in order to minimize discrepancies. Significance The influence of the parameters surrounding the design of the samples should be controlled and defined so as not to include bias in the studies carried out. This will allow literature studies to be compared with more accuracy.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Polymer Nanocomposites and Properties · Photopolymerization techniques and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. Degree of conversion of three composite materials employed in the adhesive cementation of indirect restorations: a micro-Raman analysis10.1016/j.jdent.2009.04.001 ↗
2. The volumetric fraction of inorganic particles and the flexural strength of composites for posterior teeth10.1016/S0300-5712(03)00049-6 ↗
3. Effect of alumina particles loading on the mechanical properties of light-cured dental resin composites10.1016/j.matdes.2013.07.069 ↗
4. The influence of distance on radiant exposure and degree of conversion using different light-emitting-diode curing units10.2341/18-004-L ↗
5. Nano-porous thermally sintered nano silica as novel fillers for dental composites10.1016/j.dental.2011.10.015 ↗
6. The effect of monolithic zirconia thickness on the degree of conversion of dental resin cements: ATR-FTIR spectroscopic analysis10.1016/j.vibspec.2016.07.015 ↗
7. Are linear elastic material properties relevant predictors of the cyclic fatigue resistance of dental resin composites?10.1016/j.dental.2014.01.009 ↗
8. Resin composites: modulus of elasticity and marginal quality10.1016/j.jdent.2014.07.004 ↗
9. Changes in irradiance and energy density in relation to different curing distances
10. Physical, mechanical and rheological characterization of resin-based pit and fissure sealants compared to flowable resin composites10.1016/j.dental.2011.11.001 ↗
11. Mechanical properties, fracture resistance, and fatigue limits of short fiber reinforced dental composite resin10.1016/j.prosdent.2015.07.012 ↗
12. Effect of photoinitiator concentration on marginal and internal adaptation of experimental composite blends photocured by modulated methods
13. Evaluation of the clinical impact of ISO 4049 in comparison with miniflexural test on mechanical performances of resin based composite
14. Curing effectiveness of resin composites at different exposure times using LED and halogen units
15. Effect of high-intensity curing lights on the polymerization of bulk-fill composites10.1016/j.dental.2018.06.005 ↗
16. International dental standards—order out of chaos?10.1016/j.dental.2011.04.004 ↗
17. Influence of curing protocol on selected properties of light-curing polymers: degree of conversion, volume contraction, elastic modulus, and glass transition temperature10.1016/j.dental.2009.08.001 ↗
18. Volume contraction in photocured dental resins: the shrinkage-conversion relationship revisited10.1016/j.dental.2005.03.014 ↗
19. Correlation of the degree of conversion with the amount of elutable substances in nano-hybrid dental composites10.1016/j.dental.2012.08.006 ↗
20. Relationship between shade and depth of cure for light-activated dental composite resins10.1016/S0109-5641(86)80057-4 ↗
21. Academy of Dental Materials guidance-Resin composites: Part II-Technique sensitivity (handling, polymerization, dimensional changes)10.1016/j.dental.2017.08.188 ↗
22. 405 nm diode laser, halogen lamp and LED device comparison in dental composites cure: an “in vitro” experimental trial10.5978/islsm.15-OR-16 ↗
23. Influence of different concentration and ratio of a photoinitiator system on the properties of experimental resin composites10.1590/0103-6440201701372 ↗
24. Light energy transmission through composite influenced by material shades10.2209/tdcpublication.50.183 ↗
25. Effect of the irradiance distribution from light curing units on the local micro-hardness of the surface of dental resins10.1016/j.dental.2014.11.003 ↗
26. The effect of filler and silane content on conversion of resin-based composite10.1016/S0109-5641(02)00062-3 ↗
27. Transmission of violet and blue light through conventional (layered) and bulk cured resin-based composites10.1016/j.jdent.2016.06.007 ↗
28. Synthesis and characterization of a novel resin monomer with low viscosity10.1016/j.jdent.2017.01.006 ↗
29. Macro-, micro- and nano-mechanical investigations on silorane and methacrylate-based composites10.1016/j.dental.2009.02.005 ↗
30. Academy of Dental Materials guidance-Resin composites: Part I-Mechanical properties10.1016/j.dental.2017.04.013 ↗
31. Degree of conversion of composites measured by DTA and FTIR10.1016/S0109-5641(00)00066-X ↗
32. 2019
33. The effect of resin shades on microhardness, polymerization shrinkage, and color change of dental composite resins
34. Vibrational spectroscopy of selective dental restorative materials10.1080/05704928.2016.1244069 ↗
35. Effect of short LED lamp exposure on wear resistance, residual monomer and degree of conversion for Filtek Z250 and Tetric EvoCeram composites10.1016/j.dental.2013.04.022 ↗
36. Role of the beam profile and sample geometry in the bonded-disk method on the shrinkage kinetics of two dental resins10.1016/j.dental.2016.05.010 ↗
37. Quantification of conversion degree and monomer elution from dental composite using HPLC and micro-Raman spectroscopy10.1007/s10337-014-2647-3 ↗
38. Multiple correlations of material parameters of light-cured dental composites10.1016/j.dental.2009.03.011 ↗
39. Degree of conversion of resin-based materials cured with dual-peak or single-peak LED light-curing units10.1111/ipd.12104 ↗
40. Effect of camphorquinone concentration in physical-mechanical properties of experimental flowable resin composites10.1155/2018/7921247 ↗
41. Effect of LED-LCU light irradiance distribution on mechanical properties of resin based materials10.1016/j.msec.2016.02.060 ↗
42. Mechanical properties and wear behavior of light-cured packable composite resins10.1016/S0109-5641(99)00082-2 ↗
43. Degree of conversion and microhardness of dental composite resin materials10.1016/j.molstruc.2012.10.062 ↗
44. Localised irradiance distribution found in dental light curing units10.1016/j.jdent.2013.11.014 ↗
45. Post-polymerization of dental resin composite evaluated with nanoindentation and micro-Raman spectroscopy
46. Infrared spectroscopy: a tool for determination of the degree of conversion in dental composites10.1590/S1678-77572008000200012 ↗
47. The reliability in flexural strength testing of a novel dental composite10.1016/S0300-5712(03)00110-6 ↗
48. The micro-Raman spectroscopy, a useful tool to determine the degree of conversion of light-activated composite resins10.1002/(SICI)1097-4636(1999)48:5<675::AID-JBM11>3.0.CO;2-P ↗
49. A critical view on biaxial and short-beam uniaxial flexural strength tests applied to resin composites using Weibull, fractographic and finite element analyses10.1016/j.dental.2009.09.002 ↗
50. The effect of specimen temperature on the polymerization of a resin-composite10.1016/j.dental.2011.06.004 ↗
51. Irradiance differences in the violet (405 nm) and blue (460 nm) spectral ranges among dental light-curing units: spectral beam uniformity from dental LCUs10.1111/j.1708-8240.2010.00368.x ↗
52. Filler characteristics of modern dental resin composites and their influence on physico-mechanical properties10.1016/j.dental.2016.09.034 ↗
53. Flexural strength and modulus of elasticity of different types of resin-based composites
54. Effect of blue and violet light on polymerization shrinkage vectors of a CQ/TPO-containing composite10.1016/j.dental.2017.04.010 ↗
55. Degree of conversion and microhardness of TPO-containing resin-based composites cured by polywave and monowave LED units10.1016/j.jdent.2012.03.007 ↗
56. Flexural properties and elastic modulus of different esthetic restorative materials: evaluation after exposure to acidic drink10.1155/2019/5109481 ↗
57. Light output from six battery operated dental curing lights10.1016/j.msec.2016.07.033 ↗
58. Aging studies of light cured dimethacrylate-based dental resins and a resin composite in water or ethanol/water10.1016/j.dental.2006.06.049 ↗
59. Physical properties of current dental nanohybrid and nanofill light-cured resin composites10.1016/j.dental.2011.02.015 ↗
60. Degree of conversion of composite resin: a Raman study10.1089/104454703322650167 ↗
61. Analysis of the degree of conversion of LED and halogen lights using micro-Raman spectroscopy
62. Determination of double bond conversion in dental resins by near infrared spectroscopy10.1016/S0109-5641(00)00062-2 ↗
63. Factors influencing marginal cavity adaptation of nanofiller containing resin composite restorations10.1016/j.dental.2010.08.189 ↗
64. Degree of conversion
65. Antibacterial, physical and mechanical properties of flowable resin composites containing zinc oxide nanoparticles10.1016/j.dental.2013.03.011 ↗
66. Mechanical properties of contemporary composite resins and their interrelations10.1016/j.dental.2013.04.025 ↗
67. Interfacial layer characterization in dental composite10.1046/j.1365-2842.2003.01008.x ↗
68. Study of visible light activated polymerization in BisGMA-TEGDMA monomers with Type 1 and Type 2 photoinitiators using Raman spectroscopy10.1016/j.dental.2016.09.002 ↗
69. How much do resin-based dental materials release? A meta-analytical approach10.1016/j.dental.2011.05.001 ↗
70. Influence of modulated photo-activation on shrinkage stress and degree of conversion of bulk-fill composites10.1590/0103-6440201902571 ↗
71. Residual shrinkage stress distributions in molars after composite restoration10.1016/j.dental.2003.05.007 ↗
72. Mechanical properties of dental restorative materials: relative contribution of laboratory tests10.1590/S1678-77572003000300002 ↗
73. Depth-dependence of degree of conversion and microhardness for dual-cure and light-cure composites
74. Comparative evaluation of the depth of cure and degree of conversion of two bulk fill flowable composites
75. A comparison of the mechanical properties of a modified silorane based dental composite with those of commercially available composite material10.1016/j.dental.2012.12.006 ↗