Load-bearing capacity of pressable lithium disilicates applied as ultra-thin occlusal veneers on molars
Source abstract
Abstract
Purpose The aim was to investigate the load bearing capacity of different pressable lithium disilicates cemented as occlusal veneers on molars. Materials and methods One control group and six test groups were formed consisting of 20 specimens each (n = 20). The six test groups differed in the utilizing pressable lithium disilicate to fabricate occlusal veneers. As a control group, “group Lis”, the lithium disilicate with the highest reported flexural strength was used (initial LiSi Press, GC Europe; Leuven, Belgium / flexural strength: 508 MPa). The test groups consisted of other pressable lithium disilicates with lower flexural strength values: “Ema” (IPS e.max press), “Vit” (VITA Ambria), “Liv” (Livento Press), “Amb” (Amber Press), “Mas” (Amber Press Master) and “Ros” (Rosetta SP)“. After the preparation of 140 extracted human molars, which included the removal of the central enamel, the specimens were scanned using a desktop scanner. With the aid of a design software, the occlusal veneers were designed in a standardized thickness of 0.5 mm. To fabricate the restorations, all tested materials were processed using heat-pressing technique. All restorations were adhesively cemented. Afterwards, the specimens underwent cyclic fatigue during an aging procedure in a chewing simulator (1’200’000 chewing-cycles, 49 N force, 5–55°C temperature changes). Subsequently, the specimens were statically loaded and the load which was necessary to fracture the specimen (F max ) were measured. Differences between the groups were compared applying the Kruskal-Wallis (KW) test and the Wilcoxon-Mann-Whitney-Test (WMW: p < 0.05). The two-parameter Weibull distribution values were calculated. Results The fatigue resistance was 100% for the groups Lis, Vit, Liv, Amb, Mas and Ros, whereas the group Ema showed a fatigue resistance of 95%. The control group Lis showed median F max values of 2’328 N. The median F max values for the test groups ranged between 1’753 N (Vit) and 2’490 N (Ros). Statistically significant difference was observed among the groups Lis (control) and Vit (KW: p < 0.001). Weibull distribution presented the highest shape values for the group Ros (12.83) and the lowest values for the group Ema (4.71). Conclusion Regarding their load-bearing capacity different pressable lithium disilicates can be recommended to fabricate ultra-thin occlusal veneers on molars when restoring occlusal tooth wear.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Trauma and Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Fracture resistance of cad/cam occlusal veneers: a systematic review of laboratory studies10.1016/j.jmbbm.2020.103948 ↗
2. Fracture toughness of two lithium disilicate dental glass ceramics10.1016/j.prosdent.2016.02.009 ↗
3. Internal fit of pressed and computer-aided design/computer-aided manufacturing ceramic crowns made from digital and conventional impressions10.1016/j.prosdent.2014.09.015 ↗
4. Masticatory function--a review of the literature. 1. The form of the masticatory cycle10.1111/j.1365-2842.1975.tb00921.x ↗
5. Flexural strength of vitreous ceramics based on lithium disilicate and lithium silicate reinforced with zirconia for cad/cam10.1155/2022/5896511 ↗
6. The effect of dentin bonding and material thickness on the flexural properties of a lithium-disilicate glass-ceramic
7. An artificial oral environment for testing dental materials10.1109/10.133228 ↗
8. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
9. Contemporary diagnosis and management of dental erosion10.1111/jerd.12706 ↗
10. Mechanical properties of zirconia reinforced lithium silicate glass-ceramic10.1016/j.dental.2016.03.013 ↗
11. Effect of firing and fabrication technique on the marginal fit of heat-pressed lithium disilicate veneers10.1016/j.prosdent.2020.11.006 ↗
12. Posterior minimally invasive full-veneers: effect of ceramic thicknesses, bonding substrate, and preparation designs on failure-load and -mode after fatigue10.1111/jerd.12861 ↗
13. Prospective clinical split-mouth study of pressed and cad/cam all-ceramic partial-coverage restorations: 7-year results10.11607/ijp.3043 ↗
14. Properties of hot-pressed lithium silicate glass-ceramics10.1016/j.dental.2019.02.027 ↗
15. Load-bearing capacity of cad/cam 3d-printed zirconia, cad/cam milled zirconia, and heat-pressed lithium disilicate ultra-thin occlusal veneers on molars10.1016/j.dental.2020.01.016 ↗
16. Ultra-thin occlusal veneers bonded to enamel and made of ceramic or hybrid materials exhibit load-bearing capacities not different from conventional restorations10.1016/j.jmbbm.2018.09.041 ↗
17. The effect of core material, veneering porcelain, and fabrication technique on the biaxial flexural strength and weibull analysis of selected dental ceramics10.1111/j.1532-849X.2012.00845.x ↗
18. Severe tooth wear: European consensus statement on management guidelines
19. Load-bearing capacities of ultra-thin occlusal veneers bonded to dentin10.1016/j.jmbbm.2019.04.006 ↗
20. Relationship between internal accuracy and load-bearing capacity of minimally invasive lithium disilicate occlusal veneers10.11607/ijp.6735 ↗
21. Restorative therapy of erosive lesions10.1159/000360562 ↗
22. Fracture strength of lithium disilicate crowns compared to polymer-infiltrated ceramic-network and zirconia reinforced lithium silicate crowns10.1016/j.jmbbm.2017.06.025 ↗
23. In vitro evaluation of a mechanical testing chewing simulator10.1016/j.dental.2008.09.010 ↗
24. Competition of fracture mechanisms in monolithic dental ceramics: flat model systems10.1002/jbm.b.31100 ↗