journal article·2023-12

Investigation of mechanical properties and low-temperature degradation of dental 3Y-TZP ceramics fabricated by stereolithography in combination with microwave sintering

Li Wang, Yang Jiao, Lian Yao, Yang Sheng, Zongdong Hao, Weizhe Tang, Rui Dou

Publisher page

Abstract

The purpose of this study was to obtain dental ceramic materials with excellent mechanical properties and high resistance to low temperature degradation (LTD) via stereolithography (SLA) in combination with microwave sintering (MWS). The results have shown that the unaged MWS-1425 °C 3Y-TZP ceramics with uniform microstructure have high density up to 99.04% and excellent mechanical properties (Vickers hardness 14.07 GPa, fracture toughness 4.32 MPa m1/2, flexural strength 947.87 MPa). After 50 h of LTD, the m-phase content of MWS 3Y-TZP ceramics accounts for only 10.3%. In addition, the surface roughness increases by only 1.3 nm, the degraded depth is less than 5 μm, and the flexural strength exceeds 900 MPa. This exhibits the high resistance to LTD and excellent mechanical properties of dental 3Y-TZP ceramics can be obtained.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced materials and composites · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. Microwave processing of ceramics10.1016/S1359-0286(98)80011-9 ↗
2. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
3. Biaxial flexure strength and low temperature degradation of Ce‐TZP/Al2O3 nanocomposite and Y‐TZP as dental restoratives10.1002/jbm.b.31131 ↗
4. Threshold strength evaluation on an Al2O3–ZrO2 multilayered system10.1016/j.jeurceramsoc.2006.05.037 ↗
5. Improvement of microstructural properties of 3Y-TZP materials by conventional and non-conventional sintering techniques10.1016/j.ceramint.2011.06.035 ↗
6. Microwave sintering of zirconia materials: mechanical and microstructural properties10.1111/j.1744-7402.2011.02741.x ↗
7. Low temperature degradation of a Y-TZP dental ceramics10.1016/j.actbio.2010.09.020 ↗
8. Theory and experiment of martensitic nucleation in ZrO 2 containing ceramics and ferrous alloys10.1016/0001-6160(85)90006-9 ↗
9. Low-temperature ageing map for 3mol% Y2O3-ZrO210.1007/BF01107426 ↗
10. 3D printing of ceramics: a review10.1016/j.jeurceramsoc.2018.11.013 ↗
11. Low‐temperature aging of Y‐TZP ceramics10.1111/j.1151-2916.1999.tb02055.x ↗
12. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗
13. Low-temperature degradation of zirconia and implications for biomedical implants10.1146/annurev.matsci.37.052506.084250 ↗
14. Weibull analysis and flexural strength of hot-pressed core and veneered ceramic structures10.1016/S0109-5641(03)00010-1 ↗
15. Comparisons of grain size-density trajectory during microwave and conventional sintering of titanium nitride10.1016/j.jallcom.2013.07.159 ↗
16. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
17. Ceramic paste for space stereolithography 3D printing technology in microgravity environment10.1016/j.jeurceramsoc.2022.03.030 ↗
18. Effect of grain size on mechanical properties of submicrometer 3Y-TZP: fracture strength and hydrothermal degradation10.1111/j.1551-2916.2007.01643.x ↗
19. Degradation during aging of transformation-toughened ZrO2-Y2O3 materials at 250°C10.1111/j.1151-2916.1986.tb07415.x ↗
20. Strength, toughness and aging stability of highly-translucent Y-TZP ceramics for dental restorations
21. Accelerated aging characteristics of three yttria-stabilized tetragonal zirconia polycrystalline dental materials10.1016/S0022-3913(12)60166-8 ↗
22. Quantification of hydrothermal degradation in zirconia by nanoindentation10.1016/j.actamat.2008.04.050 ↗
23. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
24. Gautam · 2016
25. Mechanical and microstructural properties of ultra-translucent dental zirconia ceramic stabilized with 5 mol% yttria
26. Additive manufacturing of dense zirconia ceramics by fused deposition modeling via screw extrusion10.1016/j.jeurceramsoc.2020.09.018 ↗
27. Calibration curve for quantitative analysis of the monoclinic-tetragonal ZrO2 system by X-ray diffraction
28. Influence of sintering conditions on low-temperature degradation of dental zirconia10.1016/j.dental.2014.03.005 ↗
29. Influence of sintering conditions on low-temperature degradation of dental zirconia10.1016/j.dental.2014.03.005 ↗
30. B.S. Institution, ISO 6872. Dentistry. Ceramic Materials,.
31. Effect of the volume fraction of zirconia suspensions on the microstructure and physical properties of products produced by additive manufacturing10.1016/j.dental.2019.02.001 ↗
32. Microwave sintering of dense and lattice 3Y-TZP samples shaped by digital light processing
33. Hybrid microwave sintering of alumina and 3 mol% Y2O3-stabilized zirconia in a multimode cavity – influence of the sintering cell10.1016/j.ceramint.2022.03.072 ↗
34. The strength and hydrothermal stability of Y‐TZP ceramics for dental applications
35. Transformation toughening: Part 3, experimental observations in the ZrO2–Y2O3 system10.1007/BF00809059 ↗
36. Environmental degradation of zirconia ceramics10.1016/0955-2219(95)00035-S ↗
37. Strength and adaptation of stereolithography-fabricated zirconia dental crowns: an in vitro study10.11607/ijp.6262 ↗
38. Stability properties and microstructure properties of microwave-sintered CeO2 doped zirconia ceramics10.1016/j.ceramint.2021.06.234 ↗
39. Methodology for measuring fracture toughness of ceramic materials by instrumented indentation test with vickers indenter10.1111/jace.14650 ↗
40. Study of structural and electrical properties of conventional furnace and microwave‐sintered BaZr0. 10Ti0. 90O3 ceramics10.1111/j.1551-2916.2008.02885.x ↗
41. An overview of zirconia ceramics: basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
42. Microstructural study of microwave sintered zirconia for dental applications10.1016/j.ceramint.2014.09.055 ↗
43. Subsurface evaluation of hydrothermal degradation of zirconia10.1016/j.actamat.2010.09.047 ↗
44. Mechanical properties and low-temperature aging of tetragonal zirconia polycrystals processed by hot isostatic pressing10.1557/JMR.2003.0337 ↗
45. Additively manufactured zirconia for dental applications10.3390/ma14133694 ↗
46. Deceleration of hydrothermal degradation of 3Y–TZP by alumina and Lanthana Co-doping
47. Hydrothermal aging behavior of nanocrystalline Y-TZP ceramics10.1111/j.1551-2916.2010.04341.x ↗
48. Comparison between microwave and conventional sintering on the properties and microstructural evolution of tetragonal zirconia10.1016/j.ceramint.2018.02.086 ↗
49. Phase transformation, roughness, and microhardness of artificially aged yttria‐and magnesia‐stabilized zirconia femoral heads10.1002/jbm.a.31438 ↗
50. Characterization of ZrO2-Al2O3 composites sintered in a 2.45 GHz electromagnetic field
51. A study of the bending resistance of implant-supported reinforced alumina and machined zirconia abutments and copies10.1016/j.dental.2007.05.021 ↗
52. Effect of two-step sintering on the hydrothermal ageing resistance of tetragonal zirconia polycrystals10.1016/j.ceramint.2017.03.052 ↗
53. Quantitative analysis of monoclinic phase in 3Y-TZP by Raman spectroscopy10.1111/j.1551-2916.2010.03635.x ↗
54. Mechanical properties of Y-PSZ after aging at low temperature
55. Fabrication of high-strength Si/SiC composites with low shrinkage rates via vat photopolymerization technology and liquid silicon infiltration
56. Additive manufacturing of low-shrinkage alumina cores for single-crystal nickel-based superalloy turbine blade casting10.1016/j.ceramint.2022.02.052 ↗
57. Surface toughening of TZP ceramics by low temperature ageing10.1016/0272-8842(89)90004-7 ↗
58. The grain size dependence of the mechanical properties in TZP ceramics
59. Strength influencing variables on CAD/CAM zirconia frameworks10.1016/j.dental.2007.06.030 ↗
60. Effect of Fe2O3 doping on color and mechanical properties of dental 3Y-TZP ceramics fabricated by stereolithography-based additive manufacturing
61. Effect of sintering temperature and low-temperature aging on microstructure and flexural strength of Fe2O3-doped 3Y-TZP ceramics fabricated by stereolithography-based additive manufacturing10.1016/j.ceramint.2023.09.055 ↗
62. Iron oxide colouring of highly-translucent 3Y-TZP ceramics for dental restorations10.1016/j.jeurceramsoc.2018.09.043 ↗
63. ZrO2 nanopowders prepared by low-temperature vapor-phase hydrolysis10.1111/j.1151-2916.2000.tb01333.x ↗
64. Extrusion-based additive manufacturing of yttria-partially-stabilized zirconia ceramics10.1016/j.ceramint.2019.10.245 ↗
65. Lifetime estimation of zirconia ceramics by linear ageing kinetics10.1016/j.actamat.2015.04.001 ↗
66. Zirconia toughened alumina (ZTA) ceramics10.1016/0010-4361(90)90021-N ↗