Simulation of CAD/CAM milling on lithium disilicate: Mechanical and topographic analyses of surface grinding different protocols
Source abstract
Abstract
The aim of this study was to evaluate the topography and the fatigue performance of lithium disilicate glass-ceramic after surface grinding through different laboratory protocols used to simulate the Computer-aided design/Computer-aided manufacturing (CAD/CAM) milling. Ceramic discs (IPS e.max CAD, Ø = 13.5 mm × 1.2 mm of thickness) were produced through different methodologies: milling in CAD/CAM system (CAD/CAM group); produced in-lab with a polished surface (POL group); or produced through in-lab methods and randomly distributed into five groups according to different grinding protocols to simulate the CAD/CAM milling [grinding with a CAD/CAM bur coupled to a mandrel (CAD/CAM Bur group); fine diamond bur using oscillatory movements (DBO group); fine diamond bur in x and y axes of the disc (DBXY group); #60-grit silicon carbide sandpaper (SiC group); and #60-grit wood sandpaper (WS group)]. The specimens were fatigue tested (n = 15) according to the step-stress method (initial load: 60 N; step-size: 20 N; 10,000 cycles/step; 20 Hz frequency). A roughness analysis was performed on all specimens, while fractal dimension (FD) and fractography were performed on representative samples. The Kaplan-Meier analysis showed that the POL (293.3 N) group presented better fatigue performance (higher load and number of cycles for failure) (p < 0.05) than the other groups (CAD/CAM = 222.7 N; CAD/CAM Bur = 181.3 N; DBO = 184.0 N; DBXY = 192.0 N; SiC = 182.6 N; WS = 182.6 N). For roughness, only the SiC (Ra = 1.616; Rz = 10.465) and WS (Ra = 1.673; Rz = 10.655) groups produced statistically similar Ra (μm) and Rz (μm) values to the CAD/CAM (Ra = 1.628; Rz = 9.571) group (p > 0.05). The surface created by CAD/CAM milling and POL group exhibited more complexity (FD) higher values than the experimental groups. For the ceramic surface topography images, the CAD/CAM milling visibly produced a uniform surface compared to the other groups; however, the POL group was the smoothest. The DBO, DBXY, SiC, and WS groups resulted in similar characteristics of surface topography. Therefore, although the SiC and WS groups showed similar roughness to the control group (CAD/CAM), no in-lab simulation method was fully capable to mimic the mechanical performance of the CAD/CAM-milled lithium disilicate glass-ceramic.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Advanced Surface Polishing Techniques · Advanced machining processes and optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Microtensile bond strength of lithium disilicate ceramics to resin adhesives
2. Machining variability impacts on the strength of a 'chair-side' CAD-CAM ceramic10.1016/j.dental.2012.04.017 ↗
3. Fracture, roughness and phase transformation in CAD/CAM milling and subsequent surface treatments of lithium metasilicate/disilicate glass-ceramics10.1016/j.jmbbm.2017.06.015 ↗
4. The effect of crown fabrication process on the fatigue life of the tooth-crown structure10.1016/j.msec.2019.110272 ↗
5. Phenomena and mechanisms of crack propagation in glass-ceramics10.1016/j.jmbbm.2007.11.005 ↗
6. The current state of chairside digital dentistry and materials
7. The contact mechanics of fractal surfaces10.1038/nmat855 ↗
8. Grinding damage assessment for CAD-CAM restorative materials10.1016/j.dental.2016.12.004 ↗
9. One-step ceramic primer as surface conditioner: effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations10.1016/j.jmbbm.2020.103686 ↗
10. The effect of internal roughness and bonding on the fracture resistance and structural reliability of lithium disilicate ceramic10.1016/j.dental.2017.09.018 ↗
11. Ceramics for dental applications: a review10.3390/ma3010351 ↗
12. Hard machining, glaze firing and hydrofluoric acid etching: do these procedures affect the flexural strength of a leucite glass-ceramic?10.1016/j.dental.2015.04.005 ↗
13. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
14. Using fractal geometry to examine failed implants and prostheses10.1016/j.dental.2018.09.007 ↗
15. Fatigue performance of distinct CAD/CAM dental ceramics
16. ISO 4287-1997 · 1997
17. 2015
18. Clinically relevant approach to failure testing of all-ceramic restorations10.1016/S0022-3913(99)70103-4 ↗
19. A Panorama of dental CAD/CAM restorative systems
20. Fatigue resistance of ultrathin CAD/CAM complete crowns with a simplified cementation process10.1016/j.prosdent.2015.04.014 ↗
21. Effect of acid etching on tridimensional microstructure of etchable CAD/CAM materials10.1016/j.dental.2018.03.013 ↗
22. In-lab simulation of CAD/CAM milling of lithium disilicate glass-ceramic specimens: effect on the fatigue behavior of the bonded ceramic10.1016/j.jmbbm.2021.104604 ↗
23. Surface milled by CAD-CAM system vs laboratorial methods to simulate the milled surface: effect on the resin bond strength to lithium disilicate glass-ceramic10.1016/j.ijadhadh.2021.103068 ↗
24. Near-surface damage- a persistent problem in crowns obtained by computer-aided design and manufacturing10.1243/095441105X9363 ↗
25. Microtensile bond strength of lithium disilicate to zirconia with the CAD-on technique10.1111/jopr.12246 ↗
26. Internal adjustments decrease the fatigue failure load of bonded simplified lithium disilicate restorations10.1016/j.dental.2018.05.015 ↗
27. The effect of abrading and cutting instruments on machinability of dental ceramics10.1007/s10856-018-6031-y ↗
28. Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: conventional ceramic etching vs etch & prime one-step primer10.1016/j.dental.2018.04.012 ↗
29. CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: fatigue performance and ceramic surface characteristics10.1016/j.jmbbm.2019.03.005 ↗
30. Dental ceramics: a review of new materials and processing methods10.1590/1807-3107bor-2017.vol31.0058 ↗
31. The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs10.1016/j.dental.2018.01.010 ↗
32. Fatigue failure load of feldspathic ceramic crowns after hydrofluoric acid etching at different concentrations10.1016/j.prosdent.2017.03.021 ↗
33. Mechanical reliability, fatigue strength and survival analysis of newpolycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
34. Accelerated loading frequency does not influence the fatigue behavior of polymer infiltrated ceramic network or lithium disilicate glass-ceramic restorations