Influence of CAD/CAM diamond bur wear on the accuracy and surface roughness of dental ceramic restorations: A systematic review
Source abstract
Abstract
OBJECTIVES: To systematically review the current literature investigating the computer-aided design/computer-aided manufacturing (CAD/CAM) diamond bur deterioration with repeated use and its effects on the accuracy, marginal and internal fit, and surface roughness of the dental ceramic restorations from the subtractive manufacturing technique. MATERIALS AND METHODS: Three online databases, Ovid, Scopus, and Web of Science, were screened up to February 2024. In vitro studies investigating bur wear and its influences on subtractively-manufactured (SMed) ceramic restorations, except zirconia, were included. The selected articles were limited to English-language and peer-reviewed publications. Additionally, a manual search was conducted by screening the reference lists of included studies. The risk of bias of included articles was assessed following the modified Consolidated Standards of Reporting Trials (CONSORT) checklist. RESULTS: Twelve studies satisfied the inclusion criteria and were included. Only one study reported that the influence of bur deterioration on the trueness of SMed restorations depended on the crown areas, but the proximal contacts showed a significant reduction. Five studies assessed the effect on marginal and internal adaptation. To a certain extent, repeated use of the same diamond burs causes a progressive increase in the marginal gap and a slight decrease in the internal luting space. Half of the included studies assessed surface roughness. The influence of bur wear was mainly due to the bur-material combination. CONCLUSIONS: During subtractive manufacturing, bur deterioration is a crucial factor influencing the quality of fabricated ceramic restorations. Diamond burs must be replaced regularly to avoid compromising the accuracy of subtractively manufactured restorations.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Anatomy and Medical Technology
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Trends in computer-aided manufacturing in prosthodontics: a review of the available streams10.1155/2014/783948 ↗
2. Machining variability impacts on the strength of a ‘chair-side’ CAD–CAM ceramic10.1016/j.dental.2012.04.017 ↗
3. A base-line study of the wear of burs used for chairside milling of ceramic crowns of different hardness: effect on internal fit and surface roughness10.17159/2519-0105/2020/v75no10a1 ↗
4. Effect of CAD-CAM tool deterioration on the trueness of ceramic restorations10.1016/j.prosdent.2020.09.035 ↗
5. Effect of CAD/CAM bur deterioration on the surface roughness of ceramic crowns10.1111/jopr.13404 ↗
6. The use of confocal microscopy to assess surface roughness of two milled CAD–CAM ceramics following two polishing techniques10.1016/j.dental.2006.06.012 ↗
7. Fabrication of dental restorations using digital technologies: techniques and materials
8. Surface quality of yttria-stabilized tetragonal zirconia polycrystal in CAD/CAM milling, sintering, polishing and sandblasting processes10.1016/j.jmbbm.2016.08.021 ↗
9. Effect of sandblasting, grinding, polishing and glazing on the flexural strength of two processable all-ceramic dental materials10.1016/j.jdent.2003.08.006 ↗
10. Trueness and precision of milled and 3D printed root-analogue implants: a comparative in vitro study10.1016/j.jdent.2023.104425 ↗
11. 3D and 2D marginal fit of pressed and CAD/CAM lithium disilicate crowns made from digital and conventional impressions10.1111/jopr.12180 ↗
12. Marginal fit comparison of CAD/CAM crowns milled from two different materials10.1111/jopr.12683 ↗
13. Digital dentistry: an overview of recent developments for CAD/CAM generated restorations10.1038/sj.bdj.2008.350 ↗
14. Effect of the microstructure on the lifetime of dental ceramics10.1016/j.dental.2011.04.003 ↗
15. A 3-dimensional accuracy analysis of chairside CAD/CAM milling processes10.1016/j.prosdent.2014.05.012 ↗
16. Effect of repeated millings on the surface integrity of diamond burs and roughness of different CAD/CAM materials10.1007/s00784-022-04500-2 ↗
17. Trueness of the inner surface of monolithic crowns fabricated by milling of a fully sintered (Y, Nb)-TZP block in chairside CAD–CAM system for single-visit dentistry10.3390/ma12193253 ↗
18. Vickers micro-hardness of new restorative CAD/CAM dental materials: evaluation and comparison after exposure to acidic drink10.3390/ma12081246 ↗
19. Marginal adaptation of ceramic crowns: a systematic review10.1016/j.prosdent.2013.08.003 ↗
20. Influence of CAD-CAM diamond bur deterioration on surface roughness and maximum failure load of Y-TZP-based restorations
21. Grinding damage assessment for CAD-CAM restorative materials10.1016/j.dental.2016.12.004 ↗
22. The use of CAD/CAM in dentistry
23. The influence of surface roughness on porcelain strength10.1016/S0109-5641(00)00030-0 ↗
24. The effect of internal roughness and bonding on the fracture resistance and structural reliability of lithium disilicate ceramic10.1016/j.dental.2017.09.018 ↗
25. Effects of nano-diamond-coated milling bits on cutting dental zirconia10.3390/coatings14040473 ↗
26. Guidelines for reporting pre-clinical in vitro studies on dental materials10.1016/j.jebdp.2012.10.001 ↗
27. Effect of in vivo crown margin discrepancies on periodontal health10.1016/0022-3913(91)90225-L ↗
28. Hard machining, glaze firing and hydrofluoric acid etching: do these procedures affect the flexural strength of a leucite glass–ceramic?10.1016/j.dental.2015.04.005 ↗
29. Emerging trends in high-speed micro-machining of dental ceramics through CAD-CAM systems
30. Microleakage—full crowns and the dental pulp10.1016/S0099-2399(06)81345-2 ↗
31. Accuracy of ceramic restorations made with two CAD/CAM systems10.1016/S0022-3913(13)60020-7 ↗
32. 2023
33. An investigation of dental luting cement solubility as a function of the marginal gap10.1016/0022-3913(91)90239-S ↗
34. Computer‐assisted technologies used in oral rehabilitation and the clinical documentation of alleged advantages – a systematic review10.1111/joor.12483 ↗
35. Evaluation of surface characteristics of dental composites using profilometry, scanning electron, atomic force microscopy and gloss-meter10.1007/s10856-006-0675-8 ↗
36. Trueness of milled prostheses according to number of ball-end mill burs10.1016/j.prosdent.2015.10.014 ↗
37. Influence of CAD/CAM tool and material on tool wear and roughness of dental prostheses after milling10.1016/j.prosdent.2014.12.021 ↗
38. Sequential usage of diamond bur for CAD/CAM milling: effect on the roughness, topography and fatigue strength of lithium disilicate glass ceramic10.1016/j.jmbbm.2018.12.037 ↗
39. The estimation of cement film thickness by an in vivo technique10.1038/sj.bdj.4802708 ↗
40. Accuracy, trueness, and precision - a guideline for the evaluation of these basic values in digital dentistry
41. The effect of milling and postmilling procedures on the surface roughness of CAD/CAM materials10.1111/jerd.12326 ↗
42. Micro-computed tomography evaluation of marginal fit of lithium disilicate crowns fabricated by using chairside CAD/CAM systems or the heat-pressing technique10.1016/j.prosdent.2014.04.028 ↗
43. The PRISMA 2020 statement: an updated guideline for reporting systematic reviews
44. Evaluating the effect of repeated use of milling burs on surface roughness and adaptation of digitally fabricated ceramic veneers10.1016/j.heliyon.2021.e06896 ↗
45. Influence of CAD-CAM milling strategies on the outcome of indirect restorations: a scoping review10.1016/j.prosdent.2024.02.021 ↗
46. Metallic glass matrix composites10.1016/j.mser.2015.12.001 ↗
47. On the nature of machining cracks in ground ceramics: Part I: SRBSN strength and fractographic analysis10.1081/MST-200059038 ↗
48. Digitalization in restorative dentistry
49. Influence of computer-aided design/computer-aided manufacturing diamond bur wear on marginal misfit of two lithium disilicate ceramic systems10.2341/19-089-L ↗
50. Near-surface damage--a persistent problem in crowns obtained by computer-aided design and manufacturing10.1243/095441105X9363 ↗
51. CAD/CAM diamond tool wear
52. Accuracy of marginal fit and axial wall contour for lithium disilicate crowns fabricated using three digital workflows10.1016/j.prosdent.2018.11.003 ↗
53. Newer vs. older CAD/CAM burs: influence of bur experience on the fatigue behavior of adhesively cemented simplified lithium-disilicate glass-ceramic restorations10.1016/j.jmbbm.2019.04.002 ↗
54. Impact of diamond tool wear on the surface finish of lithium silicate glass ceramics machined with the assistance of CAD/CAM systems10.1007/s40430-022-03952-7 ↗
55. The marginal gaps of sequentially milled lithium disilicate crowns using two different milling units10.1111/adj.12909 ↗
56. J. Prosthet. Dent · 2023 · 130 · e710.1016/j.prosdent.2023.03.002 ↗
57. Machining accuracy of CAD/CAM ceramic crowns fabricated with repeated machining using the same diamond bur10.4012/dmj.24.123 ↗
58. Effect of the region of the CAD/CAM block on the flexural strength and structural reliability of restorative materials10.1016/j.jmbbm.2022.105597 ↗
59. Durability of diamond burs for the fabrication of ceramic crowns using dental CAD/CAM10.4012/dmj.24.134 ↗
60. An overview of in vitro abrasive finishing & CAD/CAM of bioceramics in restorative dentistry10.1016/j.ijmachtools.2005.07.045 ↗
61. Comparative evaluation of mechanical properties and wear ability of five CAD/CAM dental blocks10.3390/ma12142252 ↗
62. Damage accumulation and fatigue life of particle-abraded ceramics