J-integral fracture toughness, Tearing modulus and tensile properties of Vitamin E stabilized radiation crosslinked UHMWPE
Source abstract
Abstract
Radiation crosslinking of ultra-high molecular weight polyethylene (UHMWPE) increases its wear resistance in total joint replacement prostheses. Unfortunately, it is accompanied by a dose-dependent decrease in several mechanical properties. In this study, the tensile properties and fracture behavior of radiation crosslinked, Vitamin E stabilized UHMWPE was studied as a function of radiation dose. The Rice and Sorensen model, applicable to elastic-plastic materials, was utilized to obtain the initial crack driving force, J1c, steady state J-integral fracture toughness, Jss and the Tearing modulus. Tensile tests showed the dependence of tensile properties on radiation dose. Jss of non-crosslinked UHMWPE was higher than for crosslinked UHMWPE׳s but there was no dose dependent change in Jss whereas there was almost no change in J1c over the entire dose range. Finally, a monotonic decrease in Tearing modulus was observed with radiation dose.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Advanced materials and composites · Total Knee Arthroplasty Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Characterization of network parameters for UHMWPE by plane strain compression10.1016/j.jmbbm.2013.12.004 ↗
2. Compression and tension fatigue resistance of medical grade ultra high molecular weight polyethylene: the effect of morphology, sterilization, aging and temperature10.1016/S0032-3861(99)00199-8 ↗
3. The effects of degree of crosslinking on the fatigue crack initiation and propagation resistance of orthopedic-grade polyethylene10.1002/jbm.a.10606 ↗
4. Oxidation behaviour in prosthetic UHMWPE components sterilised with high energy radiation in a low-oxygen environment10.1016/j.polymdegradstab.2006.02.003 ↗
5. Gamma irradiation alters fatigue-crack behavior and fracture toughness in 1900H and GUR 1050 UHMWPE10.1002/jbm.10335 ↗
6. Oxidation of orthopaedic UHMWPE10.1016/S0142-9612(01)00288-5 ↗
7. Oxidation of orthopaedic UHMWPE (vol 23, pg 1613, 2002)
8. Oxidation and oxidation potential in contemporary packaging for polyethylene total joint replacement components10.1002/jbm.b.30454 ↗
9. High temperature melted, radiation cross-linked, vitamin E stabilized oxidation resistant UHMWPE with low wear and high impact strength10.1016/j.polymer.2012.11.017 ↗
10. The effects of gamma radiation sterilization and ageing on the structure and morphology of medical grade ultra high molecular weight polyethylene10.1016/0032-3861(96)89386-4 ↗
11. J-integral fracture toughness and tearing modulus measurement of radiation cross-linked UHMWPE10.1016/S0736-0266(02)00073-6 ↗
12. Kumar · 1981
13. Advances in the processing, sterilization, and crosslinking of ultra-high molecular weight polyethylene for total joint arthroplasty10.1016/S0142-9612(99)00053-8 ↗
14. Development of an extremely wear-resistant ultra high molecular weight polyethylene for total hip replacements10.1002/jor.1100170203 ↗
15. Effect of sterilization method and other modifications on the wear resistance of acetabular cups made of ultra-high molecular weight polyethylene – a hip-simulator study10.2106/00004623-200012000-00004 ↗
16. Effect of molecular weight, calcium stearate, and sterilization methods on the wear of ultra high molecular weight polyethylene acetabular cups in a hip joint simulator10.1002/jor.1100170306 ↗
17. Comparative fatigue behavior and toughness of remelted and annealed highly crosslinked polyethylenes10.1002/jbm.b.30807 ↗
18. Microstructural fracture processes accompanying growing cracks in tough rubber-modified polyamides10.1016/0032-3861(95)99294-5 ↗
19. Unified wear model for highly crosslinked ultra-high molecular weight polyethylenes (UHMWPE)10.1016/S0142-9612(99)00039-3 ↗
20. Vitamin E diffused, highly crosslinked UHMWPE: a review10.1007/s00264-010-1161-y ↗
21. Mechanisms of decrease in fatigue crack propagation resistance in irradiated and melted UHMWPE10.1016/j.biomaterials.2005.06.025 ↗
22. The effects of high dose irradiation on the cross-linking of vitamin E-blended ultrahigh molecular weight polyethylene10.1016/j.biomaterials.2008.05.004 ↗
23. Characterization of irradiated blends of alpha-tocopherol and UHMWPE10.1016/j.biomaterials.2005.04.026 ↗
24. Viscosity and self-diffusion coefficient of hydrogenated polybutadiene10.1021/ma00081a014 ↗
25. Molecular rearrangements in ultra high molecular weight polyethylene after irradiation and long-term storage in air10.1016/S0032-3861(98)00438-8 ↗
26. A path independent integral and approximate analysis of strain concentration by notches and cracks10.1115/1.3601206 ↗
27. Continuing crack-tip deformation and fracture for plane-strain crack growth in elastic-plastic solids10.1016/0022-5096(78)90007-8 ↗
28. Prevention of fatigue cracks in ultrahigh molecular weight polyethylene joint components by the addition of vitamin E10.1002/(SICI)1097-4636(1999)48:4<474::AID-JBM11>3.0.CO;2-T ↗
29. The antioxidant and non-antioxidant contributions of vitamin E in vitamin E blended ultra-high molecular weight polyethylene for total knee replacement10.1016/j.jmbbm.2012.12.006 ↗
30. Rheology and reptation of linear polymers. Ultrahigh molecular weight chain dynamics in the melt10.1122/1.1718367 ↗