Effect of different finishing/polishing techniques and glaze application on the flexural strength of ultratranslucent zirconia after hydrothermal aging
Source abstract
Abstract
Purpose To evaluate the effect of different finishing/polishing procedures and glaze on the surface roughness, flexure strength, and microstructure of an ultratranslucent zirconia (UZ) submitted aging. Methodology Two hundred and forty (240) UZ bars were sintered (8 × 2 × 1 mm) and treated according to the factors (n = 15): Type of finishing/polishing procedure (Control - Ctrl; Ultra-fine Diamond Burr - FG; Medium grit diamond burr- MG; Stone Bur - Stone; Rubber - Rub; FG + Rub; MG + Rub; Stone + Rub), and "Glaze" (Without and With - Gl). The bars were hydrothermally degraded (24 h, 127 °C, 1.7 bar), submitted to roughness analysis and 3-point mini flexural strength (FS) test. Scanning Electron Microscopy (SEM), X-ray Diffraction (XDR), and Weibull analysis were performed. Data were analyzed by 2-way ANOVA and Tukey test (5%). Results Finishing/Polishing' and its interaction with 'Glaze' were statistically significant (P < 0.0001) for FS, unlike 'Glaze' alone (P = 0.8827). Rub (602.11 MPaA), Stone + Rub (555.50 MPaAB), and Ctrl (621.72 MPaA) showed superior FS, while FG_GL showed the lowest FS. Stone + Rub showed the highest Weibull modulus (13.15a). Ctrl_Gl (0.18 ± 0.02F μm) and Ctrl + Rub_Gl (0.29 ± 0.07F μm) showed the lowest roughness. Glaze (0.48B) reduced the roughness of the groups that did not receive it (1.56A), with MG (2.60 ± 0.69A μm) and FG (2.50 ± 0.7A μm) exhibiting rougher surfaces. Conclusions Rubber polishers are ideal for minor adjustments to UZ while Stone followed by rubber is effective for greater abrasion without compromising mechanical strength. The application of glaze did not reduce mechanical strength and resulted in lower surface roughness compared to the non-glazed groups, with the exception of the FG groups.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Bridging the gap between clinical failure and laboratory fracture strength tests using a fractographic approach10.1016/j.dental.2008.09.001 ↗
2. Does diamond stone grinding change the surface characteristics and flexural strength of monolithic zirconia?10.2341/19-023-L ↗
3. Low-temperature degradation of a Y-TZP ceramic after surface treatments10.1002/jbm.b.32957 ↗
4. Comparative evaluation of the efficiency of four ceramic finishing systems
5. Effect of polishing procedures and hydrothermal aging on wear characteristics and phase transformation of Zirconium Dioxide10.1016/j.prosdent.2016.09.004 ↗
6. Longevity of extrinsic stains on monolithic zirconia restorations: an in vitro study10.1016/j.prosdent.2023.09.008 ↗
7. Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications10.1016/j.dental.2018.03.006 ↗
8. Effect of finishing/polishing techniques and aging on topography, C. albicans adherence, and flexural strength of ultra-translucent zirconia: an in situ study10.1007/s00784-021-04068-3 ↗
9. Recent advances in dental zirconia: 15 years of material and processing evolution10.1016/j.dental.2024.02.026 ↗
10. In vitro evaluation of bond strength between zirconia core and CAD/CAM-Produced veneers10.1111/jopr.13068 ↗
11. Monolithic ceramics: effect of finishing techniques on surface properties, bacterial adhesion and cell viability10.2341/17-011-L ↗
12. Should finishing, polishing or glazing be performed after grinding YSZ ceramics? A systematic review and meta-analysis10.1016/j.jmbbm.2023.105654 ↗
13. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
14. 2019
15. Grinding with diamond burs and hydrothermal aging of a Y-TZP material: effect on the material surface characteristics and bacterial adhesion10.2341/16-108-L ↗
16. The effect of glaze on porcelain strength10.1016/0109-5641(92)90084-P ↗
17. Edge chipping of translucent zirconia10.1016/j.prosdent.2020.12.009 ↗
18. Resistência à fratura de restaurações monolíticas de vitrocerâmica versus restaurações bicamadas à base de zircônia
19. The mechanical behavior of high-translucent monolithic zirconia after adjustment and finishing procedures and artificial aging10.1016/j.prosdent.2018.12.013 ↗
20. Surface roughness of zirconia for full-contour crowns after clinically simulated grinding and polishing10.1038/ijos.2014.34 ↗
21. Effect of grinding and polishing on roughness and strength of zirconia10.1016/j.prosdent.2017.04.003 ↗
22. Concerns of hydrothermal degradation in CAD/CAM Zirconia10.1177/0022034509354193 ↗
23. Clinical risk factors related to failures with zirconia-based restorations: an up to 9-year retrospective study10.1016/j.jdent.2013.10.009 ↗
24. Strength and reliability of surface treated Y-TZP dental ceramics10.1002/1097-4636(2000)53:4<304::AID-JBM4>3.0.CO;2-S ↗
25. Effects of different surface finishing protocols for zirconia on surface roughness and bacterial biofilm formation10.4047/jap.2019.11.1.41 ↗
26. Effect of glazing application side and mechanical cycling on the biaxial flexural strength and Weibull characteristics of a Y-TZP ceramic10.1590/1678-7757-2020-0438 ↗
27. Effect of printing layer orientation and polishing on the fatigue strength of 3D-printed dental zirconia10.1016/j.dental.2023.11.007 ↗
28. Graded ultra-translucent zirconia (5Y-PSZ) for strength and functionalities10.1177/0022034518771287 ↗
29. Effect of intra-oral aging on T→M phase transformation, microstructure, and mechanical properties of Y-TZP dental ceramics10.1016/j.jmbbm.2017.04.014 ↗
30. A fractographic study of clinically retrieved zirconia-ceramic and metal-ceramic fixed dental prostheses10.1016/j.dental.2015.07.003 ↗
31. The effect of grinding on the mechanical behavior of Y-TZP ceramics: a systematic review and meta-analyses10.1016/j.jmbbm.2016.06.028 ↗
32. A systematic review of the survival and complication rates of zirconia-ceramic and metal-ceramic single crowns10.1111/clr.13306 ↗
33. Prosthodontic rehabilitation with fixed monolithic translucent zirconia restorations: a case history report10.11607/ijp.6194 ↗
34. Adhesion behavior of conventional and high-translucent zirconia: Effect of surface conditioning methods and aging using an experimental methodology10.1111/jerd.12490 ↗
35. Effect of surface finishing and polishing procedures on color properties and translucency of monolithic zirconia restorations at varying thickness10.1111/jerd.12681 ↗
36. ADM guidance-Ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
37. Clinical performance of minimally invasive monolithic ultratranslucent zirconia veneers: a case series up to five years of follow-up10.2341/22-118-T ↗
38. Flexural strength and crystalline stability of a monolithic translucent zirconia subjected to grinding, polishing and thermal challenges10.1016/j.ceramint.2020.07.114 ↗
39. Ultrathin monolithic zirconia veneers: reality or future? Report of a clinical case and one-year follow-up10.2341/16-350-T ↗
40. Time-lasting ceramic stains and glaze: a toothbrush simulation study10.1111/jerd.12590 ↗
41. Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing10.1016/j.dental.2004.07.013 ↗
42. Effect of finishing/polishing techniques and low temperature degradation on the surface topography, phase transformation and flexural strength of ultra-translucent ZrO2 ceramic10.1016/j.dental.2020.01.004 ↗
43. Zirconia-based screw-retained prostheses supported by implants: a retrospective study on technical complications and failures10.1111/cid.12214 ↗
44. Polishing of ground Y-TZP ceramic is mandatory for improving the mechanical behavior10.1590/0103-6440201802044 ↗
45. Influence of finishing/polishing on the fatigue strength, surface topography, and roughness of anyttrium-stabilized tetragonal zirconia polycrystals subjected to grinding10.1016/j.jmbbm.2019.02.013 ↗
46. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗