Influence of different surface finishing procedures of strength-gradient multilayered zirconia crowns on two-body wear and fracture load: Lithium silicate or leucite glazing versus polishing?
Source abstract
Abstract
Objectives To examine the influence of different finishing procedures on the surface roughness, wear resistance and fracture load of strength-gradient multilayered zirconia. Materials and methods Zirconia crowns (Multilayer 3D pro; n = 96) were manufactured and treated with a lithium-silicate- (LISI_S), leucite-based glaze spray (LEU_S), leucite-based glaze mass (LEU_M) or polished (POL). Natural molars (CG; n = 24) acted as a control. Roughness was determined on flat glazed specimens (n = 28). Two-body wear was examined by digitalizing and matching the occlusal surface before and after thermo-mechanical aging (6,000 thermal and 1,200,000 chewing cycles). The groups were split to measure fracture load initially and after aging. Kolmogorov-Smirnov, Spearman correlation, Kruskal-Wallis-H, Levene's test, one-way ANOVA with Scheffé post-hoc and Weibull modulus were computed. Results POL presented the lowest and LEU_S the highest roughness. Following POL, no ceramic loss was observed. LISI_S, LEU_S and LEU_M showed lower ceramic wear than the CG. The lowest wear of the antagonist was observed for the CG. LISI_S showed a lower antagonistic wear than LEU_S, LEU_M and POL. LISI_S, LEU_S, LEU_M and POL showed higher fracture load values and Weibull moduli than the CG. Artificial aging did not impact the fracture load or Weibull moduli. Significance With glazed groups showing height losses closer to the CG, glazing should be preferred to polishing when approximating the wear behavior of a natural dentition. Finishing of monolithic zirconia by glazing with a lithium silicate-based spray is recommended to preserve the antagonists. All examined zirconia crowns presented sufficient mechanical properties to withstand masticatory forces, even after prolonged aging.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Advanced ceramic materials synthesis · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Clinical trials in zirconia: a systematic review
2. Enamel wear against monolithic zirconia restorations: a meta-analysis and systematic review of in vitro studies10.1111/jerd.12823 ↗
3. Comparative evaluation of the efficiency of four ceramic finishing systems
4. Effect of glaze thickness on the fracture toughness and hardness of alumina-reinforced porcelain10.1016/S0022-3913(99)70204-0 ↗
5. Two-body wear performance of dental colored zirconia after different surface treatments10.1016/j.prosdent.2016.02.006 ↗
6. Masticatory function-a review of the literature: (II) Speed of movement of the mandible, rate of chewing and forces developed in chewing10.1111/j.1365-2842.1975.tb01535.x ↗
7. Masticatory function - a review of the literature. III. Masticatory performance and efficiency10.1111/j.1365-2842.1976.tb00929.x ↗
8. Two regression methods for estimation of a two-parameter Weibull distribution for reliability of dental materials10.1016/j.dental.2014.11.014 ↗
9. The influence of gender and bruxism on the human maximum bite force10.1590/S1678-77572006000600011 ↗
10. Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications10.1016/j.dental.2018.03.006 ↗
11. Confocal examination of subsurface cracking in ceramic materials10.1111/j.1532-849X.2009.00447.x ↗
12. The effect of glaze on porcelain strength10.1016/0109-5641(92)90084-P ↗
13. Effect of external staining on the optical properties and surface roughness of monolithic zirconia of different thicknesses10.1016/j.prosdent.2021.08.014 ↗
14. Reliability and strength of all-ceramic dental restorations fabricated by direct ceramic machining (DCM)
15. Evaluation of the effect of different glazing brands on surface roughness of monolithic zirconia10.51173/jt.v5i2.940 ↗
16. Zirconia and its novel compositions: what do clinicians need to know?
17. The mechanical behavior of high-translucent monolithic zirconia after adjustment and finishing procedures and artificial aging10.1016/j.prosdent.2018.12.013 ↗
18. Impact of multiple firings on fracture load of veneered zirconia restorations10.1016/j.jmbbm.2022.105213 ↗
19. Impact of multiple firings on thermal properties and bond strength of veneered zirconia restorations10.1016/j.jmbbm.2022.105134 ↗
20. A comparison of the microstructure and properties of the IPS Empress 2 and the IPS Empress glass-ceramics10.1002/1097-4636(2000)53:4<297::AID-JBM3>3.0.CO;2-G ↗
21. Wear behavior of graded glass/zirconia crowns and their antagonists10.1177/0022034518820918 ↗
22. Effect of grinding and polishing on roughness and strength of zirconia10.1016/j.prosdent.2017.04.003 ↗
23. Wear evaluation of the human enamel opposing different Y-TZP dental ceramics and other porcelains10.1016/j.jdent.2012.08.004 ↗
24. The effects of artificial aging on high translucent zirconia
25. Effects of crystal size on the mechanical properties of a lithium disilicate glass-ceramic10.1016/j.msea.2016.05.068 ↗
26. The effect of core material, veneering porcelain, and fabrication technique on the biaxial flexural strength and weibull analysis of selected dental ceramics10.1111/j.1532-849X.2012.00845.x ↗
27. Evaluation of wear behavior of dental restorative materials against zirconia in vitro10.1016/j.dental.2022.04.016 ↗
28. Comparison between novel strength-gradient and color-gradient multilayered zirconia using conventional and high-speed sintering10.1016/j.jmbbm.2020.103977 ↗
29. Effect of glazing on translucency, color, and surface roughness of monolithic zirconia materials10.1111/jerd.12493 ↗
30. Effect of coarse grinding, overglazing, and 2 polishing systems on the flexural strength, surface roughness, and phase transformation of yttrium-stabilized tetragonal zirconia
31. Monolithic zirconia crowns – wall thickness, surface treatment and load at fracture10.1080/26415275.2019.1642112 ↗
32. Mechanical reliability, fatigue strength and survival analysis of new polycrystalline translucent zirconia ceramics for monolithic restorations10.1016/j.jmbbm.2018.05.029 ↗
33. Wear performance of substructure ceramics and veneering porcelains10.1016/j.dental.2011.04.001 ↗
34. Stability and wear of zirconia crowns with micro-layering10.1016/j.jdent.2023.104560 ↗
35. Fatigue and wear behaviour of zirconia materials10.1016/j.jmbbm.2020.103970 ↗
36. Two-body wear of dental porcelain and substructure oxide ceramics10.1007/s00784-011-0589-9 ↗
37. 10-year randomized trial (RCT) of zirconia-ceramic and metal-ceramic fixed dental prostheses10.1016/j.jdent.2018.05.015 ↗
38. Effects of dynamic aging on the wear and fracture strength of monolithic zirconia restorations10.1186/s12903-018-0618-z ↗
39. Methodology investigation: impact of crown geometry, crown, abutment and antagonist material and thermal loading on the two-body wear of dental materials10.1016/j.dental.2021.12.009 ↗
40. In vitro fracture load of monolithic lithium disilicate ceramic molar crowns with different wall thicknesses10.1007/s00784-013-1062-8 ↗
41. Comparative evaluation of enamel surface roughness after debonding using four finishing and polishing systems for residual resin removal - an in vitro study10.1186/s40510-019-0269-x ↗
42. Potential countersample materials for in vitro simulation wear testing10.1016/S0109-5641(01)00043-4 ↗
43. Three generations of zirconia: from veneered to monolithic. Part I
44. Three generations of zirconia: from veneered to monolithic. Part II
45. Two-body wear of monolithic, veneered and glazed zirconia and their corresponding enamel antagonists10.3109/00016357.2011.654248 ↗
46. In vitro evaluation of a mechanical testing chewing simulator10.1016/j.dental.2008.09.010 ↗
47. Load-bearing capacity and the recommended thickness of dental monolithic zirconia single crowns10.1016/j.jmbbm.2014.03.014 ↗
48. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
49. Influence of different surface treatments on two-body wear and fracture load of monolithic CAD/CAM ceramics10.1007/s00784-019-03173-8 ↗
50. Surface roughness of enamel and root surface after scaling, root planning and polishing procedures: an in-vitro study10.1016/j.jobcr.2021.02.013 ↗
51. Clinical esthetic comparison between monolithic high-translucency multilayer zirconia and traditional veneered zirconia for single implant restoration in maxillary esthetic areas: prosthetic and patient-centered outcomes10.1016/j.jds.2022.01.012 ↗
52. Novel zirconia materials in dentistry10.1177/0022034517737483 ↗