Micromechanical characteristics of titanium alloy (Ti-6Al-4V) made by laser powder bed fusion using an in-situ SEM micropillar compression technique
Source abstract
Abstract
While titanium alloy (Ti-6Al-4V) made by laser powder bed fusion (L-PBF) exhibits complex deformation behaviors, its important micromechanical properties in relation to loading directions are not fully understood. This research aims to investigate the micromechanical behaviors of printed L-PBF Ti-6Al-4V alloys under vertical (i.e., the loading direction perpendicular to printed layers) and horizontal (i.e., the loading direction parallel to printed layers) compressions using in-situ scanning electron microscopy (SEM) micropillar techniques. Ti-6Al-4V alloys were L-PBF-printed using a 45° rotate scanning strategy with vertical and horizontal build directions. The microstructures of the two alloys were analyzed using the SEM with energy-dispersive X-ray spectroscopy (EDS). The titanium alloy micropillars were produced using focused ion beam (FIB) milling in the SEM. In-situ SEM micropillar compressions were conducted using a flat diamond indenter. Vertical alloy had smaller cross-patterned finer α' martensite than horizontal one. While both vertical and horizontal micropillars showed elastic-plastic behaviors, the former had significantly higher yield, fracture, and compression strength values, as well as resilience and toughness, than the latter, leading to the formation of favorable shear bands. Both micropillars exhibited ductile fractures but had distinct failure mechanisms. The ductile fracture in the vertical micropillars was due to strain hardening, large plastic deformation, and shear band formation, while the ductile fracture in the horizontal ones was attributed to compression-induced bending and plastic buckling. The micromechanical characteristics of L-PBF Ti-6Al-4V materials provides an important insight into the small-scale deformation and failure mechanisms of the alloys influenced by loading directions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. A review of the as-built SLM Ti-6Al-4V mechanical properties towards achieving fatigue resistant designs10.3390/met8010075 ↗
2. Buckling phenomena in AM lattice strut elements: a design tool applied to Ti6Al4V LBPBF10.1016/j.matdes.2021.109892 ↗
3. Effective post processing of SLM fabricated Ti-6Al-4 V alloy: machining vs thermal treatment10.1016/j.jmapro.2021.06.035 ↗
4. Experimental realisation of build orientation effects on the mechanical properties of truly as-built Ti-6Al-4V SLM parts10.1016/j.jmapro.2021.01.027 ↗
5. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
6. Deformation and strengthening of SiC reinforced Al-MMCs during in-situ micro-pillar compression10.1016/j.msea.2019.138141 ↗
7. Multi-perspective analysis of building orientation effects on microstructure, mechanical and surface properties of SLM Ti6Al4V with specific geometry10.3390/ma14164392 ↗
8. Size and plasticity effects in zirconia micropillars compression10.1016/j.actamat.2015.10.047 ↗
9. Laser powder bed fusion: a state-of-the-art review of the technology, materials, properties & defects, and numerical modelling10.1016/j.jmrt.2022.07.121 ↗
10. Overview on micro- and nanomechanical testing: new insights in interface plasticity and fracture at small length scales10.1016/j.actamat.2017.06.019 ↗
11. Investigation on Ti-6Al-4V microstructure evolution in selective laser melting10.3390/met9121270 ↗
12. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
13. Microstructure and mechanical properties of Ti-6Al-4V manufactured by selective laser melting after stress relieving, hot isostatic pressing treatment, and post-heat treatment10.1007/s11665-021-05753-w ↗
14. Microstructural characterization and mechanical properties of SLM-printed Ti–6Al–4V alloy: effect of build orientation10.1557/s43578-021-00468-z ↗
15. Ductility of a Ti‐6Al‐4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
16. Plasticity in small-sized metallic systems: intrinsic versus extrinsic size effect10.1016/j.pmatsci.2011.01.005 ↗
17. Failure modes in dual layer thickness Laser Powder Bed Fusion components using a novel post-mortem reconstruction technique
18. Biomedical applications of the powder-based 3D printed titanium alloys: a review10.1016/j.jmst.2021.11.084 ↗
19. Microstructural examination and corrosion behavior of selective laser melted and conventionally manufactured Ti6Al4V for dental applications10.1016/j.msec.2020.110980 ↗
20. Microstructural characteristic and mechanical property of Ti6Al4V alloy fabricated by selective laser melting10.1016/j.vacuum.2018.01.026 ↗
21. Analysis of fracture toughness and crack propagation of Ti6Al4V produced by selective laser melting10.1002/adem.201100233 ↗
22. Size scaling in bi-crystalline Cu micropillars containing a coherent twin boundary10.1016/j.actamat.2022.117841 ↗
23. Differences in deformation behavior of bicrystalline Cu micropillars containing a twin boundary or a large-angle grain boundary10.1016/j.actamat.2014.04.022 ↗
24. Scanning strategy in selective laser melting (SLM): a review10.1007/s00170-021-06810-3 ↗
25. Failure mechanisms in in-situ SEM micropillar compressions of pre-crystallized and crystallized zirconia-containing lithium silicate glass-ceramics10.1016/j.ceramint.2023.05.261 ↗
26. In-situ SEM micropillar compression of porous and dense zirconia materials10.1016/j.jmbbm.2022.105268 ↗
27. X-ray micro-computed tomography of porosities in large-volume 3D-printed Ti–6Al–4V components using laser powder-bed fusion and their tensile properties10.1016/j.jmrt.2024.07.029 ↗
28. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
29. Superior plasticity stability and excellent strength in Ti-55531 alloy micropillars via harmony slip in nanoscale α/β phases10.1038/s41598-019-41574-7 ↗
30. Micro-mechanical behaviour of selective laser melted Ti6Al4V under compression10.1016/j.msea.2021.141975 ↗
31. Effect of laser spot size, scanning strategy, scanning speed, and laser power on microstructure and mechanical behavior of 316L stainless steel fabricated via selective laser melting
32. Thermomechanical response of 3D laser-deposited Ti–6Al–4V alloy over a wide range of strain rates and temperatures10.1016/j.msea.2015.08.043 ↗
33. Influence of stacking fault energy and dislocation character on slip transfer at coherent twin boundaries studied by micropillar compression10.1016/j.actamat.2018.05.037 ↗
34. Nano-mechanical behavior of Ti6Al4V alloy manufactured using laser powder bed fusion10.3390/ma16124341 ↗
35. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
36. Synchrotron X-ray diffraction study of the phase transformations in titanium alloys10.1016/S1044-5803(02)00286-3 ↗
37. Microstructure-properties relationships of Ti-6Al-4V parts fabricated by selective laser melting10.1007/s40684-018-0062-1 ↗
38. Size-induced twinning in InSb semiconductor during room temperature deformation10.1038/s41598-021-98492-w ↗
39. Deformation and failure mechanisms of Ti–6Al–4V as built by selective laser melting10.1016/j.msea.2019.138456 ↗
40. Microstructure and mechanical behavior of Ti–6Al–4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
41. A critical review on additive manufacturing of Ti-6Al-4V alloy: microstructure and mechanical properties10.1016/j.jmrt.2022.04.055 ↗
42. Recent research and development in titanium alloys for biomedical applications and healthcare goods10.1016/j.stam.2003.09.002 ↗
43. Micromechanical characterization of additively manufactured Ti-6Al-4V parts produced by electron beam melting
44. Computational assessment of thermokinetics and associated microstructural evolution in laser powder bed fusion manufacturing of Ti6Al4V alloy10.1038/s41598-020-63281-4 ↗
45. Design and 3D-printing of titanium bone implants: brief review of approach and clinical cases10.1007/s13534-018-0080-5 ↗
46. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
47. Globularization using heat treatment in additively manufactured Ti-6Al-4V for high strength and toughness10.1016/j.actamat.2018.09.064 ↗
48. In situ micropillar compression reveals superior strength and ductility but an absence of damage in lamellar bone10.1038/nmat3959 ↗
49. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
50. The relation between load and penetration in the axisymmetric boussinesq problem for a punch of arbitrary profile
51. Effect of misorientation on the compression of highly anisotropic single-crystal micropillars10.1002/adem.201200019 ↗
52. Effects of processing parameters on microstructure and mechanical property of selective laser melted Ti6Al4V10.1016/j.matdes.2011.09.051 ↗
53. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
54. A methodology to investigate size scale effects in crystalline plasticity using uniaxial compression testing10.1016/j.msea.2005.03.082 ↗
55. Sample dimensions influence strength and crystal plasticity10.1126/science.1098993 ↗
56. Defects-dictated tensile properties of selective laser melted Ti-6Al-4V10.1016/j.matdes.2018.08.004 ↗
57. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
58. Investigation of precipitate hardening of slip and twinning in Mg5%Zn by micropillar compression10.1016/j.actamat.2015.08.012 ↗
59. EBSD study of beam speed effects on Ti-6Al-4V alloy by powder bed electron beam additive manufacturing10.1016/j.jallcom.2018.03.173 ↗
60. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
61. Effect of hot isostatic pressing (HIP) treatment on the compressive properties of Ti6Al4V lattice structure fabricated by selective laser melting10.1016/j.matlet.2019.126537 ↗
62. An investigation of ductile fracture behavior of Ti6Al4V alloy fabricated by selective laser melting10.1016/j.jallcom.2021.161926 ↗
63. In situ micropillar compression of an anisotropic metal-organic framework single crystal10.1038/s42004-023-00858-w ↗
64. Plate-like precipitate effects on plasticity of Al-Cu micro-pillar: {100}-interfacial slip10.1016/j.mtla.2019.100416 ↗
65. Difference in compressive and tensile fracture mechanisms of Zr59Cu20Al10Ni8Ti3 bulk metallic glass10.1016/S1359-6454(02)00521-9 ↗
66. In situ measurements of a homogeneous to heterogeneous transition in the plastic response of ion-irradiated ⟨1 1 1⟩ Ni microspecimens10.1016/j.actamat.2015.01.007 ↗