The fracture resistance (R-curve behaviour) of two commercial dental composites (Filtek Z350(®) and Concept Advanced(®)) were studied using Double Cantilever Beam sandwich specimens loaded with pure bending moments to obtain stable crack growth. The experiments were conducted in an environmental scanning electron microscope to (a) accurately measure the applied energy-release rate for crack initiation, (b) measure the early (rising) part of the R-curve, and (c) provide direct microscopic evidence of the toughening mechanisms ahead of and/or in the wake of the crack tip. The two tested composites displayed distinctly different R-curve behaviours. The difference was related to different toughening mechanisms as the two composites had markedly different microstructures. Contrary to common experience, the composite with the finer microstructure (smaller particles), the Concept Advanced(®), showed significantly higher fracture resistance than the composite with the coarser microstructure. The fracture properties were related to the flexural strength of the dental composites. The method, thus, can provide useful insight into how the microstructure enhances toughness, which is necessary for the future development of such materials.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Injection Molding Process and Properties · Engineering Technology and Methodologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. The role of material orthotropy in fracture specimens for composites10.1016/0020-7683(92)90138-J ↗
2. Remarks on crack-bridging concepts10.1115/1.3119764 ↗
3. Microstructural design of silicon nitride with improved fracture toughness: I, Effects of grain shape and size10.1111/j.1151-2916.1998.tb02702.x ↗
4. Characterization of nanofilled compared to universal and microfilled composites10.1016/j.dental.2005.12.003 ↗
5. Fracture toughness of nine flowable resin composites10.1067/mpr.2003.33 ↗
6. Broek · 1986
7. Strength characteristics of transformation-toughened zirconia10.1016/0020-7683(83)90031-8 ↗
8. On the analysis of mixed-mode failure10.1007/BF00035361 ↗
9. Remaining challenges with Class II resin-based composite restorations10.14219/jada.archive.2007.0085 ↗
10. An investigation into the fracture-behavior of a particulate-filled Bis-GMA resin10.1177/00220345870660060701 ↗
11. Crack deflection processes. 1. Theory10.1016/0001-6160(83)90046-9 ↗
12. Crack deflection processes. 2. Experiment10.1016/0001-6160(83)90047-0 ↗
13. A micromechanical basis for partitioning the evolution of grain bridging in brittle materials10.1016/j.jmps.2006.10.009 ↗
14. Transformation toughening in ZrO2- containing ceramics10.1111/j.1151-2916.1987.tb04865.x ↗
15. Resistance curve behavior of supertough MgO-partially-stabilized ZrO2∗10.1016/0025-5416(88)90483-1 ↗
16. Trends in materials science from the point of view of a practicing dentist10.1016/j.jeurceramsoc.2008.08.014 ↗
17. Clinical results and new developments of direct posterior restorations
18. Crack tip shielding by micro-cracking in brittle solids10.1016/0001-6160(87)90108-8 ↗
19. Effect of side grooves on the elastic–plastic stress state of fracture toughness specimens — three dimensional finite element analysis10.1016/0013-7944(82)90019-4 ↗
20. Fracture toughness of water-aged resin composite restorative materials10.1016/0109-5641(95)80019-0 ↗
21. Influence of toughness on Weibull modulus of ceramic bending strength10.1557/JMR.1986.0120 ↗
22. Microfracture mechanisms of dental resin composites containing spherically-shaped filler particles10.1177/00220345940730020301 ↗
23. Mechanical-properties of Bis-GMA resin short glass-fiber composites10.1002/jbm.820231008 ↗
24. Fracture resistance and stable crack-growth behavior of 8-mol%-ytria-stabilised zirconia10.1111/j.1151-2916.2000.tb01354.x ↗
25. On the fracture toughness of advanced materials10.1002/adma.200803322 ↗
26. Strength and fatigue performance versus filler fraction of different types of direct dental restoratives10.1002/jbm.b.30338 ↗
27. Review of the clinical survival of direct and indirect restorations in posterior teeth of the permanent dentition
28. Mechanical properties of new composite restorative materials10.1002/1097-4636(2000)53:4<353::AID-JBM9>3.0.CO;2-B ↗
29. Effect of liquid rubber additions on physical properties of Bis-GMA based dental resins10.1016/j.dental.2009.09.010 ↗
30. Strength characteristics of transformation-toughened zirconia10.1111/j.1151-2916.1986.tb07402.x ↗
31. Influence of artificial saliva on abrasive wear and microhardness of dental composites filled with nanoparticles10.1016/j.jdent.2008.05.001 ↗
32. Mechanics and mechanisms of toughening of advanced ceramics10.1016/0924-0136(95)01909-X ↗
33. Effects of resin formulation and nanofiller surface treatment on the properties of experimental hybrid resin composite10.1016/j.biomaterials.2003.11.003 ↗
34. Effect of notch root radius on the fracture toughness of a fine-grained alumina10.1111/j.1151-2916.1994.tb07038.x ↗
35. The influence of short and medium-term water immersion on the hydrolytic stability of novel low-shrink dental composites10.1016/j.dental.2005.01.004 ↗
36. A path independent integral and the approximate analysis of strain concentrations by notches and cracks10.1115/1.3601206 ↗
37. Microstructural characterization and fracture behavior of a microhybrid and a nanofill composite10.1016/j.dental.2008.02.006 ↗
38. The problems associated with substituting composite resins for amalgam: a status report on posterior composites10.1016/0300-5712(88)90001-2 ↗
39. Effects of polymerization contraction in composite restorations10.1016/0300-5712(92)90133-W ↗
40. R-curve behavior and micromechanisms of fracture in resin based dental restorative composites10.1016/j.jmbbm.2008.12.005 ↗
41. R-curve behavior and toughening mechanisms of resin-based dental composites: Effects of hydration and post-cure heat treatment10.1016/j.dental.2008.12.004 ↗
42. Controlled crack growth in ceramics: the DCB specimen loaded with pure moments10.1016/0955-2219(96)00021-0 ↗
43. Fracture resistance measurement method for in situ observation of crack mechanisms10.1111/j.1151-2916.1998.tb02387.x ↗
44. Delamination R-curve phenomena due to damage10.1016/0022-5096(92)90198-B ↗
45. R-curve behavior in a polycrystalline alumina material10.1007/BF01729403 ↗
46. Direct resin composite inlays/onlays: an 11 year follow-up10.1016/S0300-5712(00)00010-5 ↗
47. An analysis of the crack tip stress field in DCB adhesive fracture specimens10.1007/BF00032383 ↗
48. Fracture toughness comparison of six resin composites10.1016/j.dental.2007.06.018 ↗
49. Ceramic whisker reinforcement of dental resin composites10.1177/00220345990780021101 ↗
50. Effects of different whiskers on the reinforcement of dental resin composites10.1016/S0109-5641(02)00078-7 ↗
51. Fracture studies of selected dental restorative composites10.1016/S0109-5641(97)80027-9 ↗