Fabrication, tribological and corrosion behaviors of ultra-fine grained Co–28Cr–6Mo alloy for biomedical applications
Source abstract
Abstract
Nickel and carbides free Co-28Cr-6Mo alloy was fabricated by combination of mechanical alloying and warm pressing. The microstructure, mechanical properties, pin-on-disk dry sliding wear and corrosion behavior in simulated physiological solution were investigated. The produced Co-28Cr-6Mo alloy has elongated ultra-fine grained (UFG) structure of ε-phase with average grain size of 600nm in length and 150nm in thickness. The hardness and modulus were determined to be 8.87±0.56GPa and 198.27±7.02GPa, respectively. The coefficient of friction upon dry sliding against alumina is pretty close to that of the forged Co-29Cr-6Mo alloy. The initial ε-phase and UFG microstructure contribute to reduce the depth of severe plastic deformation region during wear and enable the alloy with excellent wear resistance. The corrosion potential of such UFG Co-Cr-Mo alloy has more positive corrosion potential and much lower corrosion current density than those of ASTM alloy.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Corrosion resistance of ultra fine-grained Ti10.1016/j.scriptamat.2004.04.011 ↗
2. High strength Co–Cr–Mo alloy by hot isostatic pressing of powder10.3109/10731197909119373 ↗
3. Joint contact stress: a reasonable surrogate for biological processes?
4. On carbide dissolution in an as-cast ASTM F-75 alloy10.1002/jbm.10001 ↗
5. Effects of plasma nitriding on mechanical and tribological properties of CoCrMo alloy10.1016/j.surfcoat.2007.08.030 ↗
6. Effects of microstructures on the sliding behavior of hot-pressed CoCrMo alloys10.1016/j.wear.2014.07.022 ↗
7. Effects of sigma phase and carbide on the wear behavior of CoCrMo alloys in Hanks׳ solution10.1016/j.wear.2013.12.010 ↗
8. Pin-on-disk wear behavior in a like-on-like configuration in a biological environment of high carbon cast and low carbon forged Co–29Cr–6Mo alloys10.1016/j.actamat.2006.10.005 ↗
9. Mechanical properties of forged low Ni and C-containing Co–Cr–Mo biomedical implant alloy10.4028/www.scientific.net/MSF.475-479.2317 ↗
10. Microstructure and mechanical properties of biomedical Co–29Cr–8Mo alloy wire fabricated by a modified melt-spinning process10.1016/j.actamat.2006.10.060 ↗
11. Solution treatment behavior of Co–Cr–Mo alloy10.1002/jbm.820130208 ↗
12. Cast vs. wrought cobalt–chromium surgical implant alloys10.1002/jbm.820090205 ↗
13. Mechanical properties of metals for biomedical applications using powder metallurgy process: a review10.1007/BF03027531 ↗
14. Microstructure, hardness, corrosion resistance and porcelain shear bond strength comparison between cast and hot pressed CoCrMo alloy for metal–ceramic dental restorations10.1016/j.jmbbm.2012.03.015 ↗
15. Microstructure and corrosion behaviour in biological environments of the new forged low-Ni Co–Cr–Mo alloys10.1016/j.biomaterials.2005.01.028 ↗
16. Grain boundary diffusion characteristics of nanostructured nickel10.1016/S1359-6462(00)00699-0 ↗
17. Corrosion testing of sintered samples made of the Co–Cr–Mo alloy for surgical applications
18. Dry friction and wear behavior of forged Co–29Cr–6Mo alloy without Ni and C additions for implant applications10.2320/matertrans.46.1578 ↗
19. Grain refinement of biomedical Co–27Cr–5Mo–0.16N alloy by reverse transformation10.1016/j.matlet.2009.10.001 ↗
20. Martensitic transformation in a cast Co–Cr–Mo–C alloy10.1007/s11661-007-9370-8 ↗
21. New insights into hard phases of CoCrMo metal-on-metal hip replacements10.1016/j.jmbbm.2012.03.013 ↗
22. The composition of the surface passive film formed on CoCrMo alloy in simulated physiological solution10.1016/S0013-4686(03)00396-7 ↗
23. Corrosion and fretting corrosion studies of medical grade CoCrMo alloy in a clinically relevant simulated body fluid environment10.1007/s11661-015-2834-3 ↗
24. A novel route for processing cobalt–chromium–molybdenum orthopaedic alloys10.1098/rsif.2010.0036 ↗
25. Influence of microstructural modifications induced by ultrasonic impact treatment on hardening and corrosion behavior of wrought Co–Cr–Mo biomedical alloy10.1016/j.msec.2015.09.004 ↗
26. Cooling rate and carbon content effect on the fraction of secondary phases precipitate in as-cast microstructure of ASTM F75 alloy10.1016/j.jmatprotec.2008.04.039 ↗
27. Resistance of nanocrystalline vis-à-vis microcrystalline Fe–Cr alloys to environmental degradation and challenges to their synthesis10.1080/14786435.2010.484402 ↗
28. Sliding wear-induced chemical nanolayering in Cu–Ag, and its implications for high wear resistance10.1016/j.actamat.2014.03.060 ↗
29. Effects of strain energy and grain size on corrosion resistance of ultrafine grained Fe-20% Cr steels with extremely low C and N fabricated by ECAP10.1155/2015/386865 ↗
30. Powder metallurgical processing of Co–28%Cr–6%Mo for dental implants: physical, mechanical and electrochemical properties10.1016/j.powtec.2010.09.024 ↗
31. Mechanical alloying of biocompatible Co–28Cr–6Mo alloy
32. Microstructure and tensile properties of hot-pressed Co–Cr–Mo alloy compacts for biomedical applications10.2320/jinstmet.72.532 ↗
33. Ion release in stable hip arthroplasties using metal-on-metal articulating surfaces: a comparison between short- and medium-term results10.1002/jbm.a.10595 ↗
34. The safety of nickel containing dental alloys10.1016/j.dental.2005.11.033 ↗
35. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
36. Quantitative analysis of the wear and wear debris from low and high carbon content cobalt chrome alloys used in metal on metal total hip replacements
37. Electrochemical characterisation of biomedical alloys for surgical implants in simulated body fluids10.1016/j.corsci.2008.04.002 ↗
38. Effect of microstructure on the dry sliding friction behavior of CoCrMo alloys used in metal-on-metal hip implants10.1002/jbm.b.30370 ↗
39. Effect of thermal treatment and applied potential on the electrochemical behaviour of CoCrMo biomedical alloy10.1016/j.electacta.2008.10.018 ↗
40. The acting wear mechanisms on metal-on-metal hip joint bearings: in vitro results10.1016/S0043-1648(01)00654-8 ↗
41. Influence of carbon addition on mechanical properties and microstructures of Ni-free Co–Cr–W alloys subjected to thermomechanical processing10.1016/j.jmbbm.2014.05.025 ↗