journal article·2013-11

In vitro load-induced dentin collagen-stabilization against MMPs degradation

Manuel Toledano, Fátima S. Aguilera, Monica Yamauti, María Estrella Ruiz-Requena, Raquel Osorio

Publisher page

Abstract

Introduction Teeth are continuously subjected to stresses during mastication, swallowing and parafunctional habits, producing a significant reduction of the bonding efficacy in adhesive restorations. The purpose of this study was to evaluate the metalloproteinases (MMPs)-mediated dentin collagen degradation of hybrid layers created by using different demineralization processes, previous resin infiltration, and in vitro mechanical loading. Methods Human dentin beams (0.75×0.75×5.0mm) were subjected to different treatments: (1) untreated dentin; (2) demineralization by 37% phosphoric acid (PA) or by 0.5% M ethylenediaminetetraacetic acid (EDTA); (3) demineralization by PA, followed by application of Adper(™) Single Bond (SB); (4) demineralization by EDTA, followed by application of SB. In half of the specimens, mechanical loadings (100,000 cycles, 2Hz, 49N) were applied to dentin beams. Specimens were stored in artificial saliva. C-terminal telopeptide (ICTP), determinations (which indicates the amount of collagen degradation) (radioimmunoassay) were performed after 24h, 1 week and 4 weeks. Results Load cycling decreased collagen degradation when dentin was untreated or PA-demineralized and EDTA-treated. ICTP values increased when both PA-demineralized and EDTA-treated and infiltrated with SB dentin beams were loaded, except in samples that were subjected to EDTA treatment and SB infiltration after 4w of storage, which showed similar values of collagenolytic activity than the non loaded specimens. Load cycling preserved the initial (24h) ICTP determination at any time point, in all groups of the study, except in PA-demineralized and SB infiltrated dentin which showed an increased of collagen degradation values, over time. This same trend was observed in all groups without loading. Interpretation Mechanical loading enhances collagen's resistance to enzymatic degradation in natural and demineralized dentin. Mild acids (EDTA) lead to a lower volume of demineralized/unprotected collagen to be cleaved by MMPs. Load cycling produced an increase of collagen degradation when PA-demineralized dentin and EDTA-treated dentin were infiltrated with resin, but EDTA-treated dentin showed a constant collagenolytic degradation, over time.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Health and Care Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Heat-induced changes in porcine annulus fibrosus biomechanics10.1016/j.jbiomech.2003.07.002 ↗
2. Evaluation of surface structural and mechanical changes following remineralization of dentin10.1002/sca.20199 ↗
3. Effect of cyclic loading under enzymatic activity on resin–dentin interfaces of two self-etching adhesives10.1016/j.dental.2007.03.008 ↗
4. Chlorhexidine stabilizes the adhesive interface: a 2-year in vitro study10.1016/j.dental.2009.11.153 ↗
5. Strain-derived canalicular fluid flow regulates osteoclast activity in a remodelling osteon--a proposal10.1016/S0021-9290(03)00126-X ↗
6. 2-hydroxyethyl methacrylate as an inhibitor of matrix metalloproteinase-210.1111/j.1600-0722.2008.00591.x ↗
7. Tissue growth and remodeling10.1146/annurev.bioeng.6.040803.140250 ↗
8. Four-year water degradation of total-etch adhesives bonded to dentin10.1177/154405910308200212 ↗
9. Inhibition of enzymatic degradation of adhesive–dentin interfaces10.1177/0022034509346952 ↗
10. Primary structure and phosphorylation of dentin matrix protein 1 (DMP1) and dentin phosphophoryn (DPP) uniquely determine their role in biomineralization10.1021/bm2005214 ↗
11. Modifications of the organic and mineral fractions of dental tissues following conditioning by self-etching adhesives10.1016/j.jdent.2010.11.004 ↗
12. Osteocytes and WNT: the mechanical control of bone formation10.1177/0022034510363963 ↗
13. The type I collagen fragments ICTP and CTX reveal distinct enzymatic pathways of bone collagen degradation10.1359/jbmr.2003.18.5.859 ↗
14. Changes in stiffness of resin-infiltrated demineralized dentin after remineralization by a bottom-up biomimetic approach10.1016/j.actbio.2009.10.052 ↗
15. In situ atomic force microscopy of partially demineralized human dentin collagen fibrils10.1016/S1047-8477(02)00029-1 ↗
16. Physiologic root resorption in primary teeth: molecular and histological events10.2334/josnusd.49.1 ↗
17. Imperfect hybrid layers created by an aggressive one-step self-etch adhesive in primary dentin are amendable to biomimetic remineralization in vitro10.1002/jbm.a.32612 ↗
18. Functional proteomics on zinc-dependent metalloproteinases using inhibitor probes10.1002/cmdc.200800284 ↗
19. In vivo degradation of resin–dentin bonds produced by a self-etch vs. a total-etch adhesive system10.1111/j.1600-0722.2004.00141.x ↗
20. Hydroxyapatite induces autolytic degradation and inactivation of matrix metalloproteinase-1 and -310.1359/jbmr.1998.13.12.1890 ↗
21. Pre-odontoblasts, odontoblasts, or odontocytes10.1177/154405910808700310 ↗
22. Human treated dentin matrix as a natural scaffold for complete human dentin tissue regeneration10.1016/j.biomaterials.2011.03.008 ↗
23. Neurotoxicity of dental amalgam is mediated by zinc10.1177/154405910308200318 ↗
24. Intermittent compressive load stimulates osteogenesis and improves osteocyte viability in bones cultured in vitro10.1007/BF02238545 ↗
25. Differential effect of calcium phosphate and calcium pyrophosphate on binding of matrix metalloproteinases to fibrin: comparison to a fibrin-binding protease from inflammatory joint fluids10.1111/j.1365-2249.2004.02413.x ↗
26. Sodium hypochlorite alterations of dentin and dentin collagen10.1016/S0039-6028(01)01310-3 ↗
27. Polymer-in-a-box mechanism for the thermal stabilization of collagen molecules in fibers10.1016/S0006-3495(99)77476-X ↗
28. Uniaxial tension inhibits tendon collagen degradation by collagenase in vitro10.1002/jor.1100140120 ↗
29. Nicholson · 2002 · 92
30. The in vitro dentin bond strengths of two adhesive systems in class I cavities of human molars
31. Effect of sodium hypochlorite on dentin bonding with a polyalkenoic acid-containing adhesive system10.1002/jbm.10074 ↗
32. Effect of load cycling and in vitro degradation on resin–dentin bonds using a self-etching primer10.1002/jbm.a.30274 ↗
33. EDTA treatment improves resin–dentin bonds' resistance to degradation10.1177/154405910508400810 ↗
34. Zinc reduces collagen degradation in demineralized human dentin explants10.1016/j.jdent.2010.11.005 ↗
35. Effect of dentin etching and chlorhexidine application on metalloproteinase-mediated collagen degradation10.1111/j.1600-0722.2010.00789.x ↗
36. Interaction of conditioners on the dentin surface
37. Effects of water and water-free polar solvents on the tensile properties of demineralized dentin10.1016/S0109-5641(02)00065-9 ↗
38. Novel selective MMP-13 inhibitors reduce collagen degradation in bovine articular and human osteoarthritis cartilage explants10.1007/s00011-009-0112-9 ↗
39. Model of aluminum-induced osteomalacia: inhibition of apatite formation and growth
40. Cartilage oligomeric matrix protein shows high affinity zinc-dependent interaction with triple helical collagen10.1074/jbc.273.32.20397 ↗
41. Strain-controlled enzymatic cleavage of collagen in loaded matrix10.1016/j.bbrc.2005.08.128 ↗
42. Resin-dentin bonds to EDTA-treated vs. acid-etched dentin using ethanol wet-bonding10.1016/j.dental.2009.12.008 ↗
43. Dentine as a bioactive extracellular matrix10.1016/j.archoralbio.2011.07.008 ↗
44. Molecular structure of acid-etched dentin smear layers: in situ study10.1177/00220345010800090601 ↗
45. Adhesive/dentin interface: the weak link in the composite restoration10.1007/s10439-010-9969-6 ↗
46. Properties of dissociatively extracted fetal tooth matrix proteins. II. Separation and purification of fetal bovine dentin phosphoprotein10.1016/S0021-9258(18)43459-X ↗
47. The activation and function of host matrix metalloproteinases in dentin matrix breakdown in caries lesions10.1177/00220345980770081001 ↗
48. Effect of cyclic loading on the microtensile bond strengths of total-etch and self-etch adhesives10.2341/04-161 ↗
49. Zinc-inhibited MMP-mediated collagen degradation after different dentine demineralization procedures10.1159/000337315 ↗
50. Surface analysis of conditioned dentin and resin-dentin bond strength10.1163/016942411X559067 ↗
51. A Zn-doped etch-and-rinse adhesive may improve the mechanical properties and the integrity at the bonded-dentin interface10.1016/j.dental.2013.04.024 ↗
52. Sclerostin in mineralized matrices and van Buchem disease10.1177/0022034509338340 ↗
53. Increased proteolysis of collagen in an in vitro tensile overload tendon model10.1007/s10439-007-9375-x ↗
54. Cyclic tensile strain and cyclic hydrostatic pressure differentially regulate expression of hypertrophic markers in primary chondrocytes10.1016/S8756-3282(03)00242-4 ↗