journal article·2013-02

Microstructure and mechanical properties of MgO-stabilized ZrO2–Al2O3 dental composites

C.B. Abi, O.F. Emrullahog˘lu, G. Said

Publisher page

Abstract

The aim of the present study was to investigate the production of tetragonal zirconia (t-ZrO(2)) particles (experimental t-ZrO(2)) from monoclinic zirconia (m-ZrO(2)) and to evaluate the effect of the t-ZrO(2) content on the fracture toughness of alumina-zirconia composites by conducting ASTM E399 standard test. In the laboratory study, t-ZrO(2) powder was produced by heat treating m-ZrO(2) containing 10wt.% MgO. Alumina and alumina-zirconia composite powders containing various types and amounts of m-ZrO(2) and t-ZrO(2) were prepared (0-20 wt.%), shaped by slip casting to achieve a uniform distribution and homogeneous microstructure in accordance with the dimensions of ASTM E399 standards, dried, sintered at three different temperatures: 1400, 1500 and 1600 °C for two hours, and characterized. The results of the XRD analysis showed that t-ZrO(2) was produced at 1400 °C. In t-ZrO(2)-doped alumina composites, t-ZrO(2) partially transformed to m-ZrO(2) after sintering, whereas commercial t-ZrO(2) (Tosoh TZ-3Y) remained intact. SEM studies on samples sintered at 1600 °C revealed that the addition of zirconia inhibited abnormal grain growth of alumina, leading to a homogeneous and equiaxed grain structure, especially at high concentrations of zirconia. ZrO(2)-doping enhanced the fracture toughness of the composites, which increased with an increase in the t-ZrO(2) content. The maximum fracture toughness was 11.5 MPam(1/2) and was observed when the t-ZrO(2) content was equal to 20 wt.%. Alternatively, the maximum fracture toughness for pure alumina was 5.9 MPam(1/2).
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Materials handbook
2. ASTM-E-399-90, 1990. Standard test method for plane-strain fracture toughness of metallic materials. Annual Book of ASTM Standards 03.01, pp. 509–539.
3. Fundamentals of ceramics
4. Barsoum · 2003
5. Fracture toughness of Al2O3 with an unstabilized ZrO2 dispersed phase10.1111/j.1151-2916.1976.tb09386.x ↗
6. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
7. Fischer-Cripps · 2007
8. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
9. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
10. Microstructure of alumina- and alumina/zirconia-glass infiltrated dental ceramics
11. Strength, reliability and mode of fracture of bilayered porcelain/zirconia (Y-TZP) dental ceramics10.1016/j.biomaterials.2004.02.036 ↗
12. Transformation toughening: an overview10.1111/j.1151-2916.1986.tb07400.x ↗
13. Ipek, M., 2005. Investigation of Sintering and Fracture Behaviour of Alumina–Zirconia Composites Produced with Two Different Routes. Ph.D. Thesis. Sakarya University, Institute of Science and Technology.
14. An evaluation of Al2O3–ZrO2 composites produced by coprecipitation method10.1016/j.jallcom.2010.09.073 ↗
15. Effect of a small amount of liquid-forming additives on the microstructure of Al2O3 ceramics10.1007/BF00365207 ↗
16. Indentation techniques for evaluating the fracture toughness of biomaterials and hard tissues10.1016/j.jmbbm.2008.10.008 ↗
17. Kübler, J., 1997. Fracture toughness of ceramics using the SEVNB method: preliminary results. In: J.P. Singh (Ed.) Ceramic Engineering and Science Proceedings, vol. 18 (4). Published by the American Ceramic Society, Westerville, OH, pp. 155–162.10.1002/9780470294444.ch18 ↗
18. Transformation toughening: part 4 fabrication, fracture toughness and strength of Al2O3–ZrO2 composites10.1007/BF00809060 ↗
19. Y-TZP ceramic processing from coprecipitated powders: a comparative study with three commercial dental ceramics10.1016/j.dental.2008.04.002 ↗
20. Lee · 1994
21. Effect of sintering on structure and mechanical properties of alumina–15vol% zirconia nanocomposite compacts10.1016/j.jallcom.2009.12.166 ↗
22. Effect of notchroot radius on the fracture toughness of a fine grained alumina10.1111/j.1151-2916.1994.tb07038.x ↗
23. Sintering, microstructure and mechanical properties of Al2O3–Y2O3–ZrO2 (AYZ) eutectic composition ceramic microcomposites10.1016/j.jeurceramsoc.2009.09.011 ↗
24. On the Vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
25. Properties of zirconia-toughened-alumina prepared via powder processing and colloidal processing routes10.1016/j.jcis.2008.10.010 ↗
26. Contemporary materials and technologies for all-ceramic fixed partial dentures: a review of the literature10.1016/j.prosdent.2004.09.015 ↗
27. Refractory ceramics: I. The forms of zirconium dioxide10.1002/zaac.19291800104 ↗
28. Preparation and characterization of an Al2O3–ZrO2 nanocomposite. Part I. Powder synthesis and transformation behavior during fracture10.1016/j.compositesa.2006.01.005 ↗
29. Alumina nanocomposites from powder alkoxide mixtures10.1016/S1359-6454(01)00413-X ↗
30. Stevens · 1986
31. Strength limitations of transformation-toughened zirconia alloys10.1111/j.1151-2916.1986.tb04785.x ↗
32. Wachtman · 1996
33. Formation of Al2O3 grains with different size and morphologies during the pulse electric current sintering process10.1557/JMR.2001.0482 ↗
34. Strength and fracture toughness of MgO-modified glass infiltrated alumina for CAD/CAM10.1016/S0109-5641(01)00026-4 ↗
35. Microstructure and mechanical properties of yttria-stabilized ZrO2/Al2O3 nanocomposite ceramics10.1016/j.ceramint.2007.06.005 ↗
36. From porcelain-fused-to-metal to zirconia: clinical and experimental considerations10.1016/j.dental.2010.10.024 ↗