journal article·2016-08

Biomechanical evaluation of laser-etched Ti implant surfaces vs. chemically modified SLA Ti implant surfaces: Removal torque and resonance frequency analysis in rabbit tibias

Jung-Tae Lee, Sung-Am Cho

Publisher page

Abstract

Purpose To compare osseointegration and implant stability of two types of laser-etched (LE) Ti implants with a chemically-modified, sandblasted, large-grit and acid-etched (SLA) Ti implant (SLActive(®), Straumann, Basel, Switzerland), by evaluating removal torque and resonance frequency between the implant surface and rabbit tibia bones. We used conventional LE Ti implants (conventional LE implant, CSM implant, Daegu, Korea) and LE Ti implants that had been chemically activated with 0.9% NaCl solution (LE active implant) for comparison with SLActive(®) implants Materials and methods Two types of 3.3×8mm laser-etched Ti implants - conventional LE implants and LE active implants were prepared. LE implants and SLActive(®) implants were installed on the left and right tibias of 10 adult rabbits weighing approximately 3.0kg LE active implants and SLActive(®) implants were installed on the left and right tibias of 11 adult rabbits. After installation, we measured insertion torque (ITQ) and resonance frequency (ISQ). Three weeks (LE active) or 4 weeks (conventional LE) after installation, we measured removal torque (RTQ) and ISQ. Results In the conventional LE experiment, the mean ITQ was 16.99±6.35Ncm for conventional LE implants and 16.11±7.36Ncm for SLActive(®) implants (p=0.778>0.05). After 4 weeks, the mean of RTQ was 39.49±17.3Ncm for LE and 42.27±20.5Ncm for SLActive(®) (p=0.747>0.05). Right after insertion of the implants, the mean ISQ was 74.8±4.98 for conventional LE and 70.1±9.15 for SLActive(®) implants (p=0.169>0.05). After 4 weeks, the mean ISQ was 64.40±6.95 for LE and 67.70±9.83 for SLActive(®) (p=0.397>0.05). In the LE active experiment, the mean ITQ was 16.24±7.49Ncm for LE active implants and 14.33±5.06Ncm for SLActive(®) implants (p=0.491>0.05). After 3 weeks, the mean RTQ was 39.25±16.41Ncm for LE active and 41.56±10.41Ncm for SLActive(®) implants (p=0.698>0.05). Right after insertion of the implants, the mean ISQ was 58.64±10.51 for LE active implants and 53.82±15.36 for SLActive(®) implants (p=0.401>0.05). After 3 weeks, the mean ISQ was 63.82±5.88 for LE active and 66.27±6.53 for SLActive(®) (p=0.365>0.05). Conclusion We observed no significant differences in biomechanical bond strength to bone or implant stability in bone between the conventional LE Ti implant surface and the surface of the SLActive(®) implant or between the chemically activated LE Ti implant surface and the surface of the SLActive(®) implant during the early stage of osseointegration.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Bone Tissue Engineering Materials · Dental Implant Techniques and Outcomes · Laser Applications in Dentistry and Medicine

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Enhanced bone apposition to a chemically modified sla titanium surface10.1177/154405910408300704 ↗
2. A removal torque of the laser-treated titanium implants in rabbit tibia10.1016/S0142-9612(03)00377-6 ↗
3. Surface configurations of dental implants10.1111/j.1600-0757.1998.tb00121.x ↗
4. Characterization and in vivo evaluation of calcium phosphate coated cp-titanium by dip-spin method10.1016/j.cap.2005.01.020 ↗
5. Evaluation of titanium implants with surface modification by laser beam: biomechanical study in rabbit tibias10.1590/S1806-83242009000200008 ↗
6. Biomechanical evaluation of the interfacial strength of a chemically modified sandblasted and acid-etched titanium surface10.1002/jbm.a.30678 ↗
7. Characterization and biocompatibility of a titanium dental implant with a laser irradiated and dual-acid etched surface
8. Early detection of implant healing process using resonance frequency analysis10.1034/j.1600-0501.2003.00818.x ↗
9. Influence of mono- and bicortical anchorage on the integration of titanium implants10.1016/S0901-5027(96)80036-1 ↗
10. Comparison of removal torques between laser-treated and SLA-treated implant surfaces in rabbit tibiae10.4047/jap.2014.6.4.302 ↗
11. Biomechanical evaluation of dental implants with different surfaces: removal torque and resonance frequency analysis in rabbits10.4047/jap.2009.1.2.107 ↗
12. Biomaterial and implant surfaces: On the role of cleanliness, contamination, and preparation procedures10.1002/jbm.820221307 ↗
13. Correlation between substratum roughness and wettability, cell adhesion, and cell migration10.1002/(SICI)1097-4636(199707)36:1<99::AID-JBM12>3.0.CO;2-E ↗
14. Surface characterization of variously treated titanium materials
15. Laser surface modification of Ti implants to improve osseointegration
16. The application of resonance frequency measurements to study the stability of titanium implants during healing in the rabbit tibia10.1034/j.1600-0501.1997.080310.x ↗
17. Assessment of implant stability as a prognostic determinant
18. Merdith · 1997
19. Effect of titanium surface roughness on human osteoblast proliferation and gene expression in vitro
20. Tistarite, Ti2O3, a new refractory mineral from the Allende meteorite10.2138/am.2009.3203 ↗
21. Titanium oral implants: surface characteristics, interface biology and clinical outcome10.1098/rsif.2010.0118.focus ↗
22. Roughness induced dynamic changes of wettability of acid etched titanium implant modifications10.1016/j.biomaterials.2003.08.015 ↗
23. Characteristics of the surface oxides on turned and electrochemically oxidized pure titanium implants up to dielectric breakdown10.1016/S0142-9612(01)00131-4 ↗
24. Advanced surface modification techniques for enhancing osseointegration of Titanium Implant10.22974/jkda.2010.48.2.002 ↗
25. Raman scattering, superconductivity, and phonon density of states of stoichiometric and nonstoichiometric TiN10.1103/PhysRevB.17.1095 ↗
26. A histomorphometric and biomechanical comparison of titanium implants inserted in rabbit cortical and cancellous bone
27. Histomorphometry of bone apposition around three types of endosseous dental implants
28. Blue shift of Raman peak from coated TiO2 nanoparticles10.1002/jrs.773 ↗
29. Characterization and in vivo evaluation of calcium phosphate coated cp-titanium by dip-spin method10.1016/j.cap.2005.01.020 ↗