Abstract

Nickel-titanium (NiTi) shape memory alloys are widely used for medical components, as they can accommodate large strains in their superelastic state. In order to further improve the mechanical properties of NiTi, grain refinement by severe plastic deformation is applied to generate an ultrafine-grained microstructure with increased strength. In this work comprehensive fracture and fatigue crack growth experiments were performed on ultrafine-grained NiTi to assess its damage tolerance, which is essential for the safe use of this material in medical applications. It was found, that equal channel angular pressing of NiTi for 8 passes route B C increases the transformation stress by a factor of 1.5 and the yield stress of the martensite by a factor of 2.6, without significantly deteriorating its fracture and fatigue crack growth behavior. The fatigue crack growth behavior at high mean stresses is even improved, with lower fatigue crack growth rates and higher threshold stress intensity factor ranges, however, beneficial contributions from crack closure are slightly reduced.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Shape Memory Alloy Transformations · Titanium Alloys Microstructure and Properties · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Grain size dependence of fracture toughness and crack-growth resistance of superelastic NiTi10.1016/j.scriptamat.2015.10.036 ↗
2. ASTM-E1820-15a, 2015. ASTM E1820-15a, Standard Test Method for Measurement of Fracture Toughness, ASTM International.
3. ASTM-E399-12e3, 2012. ASTM E399-12e3, Standard Test Method for Linear-Elastic Plane-Strain Fracture Toughness KIc of Metallic Materials, ASTM International.
4. ASTM-E647-15, 2015. ASTM E647-15, Standard Test Method for Measurement of Fatigue Crack Growth Rates, ASTM International.
5. A summary of recent research on the Nitinol alloys and their potential application in ocean engineering10.1016/0029-8018(68)90019-X ↗
6. An overview of nitinol medical applications10.1016/S0921-5093(99)00294-4 ↗
7. Structural and functional fatigue of NiTi shape memory alloys10.1016/j.msea.2003.10.327 ↗
8. Eiselstein, L.E., Sire, R.A., James, B.A., 2006. Review of fatigue and fracture behavior in NiTi, in: Medical Device Materials III – Proceedings of the Materials and Processes for Medical Devices Conference 2005, pp. 135–147.
9. Improving the ductility of nanocrystalline bcc metals10.1021/nl0515807 ↗
10. Compact tension testing of martensitic/pseudoplastic NiTi shape memory alloys10.1016/j.msea.2007.03.126 ↗
11. Fracture mechanics and microstructure in NiTi shape memory alloys10.1016/j.actamat.2008.10.055 ↗
12. Direct physical evidence for the back-transformation of stress-induced martensite in the vicinity of cracks in pseudoelastic NiTi shape memory alloys10.1016/j.actamat.2009.08.015 ↗
13. Microstructure and mechanical properties of the SPD-processed TiNi alloys10.4028/www.scientific.net/MSF.738-739.486 ↗
14. Fatigue behavior of nanocrystalline metals and alloys10.1016/j.ijfatigue.2005.06.035 ↗
15. Fracture and fracture toughness of nanopolycrystalline metals produced by severe plastic deformation
16. Fracture of ECAP-deformed iron and the role of extrinsic toughening mechanisms10.1016/j.actamat.2013.01.057 ↗
17. A comprehensive study on the damage tolerance of ultrafine-grained copper10.1016/j.msea.2012.01.089 ↗
18. Fracture toughness evaluation of ultrafine-grained nickel10.1016/j.scriptamat.2011.02.007 ↗
19. Anisotropic fracture behavior of ultrafine-grained iron10.1016/j.msea.2009.12.033 ↗
20. Effect of large shear deformations on the fracture behavior of a fully pearlitic steel10.1007/s11661-010-0541-7 ↗
21. Fatigue thresholds of Ni-Ti alloy near the shape memory transition temperature10.1016/S0142-1123(99)00065-1 ↗
22. Irwin, G.R., 1960. Plastic zone near a crack and fracture toughness, Proc. seventh Sagamore Ordnance Mater. Res. Conf. IV-63.
23. Jackson, C.M., Wagner, H.J., Wasilewski, R.J., 1972. The alloy with a memory, 55-Nitinol: its physical metallurgy, properties, and applications, Nasa Rep. SP 5110.
24. Thermomechanical cyclic response of an ultrafine-grained NiTi shape memory alloy10.1016/j.actamat.2008.04.001 ↗
25. Laird, C., 1967. The influence of metallurgical structure on the mechanisms of fatigue crack propagation, Fatigue Crack Propagation, ASTM STP 415, 131. http://dx.doi.org/10.1520/STP47230S.10.1520/STP47230S ↗
26. Crack propagation in high stress fatigue10.1080/14786436208212674 ↗
27. Molecular dynamics investigation of the fracture behavior of nanocrystalline α -Fe10.1103/PhysRevB.69.134110 ↗
28. Fatigue crack growth anisotropy in ultrafine-grained iron
29. Revisiting fatigue crack growth in various grain size regimes of Ni10.1016/j.msea.2015.08.071 ↗
30. Fracture properties of polycrystalline NiTi shape memory alloy10.1016/j.msea.2015.12.014 ↗
31. Crack-tip thermal and mechanical hysteresis in shape memory alloys under fatigue loading10.1016/j.msea.2014.08.007 ↗
32. Fatigue-crack growth behavior in the superelastic and shape-memory alloy nitinol10.1007/s11661-001-1008-7 ↗
33. Fatigue of NITI thermoelastic martensites10.1016/0001-6160(79)90065-8 ↗
34. Coarse slip model of fatigue10.1016/0001-6160(69)90099-6 ↗
35. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
36. A review of fatigue behavior in nanocrystalline metals10.1007/s11340-009-9301-2 ↗
37. Dislocation emission and fatigue crack growth threshold10.1016/0956-7151(91)90304-J ↗
38. Use of fatigue specimens precracked in compression for measuring threshold values and crack growth10.1520/JTE12641J ↗
39. Mechanical reasons for plasticity-induced crack closure under plane strain conditions10.1046/j.1460-2695.1998.00131.x ↗
40. Mechanisms of fatigue crack propagation in metals, ceramics and composites: role of crack tip shielding10.1016/0025-5416(88)90547-2 ↗
41. Mechanical fatigue and fracture of Nitinol10.1179/1743280411Y.0000000009 ↗
42. In vitro fatigue-crack growth and fracture toughness behavior of thin-walled superelastic Nitinol tube for endovascular stents: a basis for defining the effect of crack-like defects10.1016/j.biomaterials.2006.09.034 ↗
43. Root canal instruments for manual use: a review10.1111/j.1600-9657.1997.tb00011.x ↗
44. On the nature of the biocompatibility and on medical applications of NiTi shape memory and superelastic alloys
45. Shape memory effect in nanocrystalline NiTi alloy processed by high-pressure torsion10.1016/j.msea.2014.12.056 ↗
46. Relationships between the J-integral and the crack opening displacement for stationary and extending cracks10.1016/0022-5096(81)90003-X ↗
47. Suresh · 1991
48. Superelasticity and its stability of an ultrafine-grained Ti49.2Ni50.8 shape memory alloy processed by equal channel angular pressing10.1016/j.msea.2013.08.049 ↗
49. Nanostructuring of metals by severe plastic deformation for advanced properties10.1038/nmat1180 ↗
50. Nanostructuring of TiNi Alloy by SPD processing for advanced properties10.2320/matertrans.ME200722 ↗
51. Fatigue limit and crack growth in ultra-fine grain metals produced by severe plastic deformation10.1007/s10853-006-0973-z ↗