Effect of grinding on subsurface modifications of pre-sintered zirconia under different cooling and lubrication conditions

P. Suya Prem Anand, N. Arunachalam, L. Vijayaraghavan

Publisher page

Abstract

Pre-sintered zirconia is preferred as a restoration material in dental applications due to its excellent strength and fracture toughness. When abrasive processes were used to obtain the required shape of (Y-TZP) yttria-stabilized tetragonal pre-sintered zirconia, it resulted in material strength degradation in the presence of coolant. Therefore, experiments were carried out on pre-sintered zirconia with diamond grinding wheel to evaluate the performance of cooling conditions such as dry, wet and minimum quantity lubrication (MQL). The effects of different environments on the grinding performance were studied based on the temperature distribution, phase transformation, flexural strength, microhardness and edge chipping damage. The Raman spectroscopy and X-ray diffraction analysis were used to estimate the quantity of monoclinic phase in pre-sintered zirconia. The temperature rise of the workpiece material during the grinding experiment was not higher and insufficient to cause the thermal stresses. The microstructural changes induced by grinding under different cooling strategies were associated with the quantitative assessment of monoclinic phase. The flexural strength of ground components was improved in the dry condition compared to the other process due to the absence of the defective layer and the occurrence of Y3+ ions segregation. After grinding, there was a slight decrease in the hardness value by (1-8 HV), which was due to the formation of microcracks in the subsurface layer of the ground surface. In addition, to ensure the presence of microcracks, the edge chipping depth was measured. The damage depth obtained from the wet condition showed a higher value of 30 µm compared to the dry and MQL conditions.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Assessment of elasticity, plasticity and resistance to machining-induced damage of porous pre-sintered zirconia using nanoindentation techniques10.1016/j.jmst.2016.02.009 ↗
2. Nano-scale mechanical properties and behavior of pre-sintered zirconia10.1016/j.jmbbm.2014.03.019 ↗
3. ASTM C1161-13 · 2002
4. ASTM C1322-05a · 2005
5. Grinding damage assessment on four high-strength ceramics10.1016/j.dental.2015.11.028 ↗
6. Measurement of crystallographically transformed zone produced by fracture in ceramics containing tetragonal zirconia10.1111/j.1151-2916.1982.tb10445.x ↗
7. Effect of oxygen vacancy on phase transition and photoluminescence properties of nanocrystalline zirconia synthesized by the one-pot reaction10.1021/jp8103497 ↗
8. Controllable synthesis of metastable tetragonal zirconia nanocrystals using citric acid assisted sol–gel method10.1016/j.ceramint.2012.09.067 ↗
9. David Green · 1998
10. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
11. Influence of surface finish and residual stresses on the ageing sensitivity of biomedical grade zirconia10.1016/j.biomaterials.2005.11.021 ↗
12. Phase analysis in zirconia system10.1111/j.1151-2916.1972.tb11290.x ↗
13. Transformation toughening: an overview10.1111/j.1151-2916.1986.tb07400.x ↗
14. Production and characterization of self-colored dental zirconia blocks10.1016/j.ceramint.2012.06.056 ↗
15. Grain boundary segregation induced phase transformation in Y-TZP10.2109/jcersj.114.230 ↗
16. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
17. Evaluation of surface and sub surface cracks of ground ceramics10.1016/S0924-0136(98)00403-8 ↗
18. Microstructural changes produced by abrading Y-TZP in presintered and sintered conditions10.1016/j.jdent.2012.06.009 ↗
19. Microstructural changes in ground 3Y-TZP and their effect on mechanical properties10.1016/j.actamat.2011.07.024 ↗
20. Effect of low-temperature aging on the mechanical behavior of ground Y-TZP10.1016/j.jmbbm.2014.12.009 ↗
21. Mechanical behavior of a Y-TZP ceramic for monolithic restorations: effect of grinding and low-temperature aging10.1016/j.msec.2016.02.049 ↗
22. The effect of grinding on the mechanical behavior of Y-TZP ceramics: a systematic review and meta-analyses10.1016/j.jmbbm.2016.06.028 ↗
23. Raman spectroscopic analysis of phase-transformation and stress patterns in zirconia hip joints10.1117/1.1647547 ↗
24. Assessment of low-temperature degradation of Y-TZP ceramics based on Raman-spectroscopic analysis and hardness indentation10.1016/j.jeurceramsoc.2014.07.018 ↗
25. Influence of surface roughness and phase transformation induced by grinding on the strength of ZrO2–Y2O310.1016/0141-6359(94)00012-O ↗
26. Calibration curve for quantitative analysis of the monoclinic tetragonal ZrO2 system by X-rays diffraction10.1111/j.1151-2916.1984.tb19715.x ↗
27. Interest of Raman spectroscopy for the study of dental material: the zirconia material example10.1016/j.irbm.2010.10.004 ↗
28. Effect of grinding on strength of tetragonal zirconia and zirconia-toughened alumina10.1080/10940349708945637 ↗