journal article·2014-04

Wear resistance of a pressable low-fusing ceramic opposed by dental alloys

Adriana Cláudia Lapria Faria, André Almeida de Oliveira, Érica Alves Gomes, Renata Cristina Silveira Rodrigues, Ricardo Faria Ribeiro

Publisher page

Abstract

Dental alloys have increasingly replaced by dental ceramics in dentistry because of aesthetics. As both dental alloys and ceramics can be present in the oral cavity, the evaluation of the wear resistance of ceramics opposed by dental alloys is important. The aim of the present study was to evaluate wear resistance of a pressable low-fusing ceramic opposed by dental alloys as well as the microhardness of the alloys and the possible correlation of wear and antagonist microhardness. Fifteen stylus tips samples of pressable low-fusing ceramic were obtained, polished and glazed. Samples were divided into three groups according to the disk of alloy/metal to be used as antagonist: Nickel-Chromium (Ni-Cr), Cobalt-Chromium (Co-Cr) and commercially pure titanium (cp Ti). Vickers microhardness of antagonist disks was evaluated before wear tests. Then, antagonist disks were sandblasted until surface roughness was adjusted to 0.75μm. Wear tests were performed at a speed of 60 cycles/min and distance of 10mm, in a total of 300,000 cycles. Before and after wear tests, samples were weighted and had their profile designed in an optical comparator to evaluate weight and height loss, respectively. Ni-Cr and cp Ti caused greater wear than Co-Cr, presenting greater weight (p=.009) and height (p=.002) loss. Cp Ti microhardness was lower than Ni-Cr and Co-Cr (p<.05). There is a positive correlation between weight and height loss (p<.05), but weight (p=.204) and height (p=.05) loss are not correlated to microhardness. The results suggest that pressable low-fusing ceramic presents different wear according to the dental alloy used as antagonist and the wear is not affected by antagonist microhardness.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Advanced materials and composites · Engineering Technology and Methodologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Three-body wear associated with three ceramics and enamel10.1016/S0022-3913(99)70037-5 ↗
2. Wear testing of composite, gold, porcelain, and enamel opposing a removable cobalt–chromium partial denture alloy10.1111/j.1532-849X.2009.00455.x ↗
3. Two-body wear of different ceramic materials opposed to zirconia ceramic10.1016/S0022-3913(10)60102-3 ↗
4. The effect of a leucite-containing ceramic filler on the abrasive wear of dental composites10.1016/j.dental.2007.03.006 ↗
5. Modeling wear of cast ti alloys10.1016/j.actbio.2006.10.007 ↗
6. Wear of enamel opposing low-fusing and conventional ceramic restorative materials10.1111/j.1532-849X.2001.00008.x ↗
7. In vitro wear of composite with varied cure, filler level, and filler treatment10.1177/00220345970760071101 ↗
8. Mechanical comparison of experimental conical-head abutment screws with conventional flat-head abutment screws for external-hex and internal tri-channel implant connections: an in vitro evaluation of loosening torque10.11607/jomi.3029 ↗
9. Wear of low-fusing dental porcelains10.1016/S0022-3913(99)80014-6 ↗
10. An evaluation of wear when enamel is opposed by various ceramic materials and gold10.1016/j.prosdent.2006.09.002 ↗
11. Wear resistance of experimental titanium alloys for dental applications10.1016/j.jmbbm.2011.06.004 ↗
12. The effects of enamel wear on the metal-porcelain interface10.1016/0022-3913(83)90198-1 ↗
13. Wear resistance of nanofilled composite resin and feldspathic ceramic artificial teeth10.1016/S0022-3913(08)60262-0 ↗
14. The influence of antagonistic surface roughness on the wear of human enamel and nanofilled composite resin artificial teeth10.1016/S0022-3913(09)60068-8 ↗
15. An in vitro investigation of the wear of enamel on porcelain and gold in saliva10.1016/S0022-3913(96)90412-6 ↗
16. Enamel wear caused by three different restorative materials10.1016/S0022-3913(05)80319-1 ↗
17. International Organization for Standardization. ISO/TS 14569-2 Dental Materials – Guidance on Testing of Wear – Part 2: Wear by Two-and/or Three Body Contact, 2001.
18. In vitro evaluation of reverse torque value of abutment screw and marginal opening in a screw- and cement-retained implant fixed partial denture design
19. In vitro investigation of the wear of human enamel by dental porcelain10.1016/S0022-3913(99)70280-5 ↗
20. Wear behavior of dental y-tzp ceramic against natural enamel after different finishing procedures10.1016/j.dental.2012.04.010 ↗
21. Factors affecting enamel and ceramic wear: a literature review10.1067/mpr.2002.123851 ↗
22. Wear performance of dental ceramics after grinding and polishing treatments10.1016/j.jmbbm.2012.03.002 ↗
23. Load fatigue performance of a single-tooth implant abutment system: effect of diameter
24. Comparative study of circumferential clasp retention force for titanium and cobalt-chromium removable partial dentures10.1067/mpr.2002.128128 ↗
25. Two-body wear of dental porcelain and substructure oxide ceramics10.1007/s00784-011-0589-9 ↗
26. Alloys for prosthodontic restorations10.1067/mpr.2002.123817 ↗