journal article·2018-02

Understanding the mechanism for the mechanical property degradation of a lithium disilicate glass-ceramic by annealing

D. Li, X.C. Li, Z.Z. Zhang, S.F. Zhang, L. He

Publisher page

Abstract

Post-crystallization annealing above the Tg was applied to a lithium disilicate glass-ceramic with microstructure consisting of glassy matrix and rod-like lithium disilicate crystals, effect of the annealing on the mechanical behavior was investigated. Flexural strength and VIF toughness of the glass-ceramic unexpectedly decreased after the annealing. The mechanical behavior variation was understood based on residual micro-stress analysis. Coefficient of thermal expansion for the glassy matrix presented a tendency to increase after the annealing, which would enlarge the thermal expansion mismatch between the glassy matrix and the lithium disilicate crystals. As a result, the residual micro-stresses in the glass-ceramic abnormally increased with increasing the annealing time. The mechanical property degradation was attributed to the annealing-induced increase of the residual micro-stresses.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Fracture toughness of two lithium disilicate dental glass ceramics10.1016/j.prosdent.2016.02.009 ↗
2. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
3. The crystallization of an aluminosilicate glass in the K2O–Al2O3–SiO2 system10.1016/j.dental.2005.02.001 ↗
4. Effect of plasma electrolytic oxidation treatment on the mechanical properties of a Zr–Cu–Ni–Ti–Al bulk metallic glass10.1016/j.msea.2016.06.068 ↗
5. Crystallization of high-strength fine-sized leucite glass-ceramics10.1177/0022034510377795 ↗
6. Crystallization and flexural strength optimization of fine-grained leucite glass-ceramics for dentistry10.1016/j.dental.2011.08.009 ↗
7. Flexural strength of glass–ceramic for structural applications10.1016/j.jeurceramsoc.2013.10.032 ↗
8. Effect of cubic leucite stabilization on the flexural strength of feldspathic dental porcelain10.1177/00220345960750120301 ↗
9. Effect of post-processing heat treatment on the fracture strength of a heat-pressed dental ceramic10.1002/jbm.b.20018 ↗
10. Phase and microstructure formation and their influence on the strength of two types of glass-ceramics10.1016/j.jnoncrysol.2013.03.009 ↗
11. Influence of annealing temperature on the strength of dental glass ceramic materials10.1016/j.dental.2004.09.004 ↗
12. Flexural resistance of heat-pressed and CAD-CAM lithium disilicate with different translucencies10.1016/j.dental.2016.10.005 ↗
13. Flexural properties of leucite and lithium disilicate ceramic materials after repeated firings10.1016/j.jds.2013.02.019 ↗
14. Enthalpy relaxation in hyperquenched glasses of different fragility10.1016/j.jnoncrysol.2007.10.023 ↗
15. Studies of crystal phase formations in high-strength lithium disilicate glass-ceramics10.1016/j.jnoncrysol.2006.06.039 ↗
16. Principles and phenomena of bioengineering with glass-ceramics for dental restoration10.1016/j.jeurceramsoc.2006.04.101 ↗
17. Residual thermal stresses in ceramic composites. Part I: with ellipsoidal inclusions10.1016/0921-5093(96)10176-3 ↗
18. Fabrication of a high-strength lithium disilicate glass-ceramic in a complex glass system10.1016/j.jascer.2013.02.007 ↗
19. In situ study of stress relaxation mechanisms of pure Al thin films during isothermal annealing10.1016/j.scriptamat.2006.02.024 ↗
20. ISO 6872 · 2008
21. ISO 25178-2 · 2012
22. Effects of crystal size on the mechanical properties of a lithium disilicate glass-ceramic10.1016/j.msea.2016.05.068 ↗
23. Microstructural evolution and physical behavior of a lithium disilicate glass–ceramic10.1016/j.dental.2015.05.003 ↗
24. X-ray stress analysis10.1007/BF02326143 ↗
25. Anisotropic residual stresses in partially crystallized Li2O–2SiO2 glass-ceramics10.1016/S0022-3093(99)00038-1 ↗
26. Characterisation and properties of lithium disilicate glass ceramics in the SiO2-Li2O-K2O-Al2O3 system for dental applications10.1155/2013/763838 ↗
27. Effect of stress relief annealing on microstructure & mechanical properties of welded joints between low alloy carbon steel and stainless steel10.1007/s11661-016-3840-9 ↗
28. Glass transition Tg, thermal expansion, and quenched-in free volume ΔVf in pyrex glass measured by time-resolved X-ray diffraction10.1016/j.jallcom.2004.07.011 ↗
29. Microstructure, mechanical properties and residual stresses as a function of welding speed in aluminium AA5083 friction stir welds10.1016/S1359-6454(03)00319-7 ↗
30. Surface and bulk residual stresses in Li2O·2SiO2 glass–ceramics10.1016/j.jnoncrysol.2007.04.007 ↗
31. On the vickers indentation fracture toughness test10.1111/j.1551-2916.2006.01482.x ↗
32. Recovery of less relaxed state in Zr-Al-Ni-Cu bulk metallic glass annealed above glass transition temperature10.1063/1.4835076 ↗
33. The effect of strontium oxide replacing calcium oxide on the crystallization and thermal expansion properties of Li2O–CaO–SiO2 glasses10.1016/j.ceramint.2014.08.047 ↗
34. Internal stresses in ceramics10.1111/j.1151-2916.1961.tb15475.x ↗
35. Internal residual stresses in partially crystallized photo-thermo-refractive glass10.1111/j.1551-2916.2010.04372.x ↗
36. Internal residual stresses in sintered and commercial low expansion Li2O–Al2O3–SiO2 glass-ceramics10.1111/j.1551-2916.2010.04220.x ↗
37. Internal residual stresses in glass-ceramics: a review10.1016/j.jnoncrysol.2012.01.040 ↗
38. Crystallization toughening of a model glass-ceramic10.1016/j.actamat.2014.12.007 ↗
39. TEM and XRD study of early crystallization of lithium disilicate glasses10.1016/j.jnoncrysol.2003.08.075 ↗
40. Crystallization of lithium disilicate-based multicomponent glasses-effect of silica-lithia ratio10.1016/j.ceramint.2014.08.074 ↗
41. The effects of repeated heat-pressing on the mechanical properties and microstructure of IPS e.max Press10.1016/j.jmbbm.2014.09.016 ↗
42. Effects of P2O5 and sintering temperature on microstructure and mechanical properties of lithium disilicate glass-ceramics10.1016/j.actamat.2007.02.009 ↗
43. Crystal growth in a multicomponent lithia aluminosilicate glass10.1016/j.matchemphys.2009.04.010 ↗
44. Effect of sintering time on the microstructure, flexural strength and translucency of lithium disilicate glass-ceramics10.1016/j.jnoncrysol.2012.11.010 ↗
45. A bright future for glass-ceramics
46. Preparation and thermal expansion behavior of glass coatings for electronic applications10.1016/S0254-0584(02)00073-1 ↗
47. Effect of heat treatment on the microstructure and properties of lithium disilicate glass-ceramics10.1016/j.jnoncrysol.2014.05.023 ↗
48. Improved densification and properties of pressureless-sintered lithium disilicate glass-ceramics10.1016/j.msea.2014.10.037 ↗
49. Effects of P2O5 and heat treatment on crystallization and microstructure in lithium disilicate glass ceramics10.1016/j.actamat.2007.10.024 ↗
50. Residual stresses in Pb(Zr0.52Ti0.48)O3 thin films deposited by metal organic decomposition10.1016/S1359-6462(03)00181-7 ↗