journal article·2018-10

Bond strength of resin cement to zirconia treated in pre-sintered stage

Kamal Ebeid, Sebastian Wille, Tarek Salah, Marwa Wahsh, Maged Zohdy, Matthias Kern

Publisher page

Abstract

Purpose Aim of this study was to evaluate the tensile bond strength (TBS) between resin cement and zirconia surface treated in different sintering stages. Materials and methods Eighty zirconia discs having final dimensions of 12 mm diameter and 3.2 mm thickness were milled then divided into three main groups according to the type of surface treatment performed (group 1: air abrasion using 50 µm Al2O3 particles, group 2: silica coating using Rocatec soft, and group 3: a control group receiving no surface treatment). Groups 1 and 2 were divided into two subgroups each according to the stage in which the surface treatment was performed (subgroup A; surface treatment performed in the pre-sintered stage and subgroup B; surface treatment performed in the post-sintered stage). Discs were later bonded to composite core materials using resin cement then tested for TBS either being subjected to 3 days of water storage or 150 days of water storage and 37,500 thermal cycles. Results Long-term aging caused a significant decrease in TBS of all subgroups except the subgroup air-abraded in the post-sintered stage. After long-term aging, the group silica coated in the pre-sintered stage showed the significantly lowest TBS compared to all other groups. There was also no significant difference between the subgroups air-abraded and silica coated in the pre-sintered stage. All specimens in the control group debonded during long-term aging. Significance Air-abrading zirconia with Al2O3 at a reduced pressure in the pre-sintered stage may result in durable bond strength to resin cement.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Endodontics and Root Canal Treatments · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Zirconia ceramic inlay-retained fixed dental prostheses - first clinical results with a new design10.1016/j.jdent.2010.12.005 ↗
2. Long-term resin bonding to zirconia ceramic with a new universal primer10.1016/S0022-3913(11)60137-6 ↗
3. Influence of surface conditioning and cleaning methods on resin bonding to zirconia ceramic10.1016/j.dental.2010.10.004 ↗
4. Resin-ceramic bonding: a review of the literature10.1067/mpr.2003.50 ↗
5. Effect of surface pre-treatments on the zirconia ceramic-resin cement microtensile bond strength10.1016/j.dental.2011.07.002 ↗
6. Effects of thermocycling on the degree of cure of two lingual retainer composites10.4012/dmj.2009-043 ↗
7. Stability of the bond between two resin cements and an yttria-stabilized zirconia ceramic after six months of aging in water10.1016/j.prosdent.2013.12.003 ↗
8. Effect of accelerated aging on dental zirconia-based materials10.1016/j.jmbbm.2016.08.023 ↗
9. Shear vs. tensile bond strength of resin composite bonded to ceramic10.1177/00220345950740091401 ↗
10. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
11. Effect of metal primers on microtensile bond strength between zirconia and resin cements10.1016/S0022-3913(11)60055-3 ↗
12. Evaluation of surface treatments of monolithic zirconia in different sintering stages10.1016/j.jpor.2017.09.001 ↗
13. Influence of sandblasting granulometry and resin cement composition on microtensile bond strength to zirconia ceramic for dental prosthetic frameworks10.1016/j.jdent.2012.09.013 ↗
14. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics10.1016/j.dental.2003.05.002 ↗
15. Dental zirconia adhesion with silicon compounds using some experimental and conventional surface conditioning methods10.1007/s12633-009-9022-2 ↗
16. Insights on ceramics as dental materials. Part I: ceramic material types in dentistry10.1007/s12633-011-9078-7 ↗
17. Meta-analysis of bonding effectiveness to zirconia ceramics10.1177/0022034514524228 ↗
18. Resin bonding to oxide ceramics for dental restorations10.1163/156856109X432721 ↗
19. Bonding to oxide ceramics-laboratory testing versus clinical outcome10.1016/j.dental.2014.06.007 ↗
20. Surface conditioning influences zirconia ceramic bonding10.1177/0022034509340881 ↗
21. Bonding to zirconia ceramic: adhesion methods and their durability10.1016/S0109-5641(98)00011-6 ↗
22. Effect of surface treatment on bond strength between an indirect composite material and a zirconia framework10.2334/josnusd.54.39 ↗
23. The effect of surface grinding and sandblasting on flexural strength and reliability of Y-TZP zirconia ceramic10.1016/S0109-5641(99)00070-6 ↗
24. Durability of resin bonding to zirconia ceramic using different primers
25. An overview of zirconia ceramics: basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
26. Evaluation of resin adhesion to zirconia ceramic using some organosilanes10.1016/j.dental.2005.11.035 ↗
27. Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics10.1016/j.dental.2008.09.002 ↗
28. Adhesion to zirconia used for dental restorations: a systematic review and meta-analysis
29. Comparison of resin cement adhesion to Y-TZP ceramic following manufacturers' instructions of the cements only10.1007/s00784-007-0151-y ↗
30. Effect of surface conditioning methods on the bond strength of luting cement to ceramics10.1016/S0109-5641(03)00019-8 ↗
31. Bonding between oxide ceramics and adhesive cement systems: a systematic review10.1002/jbm.b.33013 ↗
32. Silicoating: evaluation of a new method of bonding composite resin to metal
33. Zirconia as a ceramic biomaterial10.1016/S0142-9612(98)00010-6 ↗
34. The shear bond strength between luting cements and zirconia ceramics after two pre-treatments
35. Relationship between surface area for adhesion and tensile bond strength--evaluation of a micro-tensile bond test10.1016/0109-5641(94)90067-1 ↗
36. CAD/CAM single retainer zirconia-ceramic resin-bonded fixed dental prostheses: clinical outcome after 5 years
37. Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?10.1016/j.dental.2010.10.022 ↗
38. Aspects of bonding between resin luting cements and glass ceramic materials10.1016/j.dental.2014.01.017 ↗
39. Fracture resistance of lithium disilicate-, alumina-, and zirconia-based three-unit fixed partial dentures: a laboratory study
40. Structural reliability of alumina-, feldspar-, leucite-, mica- and zirconia-based ceramics10.1016/S0300-5712(00)00030-0 ↗
41. Long-term resin bond strength to zirconia ceramic
42. Durability of the resin bond strength to zirconia ceramic after using different surface conditioning methods10.1016/j.dental.2005.11.040 ↗
43. Influence of air-abrasion on zirconia ceramic bonding using an adhesive composite resin10.1016/j.dental.2009.08.008 ↗
44. Effect of sandblasting on the long-term performance of dental ceramics10.1002/jbm.b.30097 ↗