journal article·2021-09Open access

In-lab simulation of CAD/CAM milling of lithium disilicate glass-ceramic specimens: Effect on the fatigue behavior of the bonded ceramic

Rafaela Oliveira Pilecco, Fernanda Dalla-Nora, Luís Felipe Guilardi, Gabriel Kalil Rocha Pereira, Guilherme Schmitt de Andrade, Renata Marques de Melo, Luiz Felipe Valandro, Marília Pivetta Rippe

Abstract

The aim of this study was to evaluate the effect of in-lab simulation procedures performed on a lithium disilicate ceramic luted to a dentin-analogue material regarding the fatigue performance and topographic changes. Lithium disilicate ceramic (IPS e.max CAD) discs (Ø = 13.5 mm and 1.5 mm of thickness) were produced in different ways: milled in a CAD/CAM system (CAD/CAM - control group); mirror-polished (POL group); produced in-lab and ground with #60 silicon carbide paper (SiC group); with #60 wood sandpaper (WS group); with a fine diamond bur (DB group); or with a CAD/CAM bur adapted in a handpiece with a custom mandrel (MANDREL group). The ceramic discs were adhesively luted (Multilink N) onto dentin analogue discs (Ø = 12 mm and 2 mm of thickness) and fatigue testing (n = 19 discs) was performed by step-stress methodology (initial load of 200 N; step-size of 50 N; 10,000 cycles per step; 20 Hz). Surface roughness and contact angle analysis were also performed. According to Kaplan-Meier and post-hoc Mantel-Cox (log-rank), distinct fabrication methods affected the fatigue performance of bonded glass-ceramic discs (p< 0.001). The CAD/CAM group presented the lowest fatigue failure loads (1250 N) and number of cycles for failure (185,000), while the POL groups obtained the highest results (1752 N; 284,444 cycles). The in-lab groups had intermediate values (1355 - 1526 N; 206,052 - 238,684 cycles). Polished specimens presented the lowest roughness values (Ra = 0.041 μm), while the SiC (1.604 μm), WS (1.701 μm), and MANDREL (1.867 μm) groups showed statistically similar roughness values to the CAD/CAM group (1.738 μm). Despite differences before etching, the contact angle was similar among the milled and simulated groups after etching, except for the polished group. Even with some topographic similarities, the tested in-lab simulation methods were not able to mimic the milled specimens in terms of fatigue findings, leading to distinct magnitude of overestimations of the results.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Additive Manufacturing and 3D Printing Technologies · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Machining variability impacts on the strength of a “chair-side” CAD-CAM ceramic10.1016/j.dental.2012.04.017 ↗
2. Fracture, roughness and phase transformation in CAD/CAM milling and subsequent surface treatments of lithium metasilicate/disilicate glass-ceramics10.1016/j.jmbbm.2017.06.015 ↗
3. Influence of CAD/CAM milling, sintering and surface treatments on the fatigue behavior of lithium disilicate glass ceramic10.1016/j.jmbbm.2020.104133 ↗
4. Mechanical behavior of bulk direct composite versus block composite and lithium disilicate indirect Class II restorations by CAD-FEM modeling10.1016/j.dental.2017.03.014 ↗
5. Contemporary dental ceramic materials, a review: chemical composition, physical and mechanical properties, indications for use. Open Access Maced
6. The current state of chairside digital dentistry and materials10.1016/j.cden.2018.11.002 ↗
7. The fracture resistance of a CAD/CAM Resin Nano Ceramic (RNC) and a CAD ceramic at different thicknesses10.1016/j.dental.2014.05.018 ↗
8. Machinability: zirconia-reinforced lithium silicate glass ceramic versus lithium disilicate glass ceramic10.1016/j.jmbbm.2019.103435 ↗
9. Bond strength of CAD/CAM restorative materials treated with different surface etching protocols
10. Grinding damage assessment for CAD-CAM restorative materials10.1016/j.dental.2016.12.004 ↗
11. Dental ceramics: a review of new materials and processing methods10.1590/1807-3107bor-2017.vol31.0058 ↗
12. One-step ceramic primer as surface conditioner: effect on the load-bearing capacity under fatigue of bonded lithium disilicate ceramic simplified restorations10.1016/j.jmbbm.2020.103686 ↗
13. Newer vs. older CAD/CAM burs: influence of bur experience on the fatigue behavior of adhesively cemented simplified lithium-disilicate glass-ceramic restorations10.1016/j.jmbbm.2019.04.002 ↗
14. The effect of internal roughness and bonding on the fracture resistance and structural reliability of lithium disilicate ceramic10.1016/j.dental.2017.09.018 ↗
15. How and when does fabrication damage adversely affect the clinical performance of ceramic restorations?10.1016/j.dental.2012.07.001 ↗
16. Fatigue strength of bilayered ceramics under cyclic loading as a function of core veneer thickness ratios10.1016/j.prosdent.2015.09.017 ↗
17. CAD-CAM in dentistry10.14219/jada.archive.1988.0096 ↗
18. Hard machining, glaze firing and hydrofluoric acid etching: do these procedures affect the flexural strength of a leucite glass-ceramic?10.1016/j.dental.2015.04.005 ↗
19. Impact of machining on the flexural fatigue strength of glass and polycrystalline CAD/CAM ceramics10.1016/j.dental.2017.07.019 ↗
20. Fatigue performance of distinct CAD/CAM dental ceramics10.1016/j.jmbbm.2019.103540 ↗
21. ISO 428
22. Surface energy of etched ceramic
23. Development of a clinically validated bulk failure test for ceramic crowns10.1016/S0022-3913(10)60129-1 ↗
24. ADM guidance-ceramics: fatigue principles and testing10.1016/j.dental.2017.09.006 ↗
25. Ceramic dental biomaterials and CAD/CAM technology: State of the art10.1016/j.jpor.2014.07.003 ↗
26. Microstructural evolution and physical behavior of a lithium disilicate glass-ceramic10.1016/j.dental.2015.05.003 ↗
27. Does a self-etching ceramic primer improve bonding to lithium disilicate ceramics? Bond strengths and FeSEM analyses10.2341/17-355-L ↗
28. Effects of cement thickness and bonding on the failure loads of CAD/CAM ceramic crowns: multi-physics FEA modeling and monotonic testing10.1016/j.dental.2012.04.033 ↗
29. Effect of acid etching on tridimensional microstructure of etchable CAD/CAM materials10.1016/j.dental.2018.03.013 ↗
30. Surface conditioning protocol for the adhesion of resin-based cements to base and noble alloys: how to condition and why?
31. How does hydrofluoric acid etching affect the cyclic load-to-failure of lithium disilicate restorations?10.1016/j.jmbbm.2018.07.040 ↗
32. Hydrofluoric acid concentrations: effect on the cyclic load-to-failure of machined lithium disilicate restorations10.1016/j.dental.2018.06.028 ↗
33. Near-surface damage - a persistent problem in crowns obtained by computer-aided design and manufacturing10.1243/095441105X9363 ↗
34. Microtensile bond strength of lithium disilicate to Zirconia with the CAD-on technique10.1111/jopr.12246 ↗
35. Internal adjustments decrease the fatigue failure load of bonded simplified lithium disilicate restorations10.1016/j.dental.2018.05.015 ↗
36. Strength-limiting damage in lithium silicate glass-ceramics associated with CAD–CAM10.1016/j.dental.2018.11.004 ↗
37. ADM guidance—ceramics: guidance to the use of fractography in failure analysis of brittle materials10.1016/j.dental.2017.03.004 ↗
38. CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: fatigue performance and ceramic surface characteristics10.1016/j.jmbbm.2019.03.005 ↗
39. Evaluation of subsurface damage in CAD/CAM machined dental ceramics10.1023/A:1008812929476 ↗
40. CAD/CAM ceramic restorative materials for natural teeth10.1177/0022034518779759 ↗
41. Aspects of bonding between resin luting cements and glass ceramic materials10.1016/j.dental.2014.01.017 ↗
42. Step-stress vs. staircase fatigue tests to evaluate the effect of intaglio adjustment on the fatigue behavior of simplified lithium disilicate glass-ceramic restorations
43. Wachtman
44. Wide applicability10.1115/1.4010337 ↗
45. Yoon, H., Sohn, P.J., Jin, S., Elani, H., Lee, S.J. Fracture resistance of CAD/CAM-Fabricated lithium disilicate MOD inlays and onlays with various cavity preparation designs. J. Prosthodont.. 2019 Feb;28(2):e524-e529. doi: 10.1111/jopr.12787.10.1111/jopr.12787 ↗
46. Dental ceramics for restoration and metal veneering10.1016/j.cden.2017.06.005 ↗
47. CAD/CAM machining vs pre-sintering in-lab fabrication techniques of Y-TZP ceramic specimens: effects on their mechanical fatigue behavior10.1016/j.jmbbm.2017.03.013 ↗