In-vivo degradation of middle-term highly cross-linked and remelted polyethylene cups: Modification induced by creep, wear and oxidation
Source abstract
Abstract
In this study Raman (RS) and Fourier Transform Infrared (FT-IR) spectroscopic techniques were exploited to study 11 retrieved liners made of remelted highly cross-linked polyethylene (HXLPE), with the intent to elucidate their in-vivo mechanical and chemical degradation. The retrievals had different follow-ups, ranging from a few months to 7 years of implantation time and belong to the first generation of highly cross-linked and remelted polyethylene clinically introduced in 1999, but still currently implanted. Raman assessments enabled to discriminate contributes of wear and creep on the total reduction of thickness in different locations of the cup. According to our results, although the most of the viscoelastic deformation occurred during the first year (bedding-in period), it progressed during the steady wear state up to 7 years with much lower but not negligible rate. Overall, the wear rate of this remelted HXLPE liner was low. Preliminary analysis on microtomed sections of the liners after in-vivo and in-vitro accelerated aging (ASTM F2003-02) enabled to obtain a phenomenological correlation between the oxidation index (OI) and the amount of orthorhombic phase fraction (αc), which can be easily non-destructively measured by RS. Profiles of αc obtained from different locations of the cups were used to judge the oxidative degradation of the 11 retrievals, considering also the ex-vivo time elapsed from the revision surgery to the spectroscopic experiments. Low but measurable level of oxidation was detected in all the short-term retrievals, while in the middle-term samples peaks of OI were observed in the subsurface (up to OI=4.5), presumably induced by the combined effect of mechanical stress, lipid absorption and prolonged ex-vivo shelf-aging in air.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Total Knee Arthroplasty Outcomes · Orthopedic Infections and Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. The effects of degree of crosslinking on the fatigue crack initiation and propagation resistance of orthopedic‐grade polyethylene10.1002/jbm.a.10606 ↗
2. Oxidation behaviour in prosthetic UHMWPE components sterilised with high-energy radiation in the presence of oxygen10.1016/j.polymdegradstab.2006.08.002 ↗
3. Oxidation behaviour in prosthetic UHMWPE components sterilised with high energy radiation in a low-oxygen environment10.1016/j.polymdegradstab.2006.02.003 ↗
4. Vitamin E-stabilized UHMWPE for total joint implants: a review10.1007/s11999-010-1717-6 ↗
5. Radiostereometric analysis comparison of wear of highly cross-linked polyethylene against 36-vs 28-mm femoral heads10.1016/j.arth.2007.03.009 ↗
6. Ultra high molecular weight polyethylene—II. Thermal-and photo-oxidation10.1016/S0141-3910(97)00010-4 ↗
7. In vivo oxidation in remelted highly cross-linked retrievals10.2106/JBJS.I.01006 ↗
8. Evaluation of oxidation and fatigue damage of retrieved crossfire polyethylene acetabular cups10.2106/JBJS.F.00336 ↗
9. THE OTTO AUFRANC AWARD: highly cross-linked polyethylene in total hip arthroplasty: randomized evaluation of penetration rate in cemented and uncemented sockets using radiostereometric analysis10.1097/01.blo.0000150314.70919.e3 ↗
10. The basis for a second-generation highly cross-linked UHMWPE10.1097/01.blo.0000238856.61862.7d ↗
11. Wear comparison between conventional and highly cross-linked polyethylene against a zirconia head: a concise follow-up, at an average 10 years, of a previous report10.1016/j.arth.2012.12.020 ↗
12. Large diameter femoral heads on highly cross-linked polyethylene: minimum 3-year results10.1097/01.blo.0000218742.61624.80 ↗
13. Fatigue crack propagation resistance of virgin and highly crosslinked, thermally treated ultra-high molecular weight polyethylene10.1016/j.biomaterials.2005.09.010 ↗
14. Gillis, A., Schmieg, J., Bhattacharyya, S., Li, S., 1999. An independent evaluation of the mechanical, chemical and fracture properties of UHMWPE cross linked by 34 different conditions. In: Proceedings of the Annual meeting-Society for biomaterials in conjunction with the international biomaterials symposium, pp. 216–216.
15. A Raman spectroscopic study of the morphological structure of the polyethylenes10.1007/BF01465438 ↗
16. Gomoll, A., Wanich, T., Bellare, A., 2001. Quantitative measurement of the morphology and fracture toughness of radiation crosslinked UHMWPE. ORS. February.
17. Challenge to the concept that UHMWPE acetabular components oxidize in vivo10.1016/0142-9612(93)90062-7 ↗
18. Deformation of press-fitted metallic resurfacing cups. Part 1: experimental simulation10.1243/095441105X69150 ↗
19. In-depth oxidation and strain profiles in UHMWPE acetabular cups non-destructively studied by confocal Raman microprobe spectroscopy10.1163/156856208X386417 ↗
20. Kurtz, S.M., 2009. Compendium of highly crosslinked UHMWPEs. In: UHMWPE Biomaterials Handbook. Amsterdam.Elsevier, pp. 291–308.10.1016/B978-0-12-374721-1.00020-1 ↗
21. History and systematic review of wear and osteolysis outcomes for first-generation highly crosslinked polyethylene10.1007/s11999-011-1872-4 ↗
22. Characterization of a highly cross-linked ultrahigh molecular-weight polyethylene in clinical use in total hip arthroplasty10.1016/j.arth.2007.06.006 ↗
23. In vivo comparative wear study of traditional and highly cross-linked polyethylene in total hip arthroplasty10.1016/j.arth.2005.03.033 ↗
24. Acetabular cup design influences deformational response in total hip arthroplasty10.1007/s11999-012-2553-7 ↗
25. Ex vivo stability loss of irradiated and melted ultra-high molecular weight polyethylene10.2106/JBJS.I.01017 ↗
26. Transition regions and surface melting in partially crystalline polyethylene: a Raman spectroscopic study10.1002/polb.1993.090310113 ↗
27. Raman spectroscopy employed for the determination of the intermediate phase in polyethylene10.1021/ma00112a050 ↗
28. Failure analysis of sandwich-type ceramic-on-ceramic hip joints: a spectroscopic investigation into the role of the polyethylene shell component10.1016/j.jmbbm.2013.01.022 ↗
29. Biomechanical modeling of acetabular component polyethylene stresses, fracture risk, and wear rate following press‐fit implantation10.1002/jor.20918 ↗
30. Correlation of wear debris-induced osteolysis and revision with volumetric wear-rates of polyethylene: a survey of 8 reports in the literature10.1080/000164701753606644 ↗
31. The elimination of free radicals in irradiated UHMWPEs with and without vitamin E stabilization by annealing under pressure10.1002/jbm.b.31799 ↗
32. A new mechanism of oxidation in ultrahigh molecular weight polyethylene caused by squalene absorption10.1002/jbm.b.32507 ↗
33. Confocal Raman spectroscopic analysis of cross-linked ultra-high molecular weight polyethylene for application in artificial hip joints10.1117/1.2710247 ↗
34. Non-destructively differentiating the roles of creep, wear and oxidation in long-term in vivo exposed polyethylene cups10.1163/092050610X537129 ↗
35. Structural profile of ultra‐high molecular weight polyethylene in acetabular cups worn on hip simulators characterized by confocal Raman spectroscopy10.1002/jor.21331 ↗
36. Structural modifications induced by compressive plastic deformation in single-step and sequentially irradiated UHMWPE for hip joint components10.1016/j.jmbbm.2013.02.019 ↗
37. Comparative oxidative stability of highly cross-linked UHMWPE after in vivo service
38. Estimation of crystallinity in polyethylene by Raman spectroscopy10.1002/jrs.1250240813 ↗
39. Current concepts review-wear in total hip and knee replacements*10.2106/00004623-199901000-00016 ↗
40. Recent advances of mechanical performance and oxidation stability in ultrahigh molecular weight polyethylene for total joint replacement: highly crosslinked and. ALPHA.-tocopherol doped10.1299/jbse.1.107 ↗
41. Standard, A., 2006. F2102-06, 2006. Standard guide for evaluating the extent of oxidation in ultra-high-molecular-weight polyethylene fabricated forms intended for surgical implants.
42. Standard, A. 2008. F2003-02, 2008. Standard practice for accelerated aging of ultra-high molecular weight polyethylene after gamma irradiation in air.
43. Raman spectroscopic method for determining the crystallinity of polyethylene
44. Reduction of wear volume from ultrahigh molecular weight polyethylene knee components by the addition of vitamin E10.1002/jor.20514 ↗
45. The seven-year wear of highly cross-linked polyethylene in total hip arthroplasty10.2106/JBJS.J.00287 ↗
46. Orientation softening in the deformation and wear of ultra-high molecular weight polyethylene10.1016/S0043-1648(96)07362-0 ↗
47. Profile of oxidation in irradiated polyethylene10.1002/(SICI)1099-0518(19980130)36:2<329::AID-POLA16>3.0.CO;2-Q ↗
48. Review article: polyethylene wear and osteolysis in total hip arthroplasty10.1177/230949900100900117 ↗