Wear performance of neat and vitamin E blended highly cross-linked PE under severe conditions: The combined effect of accelerated ageing and third body particles during wear test

Saverio Affatato, Jonathan Salvatore De Mattia, Pierangiola Bracco, Eleonora Pavoni, Paola Taddei

Publisher page

Abstract

The objective of this study is to evaluate the effects of third-body particles on the in vitro wear behaviour of three different sets of polyethylene acetabular cups after prolonged testing in a hip simulator and accelerated ageing. Vitamin E-blended, cross-linked polyethylene (XLPE_VE), cross-linked polyethylene (XLPE) and conventional polyethylene (STD_PE) acetabular cups were simulator tested for two million cycles under severe conditions (i.e. by adding third-body particles to the bovine calf serum lubricant). Micro-Fourier Transform Infrared and micro-Raman spectroscopic analyses, differential scanning calorimetry, and crosslink density measurements were used to characterize the samples at a molecular level. The STD_PE cups had twice mass loss than the XLPE_VE components and four times than the XLPE samples; statistically significant differences were found between the mass losses of the three sets of cups. The observed wear trend was justified on the basis of the differences in cross-link density among the samples (XLPE>XLPE_VE>STD_PE). FTIR crystallinity profiles, bulk DSC crystallinity and surface micro-Raman crystallinity seemed to have a similar behaviour upon testing: all of them (as well as the all-trans and ortho-trans contents) revealed the most significant changes in XLPE and XLPE_VE samples. The more severe third-body wear testing conditions determined more noticeable changes in all spectroscopic markers with respect to previous tests. Unexpectedly, traces of bulk oxidation were found in both STD_PE (unirradiated) and XLPE (remelting-stabilized), which were expected to be stable to oxidation; on the contrary, XLPE_VE demonstrated a high oxidative stability in the present, highly demanding conditions.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Orthopaedic implants and arthroplasty · Total Knee Arthroplasty Outcomes · Orthopedic Infections and Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. In vitro effects on mobile polyethylene insert under highly demanding daily activities: stair climbing
2. The performance of gamma- and EtO-sterilised UHMWPE acetabulars cups tested under severe simulator conditions. Part 1: role of the third-body wear process10.1016/S0142-9612(02)00238-7 ↗
3. The predictive power of surface profile parameters on the amount of wear measured in vitro on metal-on-polyethylene artificial hip joints10.1243/09544119JEIM95 ↗
4. In vitro wear performance of standard, crosslinked, and vitamin-E-blended UHMWPE10.1002/jbm.a.33297 ↗
5. Does cyclic stress and accelerated ageing in fluence the wear behavior of highly crosslinked polyethylene ?10.1016/j.jmbbm.2016.02.029 ↗
6. ASTM F2102-3, 2013. ASTM F2102 − 13 – Standard Guide for Evaluating the Extent of Oxidation in Polyethylene Fabricated Forms Intended for Surgical Implants. 〈https://www.astm.org/Standards/F2102.htm〉.
7. The relative effects of radiation crosslinking and type of counterface on the wear resistance of ultrahigh-molecular-weight polyethylene10.1016/j.actbio.2011.05.018 ↗
8. Analysis of wear, wear particles, and reduced inflammatory potential of vitamin E ultrahigh-molecular-weight polyethylene for use in total joint replacement10.1002/jbm.b.32904 ↗
9. Vitamin E-stabilized UHMWPE for total joint implants: a review10.1007/s11999-010-1717-6 ↗
10. Oxidation behaviour in prosthetic UHMWPE components sterilised with high energy radiation in a low-oxygen environment10.1016/j.polymdegradstab.2006.02.003 ↗
11. Oxidation behaviour in prosthetic UHMWPE components sterilised with high-energy radiation in the presence of oxygen10.1016/j.polymdegradstab.2006.08.002 ↗
12. UHMWPE for arthroplasty: past or future?10.1007/s10195-008-0038-y ↗
13. Third-body wear of highly cross-linked polyethylene in a hip simulator10.1016/S0883-5403(03)00146-3 ↗
14. Effects of microtomy on the material properties of ultra high molecular weight polyethylene10.1016/S0142-9418(00)00088-X ↗
15. Comprehensive study of parameters for characterizing three-dimensional surface topography II: statistical properties of parameter variation10.1016/0043-1648(93)90050-V ↗
16. The basis for a second-generation highly cross-linked UHMWPE10.1097/01.blo.0000238856.61862.7d ↗
17. Zirconia phase transformation, metal transfer, and surface roughness in retrieved ceramic composite femoral heads in total hip arthroplasty10.1016/j.arth.2014.08.011 ↗
18. An activated energy approach for accelerated testing of the deformation of UHMWPE in artificial joints10.1016/j.jmbbm.2010.01.004 ↗
19. The effects of gamma radiation sterilization and ageing on the structure and morphology of medical grade ultra high molecular weight polyethylene10.1016/0032-3861(96)89386-4 ↗
20. Biotribology of a vitamin E-stabilized polyethylene for hip arthroplasty – influence of artificial ageing and third-body particles on wear10.1016/j.actbio.2014.02.052 ↗
21. Biological reactions to wear debris in total joint replacement10.1243/0954411001535219 ↗
22. James, S.P., Oldinski, R. (Kurkowski), Zhang, M., Schwartz, H., 2009. UHMWPE Biomaterials Handbook. 〈http://dx.doi.org/10.1016/B978-0-12-374721-1.00018-3〉.10.1016/B978-0-12-374721-1.00018-3 ↗
23. Friction and wear behavior of ultra-high molecular weight polyethylene as a function of polymer crystallinity10.1016/j.actbio.2008.02.022 ↗
24. The effect of gamma-irradiation on ultra-high molecular weight polyethylene recrystallized under different cooling conditions10.1016/S0969-806X(00)00333-9 ↗
25. Aggressive 3rd-body wear challenge to highly crosslinked polyethylene: a hip simulator model10.1016/j.wear.2009.01.029 ↗
26. Bearing surfaces in hip replacement – evolution and likely future10.1016/j.mjafi.2014.04.015 ↗
27. Kurtz · 2015
28. Trace concentrations of vitamin E protect radiation crosslinked UHMWPE from oxidative degradation10.1002/jbm.a.32122 ↗
29. Wear in highly crosslinked polyethylenes10.1016/j.cuor.2008.10.011 ↗
30. Interlaboratory reproducibility of standard accelerated aging methods for oxidation of UHMWPE10.1016/S0142-9612(00)00333-1 ↗
31. Evolution of morphology in UHMWPE following accelerated aging: the effect of heating rates10.1002/(SICI)1097-4636(199907)46:1<112::AID-JBM13>3.0.CO;2-U ↗
32. Accelerated aqueous aging simulation of in vivo oxidation for gamma-sterilized UHMWPE10.1002/jbm.b.31294 ↗
33. Morphological characterisation of the crystalline structure of cold-drawn HDPE used as a model material for the environmental stress cracking (ESC) phenomenon10.1016/S0032-3861(98)00500-X ↗
34. Use of vitamin E to protect cross-linked UHMWPE from oxidation10.1016/j.biomaterials.2010.01.076 ↗
35. Development of an extremely wear-resistant ultra high molecular weight polyethylene for total hip replacements10.1002/jor.1100170203 ↗
36. Muratoglu, O.K., 2009. Highly crosslinked and melted UHMWPE. In: UHMWPE Biomaterials Handbook, Elsevier, pp. 197–204. doi: 〈http://dx.doi.org/10.1016/B978-0-12-374721-1.00013-4〉.10.1016/B978-0-12-374721-1.00013-4 ↗
37. A novel method of cross-linking ultra-high-molecular-weight polyethylene to improve wear, reduce oxidation, and retain mechanical properties. Recipient of the 1999 HAP Paul Award10.1054/arth.2001.20540 ↗
38. Ex vivo stability loss of irradiated and melted ultra-high molecular weight polyethylene10.2106/JBJS.I.01017 ↗
39. Surface cross-linked UHMWPE can enable the use of larger femoral heads in total joints10.1002/jor.22195 ↗
40. Organization, I.S. of, 2012. ISO 14242-1:2012(en), Implants for surgery — wear of total hip-joint prostheses — Part 1: loading and displacement parameters for wear-testing machines and corresponding environmental conditions for test.
41. Characterization of molecular-orientaiton in polyethyleen by Raman-spectroscopy10.1021/ma00020a032 ↗
42. Surface roughness quantification of CoCrMo implant alloys10.1002/(SICI)1097-4636(1999)48:5<705::AID-JBM16>3.0.CO;2-U ↗
43. Surface roughness of retrieved CoCrMo alloy femoral components from PCA artificial total knee joints
44. Correlation between in vivo stresses and oxidation of UHMWPE in total hip arthroplasty10.1007/s10856-014-5254-9 ↗
45. Oxidation and other property changes of a remelted highly crosslinked UHMWPE in retrieved tibial bearings10.1002/jbm.b.33240 ↗
46. Characterization and accelerated ageing of UHMWPE used in orthopedic prosthesis by peroxide10.3390/ma2020562 ↗
47. The combined effects of crosslinking and high crystallinity on the microstructural and mechanical properties of ultra high molecular weight polyethylene10.1016/j.biomaterials.2005.09.033 ↗
48. Ultra high molecular weight polyethylene: mechanics, morphology, and clinical behavior10.1016/j.jmbbm.2008.12.006 ↗
49. Raman spectroscopic method for determining the crystallinity of polyethylene10.1002/pol.1978.180160704 ↗
50. Wear behaviour, fluorescence and SEM investigations on nanocomposite zirconia-toughened alumina10.1007/s10853-006-0356-5 ↗
51. Highly cross-linked polyethylene in total hip and knee replacement: spatial distribution of molecular orientation and shape recovery behavior10.1155/2014/808369 ↗
52. The effects of contact area and applied load on the morphology of in vitro worn ultra-high molecular weight knee prostheses: a micro-Raman and gravimetric study10.1002/jrs.4545 ↗
53. Three-body wear of UHMWPE acetabular cups by PMMA particles against CoCr, alumina and zirconia heads in a hip joint simulator10.1016/S0043-1648(01)00643-3 ↗
54. Highly crosslinked polyethylenes in hip replacements: improved wear performance or paradox?10.1080/10402000701325204 ↗
55. Specific heat of synthetic high polymers. VIII. Low pressure polyethylene10.1002/pol.1957.1202410604 ↗