journal article·2021-03

Aging behavior of high-translucent CAD/CAM resin-based composite blocks

Vivian Marie Ducke, Nicoleta Ilie

Publisher page

Abstract

Objective The aim of this study was to investigate the influence of artificial aging on the mechanical properties and fracture patterns of novel CAD/CAM resin-based composite blocks (RCB). Methods Flexural strength and modulus of RCBs from seven manufacturers (Voco, Grandio Blocs, GB; Ivoclar Vivadent, Tetric®CAD, TC; DMG, Luxacam Composite, LC; Shofu Block HC, SF; 3M, Lava™ Ultimate, LU; GC, Cerasmart®, CS; Coltene, BRILLIANT Crios, CB) were assessed in a three-point-bending test after an aging process consisting of three sequential steps (14 days storage in artificial saliva, 10,000 thermo-cycles in distilled water between 5/55 °C, 48 h storage in ethanol 75%). Fracture origins were determined in a fractographic examination using reflected light stereomicroscopy combined with transillumination and scanning electron microscopy. Effects of aging were statistically analysed using one-way ANOVA with Tukey's HSD post hoc test (α = 0.05) and Weibull statistics. Correlations regarding filler amount were analysed using linear regression analysis. Results The strongest influence on the flexural modulus and strength was exerted based on the parameter material (p < 0.001, ɳP2 = 0.957; ɳP2 = 0.770), but the influence of in vitro aging was also significant (p < 0.001, ɳP2 = 0.623; ɳP2 = 0.407). Storage in artificial saliva decreased the flexural modulus and flexural strength of all materials, apart from CS, significantly (p < 0.05). The Weibull moduli varied from 5.8 to 22.4. Filler amount correlated significantly with flexural modulus (p < 0.001; R2 = 0.739). Fractography revealed four different fracture patterns with fracture origins from the corner, edge or sub-surface and a smooth fracture surface with non-identifiable fracture origin. Specimens with smooth fracture surface showed the significantly lowest flexural strength (p < 0.001). Pores, agglomerates and inclusions were identified as fracture origins. Conclusions Storage in artificial saliva mainly reduced the mechanical properties significantly while additional thermal aging mostly maintained the results. Aging in ethanol mostly maintained the results for flexural modulus but led to an increase in flexural strength values to the level of the unaged specimens. Fractographic analysis revealed a significant accumulation of sub-surface fracture origins after storage in ethanol arising from inherent flaws.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Epoxy Resin Curing Processes · Polymer Nanocomposites and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Effect of aging regimens on resin nanoceramic chairside CAD/CAM material10.1111/jopr.12408 ↗
2. Effect of the composition of CAD/CAM composite blocks on mechanical properties10.1155/2018/4893143 ↗
3. Influence of UEDMA BisGMA and TEGDMA on selected mechanical properties of experimental resin composites
4. Mechanical properties of resin-ceramic CAD/CAM restorative materials10.1016/j.prosdent.2015.04.016 ↗
5. The effects of light intensity and light-curing time on the degree of polymerization of dental composite resins10.4012/dmj.27.523 ↗
6. Mechanical properties of resin-ceramic CAD-CAM materials after accelerated aging10.1016/j.prosdent.2017.08.016 ↗
7. Influence of filler type and water exposure on flexural strength of experimental composite resins10.1177/00220345880670050801 ↗
8. Factors affecting the mechanical behavior of Y-TZP10.1016/j.jmbbm.2014.05.013 ↗
9. Does artificial aging affect mechanical properties of CAD/CAM composite materials10.1016/j.jpor.2017.06.001 ↗
10. In vitro aging of dental composites in water--effect of degree of conversion, filler volume, and filler/matrix coupling10.1002/(SICI)1097-4636(19981205)42:3<465::AID-JBM17>3.0.CO;2-F ↗
11. Microstructural and mechanical characterization of CAD/CAM materials for monolithic dental restorations10.1111/jopr.12964 ↗
12. Thermal cycling procedures for laboratory testing of dental restorations10.1016/S0300-5712(98)00037-2 ↗
13. Mechanical properties and internal fit of 4 CAD-CAM block materials10.1016/j.prosdent.2017.03.001 ↗
14. Laboratory mechanical parameters of composite resins and their relation to fractures and wear in clinical trials-A systematic review10.1016/j.dental.2016.11.013 ↗
15. Hussain · 2017 · 33 · 1362
16. Altering of optical and mechanical properties in high-translucent CAD-CAM resin composites during aging10.1016/j.jdent.2019.05.015 ↗
17. Investigations on mechanical behaviour of dental composites10.1007/s00784-009-0258-4 ↗
18. Macro-, micro- and nano-mechanical investigations on silorane and methacrylate-based composites10.1016/j.dental.2009.02.005 ↗
19. Mechanical properties of composite resin blocks for CAD/CAM10.4012/dmj.2014-208 ↗
20. Wear, strength, modulus and hardness of CAD/CAM restorative materials
21. Fractography of clinically fractured, implant-supported dental computer-aided design and computer-aided manufacturing crowns
22. Fracture toughness, flexural strength, and flexural modulus of new CAD/CAM resin composite blocks10.1111/jopr.13123 ↗
23. Fractography and mechanical properties of urethane dimethacrylate dental composites reinforced with glass nanoparticles
24. Mechanical properties and wear behavior of light-cured packable composite resins10.1016/S0109-5641(99)00082-2 ↗
25. In vitro surface degradation of composites by water and thermal cycling10.1016/S0109-5641(86)80012-4 ↗
26. Wear characteristics of current aesthetic dental restorative CAD/CAM materials: two-body wear, gloss retention, roughness and Martens hardness10.1016/j.jmbbm.2013.01.003 ↗
27. Resin composite blocks via high-pressure high-temperature polymerization
28. Subcritical crack growth and in vitro lifetime prediction of resin composites with different filler distributions10.1016/j.dental.2012.05.001 ↗
29. Mechanical properties of experimental composites containing bioactive glass after artificial aging in water and ethanol10.1007/s00784-018-2713-6 ↗
30. Bis-GMA co-polymerizations: influence on conversion, flexural properties, fracture toughness and susceptibility to ethanol degradation of experimental composites10.1016/j.dental.2009.03.010 ↗
31. The effect of thermal stresses on the functional properties of various dental composites10.1016/j.triboint.2020.106509 ↗
32. The biaxial flexural strength and fatigue property of Lava Y-TZP dental ceramic
33. Weibull strength scaling for A standardized rectangular flexure specimens10.1111/j.1151-2916.2003.tb03329.x ↗
34. Chipping fracture resistance of dental CAD/CAM restorative materials: part I--procedures and results
35. Material properties and fractography of an indirect dental resin composite
36. A practical and systematic review of Weibull statistics for reporting strengths of dental materials10.1016/j.dental.2009.09.006 ↗
37. Physical characterization of unfilled and nanofilled dental resins: static versus dynamic mechanical properties
38. ADM guidance-Ceramics: guidance to the use of fractography in failure analysis of brittle materials
39. Study of water sorption, solubility and modulus of elasticity of light-cured dimethacrylate-based dental resins10.1016/S0142-9612(02)00380-0 ↗
40. Aging studies of light cured dimethacrylate-based dental resins and a resin composite in water or ethanol/water
41. Filler leachability of composites stored in distilled water or artificial saliva10.1177/00220345960750091201 ↗
42. Influence of water exposure on the tensile strength of composites10.1177/00220345900690120501 ↗
43. Evaluation of five CAD/CAM materials by microstructural characterization and mechanical tests: a comparative in vitro study10.1186/s12903-017-0458-2 ↗
44. Standardization · 2019
45. Evaluation of mechanical and optical behavior of current esthetic dental restorative CAD/CAM composites10.1016/j.jmbbm.2015.10.004 ↗
46. Technology · 1992
47. Two-year performance of CAD/CAM fabricated resin composite inlay restorations: a randomized controlled clinical trial10.1111/jerd.12534 ↗
48. Chairside CAD/CAM materials. Part 2: flexural strength testing
49. Comparative in vitro wear resistance of CAD/CAM composite resin and ceramic materials10.1016/j.prosdent.2015.07.011 ↗