journal article·2020-09Open access

Durability of staining and glazing on a hybrid ceramics after the three-body wear

João P.M. Tribst, Amanda M.O. Dal Piva, Arie Werner, Lilian C. Anami, Marco A. Bottino, Cornelis J. Kleverlaan

Abstract

Hybrid ceramic is a promising material for monolithic restorations that could require an individualization through the extrinsic staining to improve aesthetics. Due to the possibilities to treat this ceramic prior to staining, this study evaluated the wear resistance of surface treatments prior to staining and glazing a hybrid ceramic. Thirty-two specimens (Vita Enamic) were divided into 8 groups according to the surface treatment prior to the staining (Polishing: Pol, Acid etching: Ac, Sandblasting with Al2O3: Sd or Self-etching silane: Ses) and glaze application (with: gl or without: gl). The specimens were submitted to the ACTA wear machine simulating the presence of food bolus and antagonist. The wear rate of the stain was determined after 7 intervals of 20,000 cycles, using a profilometer. The surface before and after staining, and after wear were inspected using Scanning Electron Microscopy (SEM). The rates were analyzed using three-way ANOVA and Tukey test. The wear was affected by surface treatment, glaze application and number of cycles (p < 0.001). 100% of the staining was removed after 20,000 cycles for Pol, 40,000 for Pol + gl, 60,000 for Ses + gl, 80,000 for Ac, 100,000 for Sd and Ses, 120,000 for Ac + gl and 140,000 for Sd + gl. SEM showed similar worn surfaces. Sandblasting followed by glaze application was the most durable treatment to maintain the external staining on the hybrid ceramic surface when subjected to three-body wear.
Source: europepmc · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (37)

Show source-provided references
1. In vivo wear determination of novel CAD/CAM ceramic crowns by using 3D alignment10.4047/jap.2019.11.2.120 ↗
2. Effect of different resin cements and surface treatments on the shear bond strength of ceramic-glass polymer materials10.1016/j.prosdent.2017.12.016 ↗
3. Assessment of wear facets produced by the ACTA wear machine10.1016/j.jdent.2015.12.003 ↗
4. Inlays made from a hybrid material: adaptation and bond strengths10.2341/13-343-L ↗
5. The influence of gender and bruxism on the human maximum bite force10.1590/S1678-77572006000600011 ↗
6. Chi · 2017 · 71
7. Monolithic ceramics: effect of finishing techniques on surface properties, bacterial adhesion and cell viability10.2341/17-011-L ↗
8. CAD-FEA modeling and analysis of different full crown monolithic restorations10.1016/j.dental.2018.06.024 ↗
9. Three-body wear effect on different CAD/CAM ceramics staining durability10.1016/j.jmbbm.2019.103579 ↗
10. Occlusal wear simulation with the ACTA wear machine10.1016/0300-5712(94)90167-8 ↗
11. Self-etching ceramic primer versus hydrofluoric acid etching: etching efficacy and bonding performance10.1016/j.jpor.2017.06.002 ↗
12. Wear behaviour and surface roughness of polymer infiltrated ceramic material compared to pressable glass ceramic10.21608/adjalexu.2015.58738 ↗
13. The effect of photo-activated glazes on the microhardness of acrylic baseplate resins10.1016/S0300-5712(01)00052-5 ↗
14. Wear resistance of a pressable low-fusing ceramic opposed by dental alloys10.1016/j.jmbbm.2013.12.018 ↗
15. Effect of toothbrushing on shade and surface roughness of extrinsically stained pressable ceramics10.1016/j.prosdent.2015.09.013 ↗
16. Wear of ceramic and antagonist--a systematic evaluation of influencing factors in vitro10.1016/j.dental.2007.06.016 ↗
17. The effect of surface treatments on the mechanical and optical behaviors of CAD/CAM restorative materials10.1111/jopr.12749 ↗
18. Wear resistance and abrasiveness of CAD-CAM monolithic materials10.1016/j.prosdent.2018.05.011 ↗
19. Effect of aging on stained monolithic resin-ceramic CAD/CAM materials: quantitative and qualitative analysis of surface roughness10.1111/jopr.12949 ↗
20. Bonding effectiveness of tooth-colored materials to resin cement provided by self-etching silane primer after short- and long-term storage10.1016/j.prosdent.2018.12.018 ↗
21. Contact- and contact-free wear between various resin composites10.1016/j.dental.2014.11.007 ↗
22. Wear of direct resin composites and teeth: considerations for oral rehabilitation10.1111/eos.12600 ↗
23. Antagonist wear of three CAD/CAM anatomic contour zirconia ceramics10.1016/j.prosdent.2013.06.002 ↗
24. Effect of zirconia polycrystal and stainless steel on the wear of resin composites, dentin and enamel10.1016/j.jmbbm.2018.12.024 ↗
25. Microstructure characterization and SCG of newly engineered dental ceramics10.1016/j.dental.2016.03.018 ↗
26. Comparison of wear between occlusal splint materials and resin composite materials10.1111/joor.12636 ↗
27. Occlusal wear of provisional implant-supported restorations10.1111/cid.12072 ↗
28. Simplified treatment of severe dental erosion with ultrathin CAD-CAM composite occlusal veneers and anterior bilaminar veneers10.1016/j.prosdent.2016.02.013 ↗
29. Full-mouth rehabilitation with monolithic CAD/CAM-fabricated hybrid and all-ceramic materials: a case report and 3-year follow up
30. Bond strength between a polymer-infiltrated ceramic network and a composite for repair: effect of several ceramic surface treatments10.1590/1807-3107bor-2018.vol32.0028 ↗
31. Three-body wear of resin denture teeth with and without nanofillers10.1016/S0022-3913(10)60014-5 ↗
32. The effect of staining and vacuum sintering on optical and mechanical properties of partially and fully stabilized monolithic zirconia10.4012/dmj.2015-054 ↗
33. The effect of glazing and aging on the surface properties of CAD/CAM resin blocks10.4047/jap.2018.10.1.50 ↗
34. The effect of sandblasting duration on the bond durability of dual-cure adhesive cement to CAD/CAM resin restoratives10.4047/jap.2018.10.3.211 ↗
35. Self-etching primers vs acid conditioning: impact on bond strength between ceramics and resin cement10.2341/16-348-L ↗
36. Early and long-term wear of 'fast-set' conventional glass-ionomer cements10.1016/j.dental.2004.09.007 ↗
37. The science and application of IPS e.Max dental ceramic10.1016/j.kjms.2018.01.012 ↗